Dr.Bass Steveo found 7s3p Module! Awesome Price!!

Batteries, Chargers, and Battery Management Systems.
User avatar
zEEz
1 kW
1 kW
Posts: 378
Joined: May 09, 2011 7:30 am
Location: around Europe

Re: Group Buy? Dr.Bass Steveo found 7s3p Module! Awesome Pri

Post by zEEz » May 11, 2012 9:09 am

SlyCayer wrote:Just finished the CBA test at 1A on a 7S3P module and, 59.729 Ah \o/ and IR is 3.7 mohms

I will recharge and retest again.
Ah number is fine but Ri is not a very conforting number ... being a parallel of 3 cells with average Ri=2 mohm.
I hope something is not good in your setup for testing, otherwise this would point out to a 10mohm per cell
that is like to say those cells are quite used and old and would heat up very quickly under strong current load. :x

hope for the best :arrow:
from 1A-1S to 300A-16S ESC ^_^ 3g to 10Kg brushless motors ... 3W to 15kW

User avatar
oatnet
100 MW
100 MW
Posts: 2930
Joined: Apr 26, 2007 3:03 pm
Location: SoCal, USA

Re: Group Buy? Dr.Bass Steveo found 7s3p Module! Awesome Pri

Post by oatnet » May 11, 2012 10:07 am

zEEz wrote:
SlyCayer wrote:Just finished the CBA test at 1A on a 7S3P module and, 59.729 Ah \o/ and IR is 3.7 mohms

I will recharge and retest again.
Ah number is fine but Ri is not a very conforting number ... being a parallel of 3 cells with average Ri=2 mohm.
I hope something is not good in your setup for testing, otherwise this would point out to a 10mohm per cell
that is like to say those cells are quite used and old and would heat up very quickly under strong current load. :x

hope for the best :arrow:
I think (hope) that is the IR for the 7s pack, not a single set of cells, which would mean .52mohm per 3p-supercell. When I IR tested the cell_man a123 prisimatics a few years back, they were between 1.00 mohm and 1.16 mohm, mostly around 1.06mohm.

Sutho, thanks for the capacity test, that is reassuring. When I saw your picture, I first thought you had gotten a totally different BMS, nice clean install of your new one. I have been thinking about cutting the connectors off too, but I might just put andersons on the balance wires instead.

Were your original BMS dated 2009 or 2010?
What color was the thermal paste/sidecovers/BMS date on the units you got marked for the fisker?

-JD
Last edited by oatnet on May 11, 2012 10:12 am, edited 1 time in total.
Member 117 of 26,000+

153v DUNE BUGGY © 164v Vectrix E-Moto © 72v Norco A-line/x5403 © 60v Specialized Enduro Comp/BMC © 72v x5tracycle © 48v TF IO/BMC © 36v Kepler FrictionDrive © Spot-Welding a123 © Pelican Front Packs © Vectrix Battery Replacement © MORE !!


Image大鸡巴 Motors
Knowledge is acquired through experience, everything else is just information - Albert Einstein
"Cheater?" I'm not competing, I'm Commuting!

SlyCayer
1 kW
1 kW
Posts: 315
Joined: Sep 06, 2010 6:24 am
Location: Limoges, Ontario
Contact:

Re: Group Buy? Dr.Bass Steveo found 7s3p Module! Awesome Pri

Post by SlyCayer » May 11, 2012 10:12 am

oatnet wrote:
zEEz wrote:I think (hope) that is the IR for the 7s pack, not a single set of cells, which would be .52mohm per 3p-supercell. When I IR tested the cell_man a123 prisimatics a few years back, they were between 1.00 mohm and 1.16 mohm, mostly around 1.06mohm.
This is the whole pack IR, not just 1 pack of 3P, it's the IR from + TERMINAL to - TERMINAL of the whole 7S3P pack, I think it's pretty good.
http://www.JCCayer.com Where you can find tools and Dewalt(A123) batteries.

