Postby Zenid » Wed Jul 04, 2012 10:30 am

After my torque arm failed and caused some bother with my new motor, I didn't have much luck getting something suitable to replace it with. Though DoctorBass had a batch of very nice torque rings made (http://endless-sphere.com/forums/viewtopic.php?f=3&t=34150&p=496417&hilit=+torque+steel+laser+cut#p496417) they're not suitable for the swingarm of the kind of scooter I have.

So I thought I'd dip into the the world of CAD design and fabrication of custom parts. Here is my first attempt. I wanted something decent to replace the flimsy things that come with the bike/motor...

Image

I finally took delivery of my order of the real thing: A batch of 12mm torque arms manufactured out of 6.3mm laser-cut steel. Here's one shown next to one of old ones. They have a 6mm hole for the adjuster bolt, and as far as I know are suitable for most 1400W/1500W motors. The torque slots are slightly wider as the 1500W motor has a 16mm axle on the cable side, as compared to the 14mm on the 1400W motor, though the slot diameter required (on mine at least) is 12mm on both. I've also made mine longer, with a wider adjustment slot so that the rear wheel can go back further to accommodate larger tyres. I got a batch of them, so there's plenty left to go in my little shop:

Image

Image

And here it is on the new motor hub, next to the even worse torque arm that came with it (those are the ones that failed):

Image

Happy trails!
Last edited by Zenid on Thu Sep 06, 2012 12:25 pm, edited 1 time in total.
Ego(Saiting/Dichao/Haocheng/Xinling) Electric Scooter Blog & Upgrade Guide http://zenid10.wordpress.com/
72V Upgrade Guide http://zenid10.wordpress.com/category/4 ... v-upgrade/
User avatar
Zenid
100 W
100 W
 
Posts: 270
Joined: Sat Oct 02, 2010 3:53 pm
Location: Nottingham, UK

Re: Heavy duty 12mm torque arm

Postby whereswally606 » Wed Jul 04, 2012 11:52 am

Zenid, love the new torque plate. are you selling do you have a price for these?
Buy a 400W 12Volt 32a server supply fitted to connect typical 4mm bullet plugs £25.30 to the UK, will ship WW. IM me for details
Ebikes: Scott Ransom & Magie Pie 48V limno2,Norco Team Race & Hub motor 12s4p lico zippy 40C
Norco Savage to receive an 80/100 motor with opticals Not halls Thanks Burtie.
Car: Honda Insight gen 1 hybrid
whereswally606
1 kW
1 kW
 
Posts: 462
Joined: Sun Jun 19, 2011 2:11 pm
Location: Cheshire, UK

Re: Heavy duty 12mm torque arm

Postby Zenid » Wed Jul 04, 2012 1:09 pm

whereswally606 wrote:Zenid, love the new torque plate. are you selling do you have a price for these?

Glad you like it :)
I wasn't going to put these on sale until I'd tested them out myself to make absolutely sure they're fine. As for a price, well unfortunately I had to order internationally and got screwed really badly for import duty and "clearance fees", so they didn't end up as cheap as I'd like (import duty alone adds £1 to the cost of each one). They'll probably be somewhere in the region of £8-10 each, but I'll have to do my sums first...

I'll have a think about it and PM you.
Ego(Saiting/Dichao/Haocheng/Xinling) Electric Scooter Blog & Upgrade Guide http://zenid10.wordpress.com/
72V Upgrade Guide http://zenid10.wordpress.com/category/4 ... v-upgrade/
User avatar
Zenid
100 W
100 W
 
Posts: 270
Joined: Sat Oct 02, 2010 3:53 pm
Location: Nottingham, UK

Re: Heavy duty 12mm torque arm

Postby Zenid » Fri Aug 03, 2012 10:55 am

I've priced them up now and posted them on my shop: £12.50 per pair untreated, or £14.00 per pair treated with hammerite. £2.50 P&P (mainland UK). If you want a quote for international shipping, PM me.
http://www.zenid.com/torquearms.htm

Here's one shown in situ
Image
Ego(Saiting/Dichao/Haocheng/Xinling) Electric Scooter Blog & Upgrade Guide http://zenid10.wordpress.com/
72V Upgrade Guide http://zenid10.wordpress.com/category/4 ... v-upgrade/
User avatar
Zenid
100 W
100 W
 
Posts: 270
Joined: Sat Oct 02, 2010 3:53 pm
Location: Nottingham, UK

Re: Heavy duty 12mm torque arm

Postby kudos » Sun Aug 26, 2012 12:49 pm

Zenid, can I ask which US site you used to get these made?