User avatar
zEEz
1 kW
1 kW
Posts: 378
Joined: May 09, 2011 7:30 am
Location: around Europe

Re: Group Buy? Dr.Bass Steveo found 7s3p Module! Awesome Pri

Post by zEEz » May 11, 2012 10:59 am

SlyCayer wrote:This is the whole pack IR, not just 1 pack of 3P, it's the IR from + TERMINAL to - TERMINAL of the whole 7S3P pack, I think it's pretty good.
Ah, cool! this is great news! 8) This is very good indeed :!:
This bring you perfectly in the ballpark numbers given for the Ri of an average
new A123 cell ... so it seems that -at least for you- this Victorpower order
was a good bargain! :mrgreen:

have fun!
from 1A-1S to 300A-16S ESC ^_^ 3g to 10Kg brushless motors ... 3W to 15kW

ga2500ev
1 mW
1 mW
Posts: 19
Joined: Mar 23, 2012 7:46 am

Re: Group Buy? Dr.Bass Steveo found 7s3p Module! Awesome Pri

Post by ga2500ev » May 11, 2012 1:32 pm

Can we get an update on the total cost + shipping for received modules?

Even though it seems like a crap shoot, it still may be worth getting a couple if the end to end cost
isn't too outrageous.

ga2500ev

User avatar
oatnet
100 MW
100 MW
Posts: 2930
Joined: Apr 26, 2007 3:03 pm
Location: SoCal, USA

Re: Group Buy? Dr.Bass Steveo found 7s3p Module! Awesome Pri

Post by oatnet » May 11, 2012 3:08 pm

ga2500ev wrote:Can we get an update on the total cost + shipping for received modules?

Even though it seems like a crap shoot, it still may be worth getting a couple if the end to end cost
isn't too outrageous.

ga2500ev
A number of people posted their pricing/shipping costs in the beginning of this thread.

-JD
Member 117 of 26,000+

153v DUNE BUGGY © 164v Vectrix E-Moto © 72v Norco A-line/x5403 © 60v Specialized Enduro Comp/BMC © 72v x5tracycle © 48v TF IO/BMC © 36v Kepler FrictionDrive © Spot-Welding a123 © Pelican Front Packs © Vectrix Battery Replacement © MORE !!


Image大鸡巴 Motors
Knowledge is acquired through experience, everything else is just information - Albert Einstein
"Cheater?" I'm not competing, I'm Commuting!

John in CR
100 GW
100 GW
Posts: 13999
Joined: May 20, 2008 12:58 am
Location: Paradise

Re: Group Buy? Dr.Bass Steveo found 7s3p Module! Awesome Pri

Post by John in CR » May 11, 2012 3:18 pm

texaspyro wrote:A123 recommends float charging their cells a 3.4V (actually they say charge them to 3.6V then float them at 3.4V). My testing shows about zero capacity difference between 3.4 and 3.6V, you just get to the fully charged state a lot quicker a 3.6V
:idea: That's enough variance that a direct connection to a DIY solar panel made up of .5V cells might just work. I didn't test many, but each of the cells I did test in varying amounts of sun put out .5V , and the current output is what varied. 7 solar cells in series + 1 low voltage drop diode repeated for each series cell in my pack and I've got a solar powered balance charger made up of single cell solar chargers.

I must be missing something, because it sounds too good to be true.

texaspyro
1 MW
1 MW
Posts: 1519
Joined: May 12, 2010 6:53 pm

Re: Group Buy? Dr.Bass Steveo found 7s3p Module! Awesome Pri

Post by texaspyro » May 11, 2012 4:27 pm

I would highly recommend a voltage regulator in there... Solar cells voltage varies widely depending upon the load. A fully charged pack represents a rather light load.

davec
1 kW
1 kW
Posts: 415
Joined: May 22, 2011 8:08 am

Re: Group Buy? Dr.Bass Steveo found 7s3p Module! Awesome Pri

Post by davec » May 11, 2012 5:51 pm

"Just finished the CBA test at 1A on a 7S3P module and, 59.729 Ah \o/ and IR is 3.7 mohms"

the ir seems ok
but 1amp discharge on this pack is like 0.01C ? at such a low c it better deliver the full 60ah
any battery will do good at 0.01c question is what can it do under a real load
1c 60a draw would be more useful
or even a 0.5c

edit: and a graph as well

999zip999
100 GW
100 GW
Posts: 8353
Joined: Jan 10, 2010 1:40 pm
Location: Dana Point So. Cal

Re: Group Buy? Dr.Bass Steveo found 7s3p Module! Awesome Pri

Post by 999zip999 » May 11, 2012 8:13 pm

Good news is good news.

kevo
1 kW
1 kW
Posts: 330
Joined: Sep 15, 2009 9:40 pm

Re: Group Buy? Dr.Bass Steveo found 7s3p Module! Awesome Pri

Post by kevo » May 11, 2012 8:28 pm

Sutho, sorry to hear of your warranted disappointment.
Oatnet glad you fared better it seems.
Regardless, both are important data points for this approach.
Thanks Justin of http://ebikes.ca for your amazing talents, dedication and contributions to ES!
Post licensed under "Open Source" http://creativecommons.org/licenses/by-nc-nd/3.0/

User avatar
oatnet
100 MW
100 MW
Posts: 2930
Joined: Apr 26, 2007 3:03 pm
Location: SoCal, USA

Re: Group Buy? Dr.Bass Steveo found 7s3p Module! Awesome Pri

Post by oatnet » May 12, 2012 9:18 am

davec wrote:"Just finished the CBA test at 1A on a 7S3P module and, 59.729 Ah \o/ and IR is 3.7 mohms"

the ir seems ok
but 1amp discharge on this pack is like 0.01C ? at such a low c it better deliver the full 60ah
any battery will do good at 0.01c question is what can it do under a real load
1c 60a draw would be more useful
or even a 0.5c

edit: and a graph as well
I can't believe this a123-hating Troll is still posting in this thread, like he has any experience with the subject or something relevant to add. Obviously, a standard CBA can't handle the 1500 watt load from a 1c discharge on a 7s 60a pack. Obviously, the pack is going to deliver really similar WH at 0.1c and 1c, and probably up to 10c. Skippy, go throw your poo at something else.

-JD
Member 117 of 26,000+

153v DUNE BUGGY © 164v Vectrix E-Moto © 72v Norco A-line/x5403 © 60v Specialized Enduro Comp/BMC © 72v x5tracycle © 48v TF IO/BMC © 36v Kepler FrictionDrive © Spot-Welding a123 © Pelican Front Packs © Vectrix Battery Replacement © MORE !!


Image大鸡巴 Motors
Knowledge is acquired through experience, everything else is just information - Albert Einstein
"Cheater?" I'm not competing, I'm Commuting!

miro13car
100 kW
100 kW
Posts: 1453
Joined: Mar 26, 2007 1:30 pm
Location: Calgary, Canada

Re: Group Buy? Dr.Bass Steveo found 7s3p Module! Awesome Pri

Post by miro13car » May 12, 2012 10:11 am

especially after he accused me and Lithuanian people of lies about faulty A123 cells.
He seems does not see what other can see on my pictures, or he pretends.

User avatar
oatnet
100 MW
100 MW
Posts: 2930
Joined: Apr 26, 2007 3:03 pm
Location: SoCal, USA

Re: Group Buy? Dr.Bass Steveo found 7s3p Module! Awesome Pri

Post by oatnet » May 12, 2012 10:24 am

After leaving the packs sit for a few days, most of the cells in the 28s and (3) 7s packs are around 3.57v-3.58v, one was 3.55v.

I accidentally let the bulk-charge run too long on one of the 7s packs, and I ended up with some cells at 3.68v and some at 3.5v. I used a light bulb to discharge the highest cell down to 3.4v, and then used the balance chargers to bring them all up to 3.65v, and left them on all night - and all of those cells are still sitting around 3.63v. I thought I saw something similar when building the Headway pack on my Vectrix, it seemed that after a charge/burn off part of the fluff charge/re-charge, or maybe it was sitting on the balance charger for an extended time, the cells held voltage much much longer. Because charging to peak voltage is hard on the cells, and as texaspyro demonstrated it does not yield significant WH, I would NOT want to do on a regular basis. Further, I'm not entirely sure I am not whacky and mis-correlating events... but if I am not, I wonder if holding voltage means that this opens pathways in the cells, or helps with top balance.

Anyhow, I built some cables to connect the batteries, using 4ga wire and lugs with 1/4" hole, crimped, soldered, with thick adhesive shrink-wrap for strain relief. Since there are two holes on each terminal, I ran two of the cables for each connection. Per the '3-up' rule, the two 4ga are equivilant to a 1/0 cable. I am running 4/0 cable through the rest of my VW bus, but the runs between the modules are so short it shouldn't matter. I also like the redundancy - if one of the cables comes loose at 175v, instead of a plasma-ball-generating arc, the other cable should still be connected.