I need a custom torque arm making up for my new ebike build.

Kudos
Build 1A Gary Fisher Wahoo Hardtail : Crystalyte HS3540 40A 49V : 31mph
Build 1B Gary Fisher Wahoo Hardtail : Mac 10T 30A 49V : 27mph
Build 1C Gary Fisher Wahoo Hardtail : Crystalyte HS3540 40A 82V :
Build 2 Mountain Cycle Fury FS : Mac 10T 30A 49V : in progress
kudos
100 W
100 W
 
Posts: 281
Joined: Tue Aug 02, 2011 12:56 pm
Location: Guernsey, Channel Islands, UK

Re: Heavy duty 12mm torque arm

Postby Zenid » Thu Sep 06, 2012 12:13 pm

kudos wrote:Zenid, can I ask which US site you used to get these made?

I need a custom torque arm making up for my new ebike build.

Kudos

I've PMed you on this.
Ego(Saiting/Dichao/Haocheng/Xinling) Electric Scooter Blog & Upgrade Guide http://zenid10.wordpress.com/
72V Upgrade Guide http://zenid10.wordpress.com/category/4 ... v-upgrade/
User avatar
Zenid
100 W
100 W
 
Posts: 270
Joined: Sat Oct 02, 2010 3:53 pm
Location: Nottingham, UK

Re: Heavy duty 12mm torque arm

Postby kudos » Fri Sep 07, 2012 4:27 am

Zenid, I don't have a PM?

Kudos
Build 1A Gary Fisher Wahoo Hardtail : Crystalyte HS3540 40A 49V : 31mph
Build 1B Gary Fisher Wahoo Hardtail : Mac 10T 30A 49V : 27mph
Build 1C Gary Fisher Wahoo Hardtail : Crystalyte HS3540 40A 82V :
Build 2 Mountain Cycle Fury FS : Mac 10T 30A 49V : in progress
kudos
100 W
100 W
 
Posts: 281
Joined: Tue Aug 02, 2011 12:56 pm
Location: Guernsey, Channel Islands, UK

Re: Heavy duty 12mm torque arm

Postby Zenid » Sat Sep 08, 2012 8:17 am

kudos wrote:Zenid, I don't have a PM?

Sorry, someone else asked me the same question by PM and I got you mixed up. PM on its way.
Ego(Saiting/Dichao/Haocheng/Xinling) Electric Scooter Blog & Upgrade Guide http://zenid10.wordpress.com/
72V Upgrade Guide http://zenid10.wordpress.com/category/4 ... v-upgrade/
User avatar
Zenid
100 W
100 W
 
Posts: 270
Joined: Sat Oct 02, 2010 3:53 pm
Location: Nottingham, UK

Re: Heavy duty 12mm torque arm

Postby ambroseliao » Sat Sep 08, 2012 8:51 am

Why not just post the site here? :? :roll:
http://www.ebikes.ca/ for the best in ebike knowledge and equipment.

Tidalforce S-750, TidalForce iO Cruiser, 2x TidalForce M-750. Crystalyte HS3540 sensorless, 72V 45A Crystalyte SL controller, ebikes.ca DrainBrain & Cycle Analyst meters. GoPro HD Hero2 camera. A123 20Ah batteries. 88.2V 10Ah LiPO. My blog: http://ebikerider.blogspot.com
Remember LiFEPo4 HVC is 3.65V and LVC is 2.7V
User avatar
ambroseliao
100 kW
100 kW
 
Posts: 1258
Joined: Mon Apr 27, 2009 3:34 pm
Location: Washington, DC, USA area

Re: Heavy duty 12mm torque arm

Postby Zenid » Sun Sep 09, 2012 4:34 am

ambroseliao wrote:Why not just post the site here? :? :roll:

Long story...
Ego(Saiting/Dichao/Haocheng/Xinling) Electric Scooter Blog & Upgrade Guide http://zenid10.wordpress.com/
72V Upgrade Guide http://zenid10.wordpress.com/category/4 ... v-upgrade/
User avatar
Zenid
100 W
100 W
 
Posts: 270
Joined: Sat Oct 02, 2010 3:53 pm
Location: Nottingham, UK


Return to E-Scooter and Motorcycle General Discussion

Who is online

Users browsing this forum: No registered users and 5 guests