It is really impressive to see a 9kw pack take up so little room, shown against a 17" car rim for scale. Next, I'll make power cables for either end of the pack, slap it in my VW Bus, and see what it can do. :D

-JD
a_IMG_3621.JPG
Why did I make 8 cables when I only needed 6?
a_IMG_3621.JPG (81.21 KiB) Viewed 1481 times
b_IMG_3627.JPG
9kw 175v pack, ready for a car.
b_IMG_3627.JPG (98.68 KiB) Viewed 1481 times
Member 117 of 26,000+

153v DUNE BUGGY © 164v Vectrix E-Moto © 72v Norco A-line/x5403 © 60v Specialized Enduro Comp/BMC © 72v x5tracycle © 48v TF IO/BMC © 36v Kepler FrictionDrive © Spot-Welding a123 © Pelican Front Packs © Vectrix Battery Replacement © MORE !!


Image大鸡巴 Motors
Knowledge is acquired through experience, everything else is just information - Albert Einstein
"Cheater?" I'm not competing, I'm Commuting!

rolf_w
100 W
100 W
Posts: 140
Joined: Aug 04, 2009 12:04 pm

Re: Group Buy? Dr.Bass Steveo found 7s3p Module! Awesome Pri

Post by rolf_w » May 12, 2012 2:54 pm

I have tried to identify the major chips on the A123 BMS (from a 7s3p battery) in order to understand the principle functions of it. Some ICs I couldn't identify - probably some here in this thread would be better qualified?

IC1 (Quadruple 2-input NOR gate)
NXP HEF 4001BT (e.g. http://www.alldatasheet.com/datasheet-p ... 001BT.html)

IC5 (Quad 2-Input NAND Schmitt Trigger)
VHCT 132A PPJG (e.g. http://www.alldatasheet.com/datasheet-p ... 132AD.html)

IC9 (???)
CEP
JX2

IC10 (Freescale Semiconductor: Microcontroller)
S9S08DZ32 (e.g. http://www.alldatasheet.com/datasheet-p ... F2CLF.html)
CLH 1M 74K
CTDR 1020Q

IC12 (Analog Devices:???)
C
4S

IC17 (Intersil Corporation: Precision, Low Noise FGA™ Voltage Reference)
21009BF (e.g. http://www.alldatasheet.com/datasheet-p ... B812Z.html)
Z41

IC19 (Analog Devices: Triple-Channel Digital Isolator)
UM1301W (e.g. http://www.alldatasheet.com/datasheet-p ... 01ARW.html)
SRWZ5SS

IC23 (NXP Semiconductors: High-speed CAN transceiver)
TJA1051 (e.g. http://www.alldatasheet.com/datasheet-p ... 1051T.html)
TC AB
P1030089e.jpg
I haven't shown the backside of the pcb , it contains amongst others the bleeding resistors ...
r

User avatar
oatnet
100 MW
100 MW
Posts: 2930
Joined: Apr 26, 2007 3:03 pm
Location: SoCal, USA

Re: Group Buy? Dr.Bass Steveo found 7s3p Module! Awesome Pri

Post by oatnet » May 12, 2012 8:22 pm

[attachment=0]IMG_3666.jpg[/attachment]

[attachment=3]IMG_3638.jpg[/attachment]

[attachment=2]IMG_3652.jpg[/attachment]

[attachment=1]IMG_3653.jpg[/attachment]
Attachments
IMG_3638.jpg
I made the main power leads today - 1/4" for the M6 bolt end, and 1/2" for the connection to the 4/0 cable going back to the controller.
IMG_3638.jpg (161.12 KiB) Viewed 1535 times
IMG_3652.jpg
I test-mounted a pair of M6 x 10 stainless hex bolts today using the new '+' power leads. One of my packs came with a few nice star-head bolts, over nylon nuts, locktite-red, which I wanted to emulate. I tried a nylon washer under an M6 washer it on the left bolt, I can only figure that the nylon is intended to prevent overtorquing. On the right, I used M6 washers and spring washers, and felt that one held the cable more securely, so that is what I will use, along with locktite blue.
IMG_3652.jpg (159.06 KiB) Viewed 1535 times
IMG_3653.jpg
The complete wiring harness, removed so I can move the modules to the VW Bus!
IMG_3653.jpg (144.54 KiB) Viewed 1535 times
IMG_3666.jpg
Dragged my super-accurate (but heavy) scale downstairs, leveled it, and tared the piece of wood the 28s would sit on. When I sild the battery on the scale, it came up exactly 107lb - minus maybe 1.3lbs for the two BMS and a handful of screws I've stripped off. That is 1.27lb per cell, packaged for installation.
IMG_3666.jpg (130.58 KiB) Viewed 1535 times
Member 117 of 26,000+

153v DUNE BUGGY © 164v Vectrix E-Moto © 72v Norco A-line/x5403 © 60v Specialized Enduro Comp/BMC © 72v x5tracycle © 48v TF IO/BMC © 36v Kepler FrictionDrive © Spot-Welding a123 © Pelican Front Packs © Vectrix Battery Replacement © MORE !!


Image大鸡巴 Motors
Knowledge is acquired through experience, everything else is just information - Albert Einstein
"Cheater?" I'm not competing, I'm Commuting!

peterperkins
100 W
100 W
Posts: 228
Joined: Jun 06, 2008 2:10 am
Contact:

Re: Group Buy? Dr.Bass Steveo found 7s3p Module! Awesome Pri

Post by peterperkins » May 12, 2012 11:58 pm

Does the A123 BMS appear to function in a standalone mode?

I.E. when connected to the pack are the bleed resistors becoming active when a cell gets above voltage x?
Or is it waiting for some master controller over the can bus to operate it?

If you could establish which bleed resistors = which chanel you could fake one channel voltage to BMS so it thinks cell is high and see if resistors start bleeding?

It might allow us to use it in some limited fashion?

On a seperate note can all those who return packs as faulty mark them in some subtle / covert manner with UV pen or similiar so we can check any new arrivals.
Under the BMS cover possibly? :wink:
Honda Insight MK1 fitted LIC Lithium Supercapacitors 50x2200F Pack
BCM Fooler, BCM Interceptor, BCM Gauge, Li-Ion BMS System, OBDIIC&C, IMAC&C
http://www.150mpg.co.uk

User avatar
Sutho
10 W
10 W
Posts: 72
Joined: Apr 11, 2012 7:19 am
Location: Newcastle, Australia

Re: Group Buy? Dr.Bass Steveo found 7s3p Module! Awesome Pri

Post by Sutho » May 13, 2012 1:33 am

peterperkins wrote:On a seperate note can all those who return packs as faulty mark them in some subtle / covert manner with UV pen or similiar so we can check any new arrivals.
Under the BMS cover possibly? :wink:
Good idea.....but then you'll know.....and then you'll want to do something about it.....and then you'll be in a similar position as me. :wink:

cwah
10 GW
10 GW
Posts: 4529
Joined: Jul 24, 2011 5:42 am
Location: Between paris and london

Re: Group Buy? Dr.Bass Steveo found 7s3p Module! Awesome Pri

Post by cwah » May 13, 2012 3:58 am

Anyone from UK interested in a group buy? This seems to be a good deal if we can receive good cells
Help me find my stolen electric brompton: http://bit.ly/1a0vbBC and Bosch Sinus B3 http://bit.ly/1eV0WQz

deVries
1 MW
1 MW
Posts: 1827
Joined: Jul 10, 2008 11:29 pm
Location: Solar Powered 3000w Texas

Re: Group Buy? Dr.Bass Steveo found 7s3p Module! Awesome Pri

Post by deVries » May 13, 2012 5:06 am

cwah wrote:Anyone from UK interested in a group buy? This seems to be a good deal if we can receive good cells
Read the recent posts starting with "page" 24 to understand the odds of getting a good module. Also, if you just need 1-2 modules, then waiting for a group buy won't save you much money. If they sell the modules for $155, then it would be a very good deal. IMO. :twisted: :idea:

cwah
10 GW
10 GW
Posts: 4529
Joined: Jul 24, 2011 5:42 am
Location: Between paris and london

Re: Group Buy? Dr.Bass Steveo found 7s3p Module! Awesome Pri

Post by cwah » May 13, 2012 5:45 am

Yeah, but I suppose the group buy would be in US. For me in europe it's not that interesting. So probably have to go for cells only.

Had a quote for 29.75$/cell... damn.. I better go lipo lol
Help me find my stolen electric brompton: http://bit.ly/1a0vbBC and Bosch Sinus B3 http://bit.ly/1eV0WQz

drdmdmd
1 µW
1 µW
Posts: 1
Joined: May 13, 2012 8:40 am

Re: Group Buy? Dr.Bass Steveo found 7s3p Module! Awesome Pri

Post by drdmdmd » May 13, 2012 8:48 am

xin wang <victpowersales@victpower.cn> wrote:

Dear:"........

Thx for ur mail

Im sorry , we dont any guarantees for those modules

And no after sell service

Buy or not , it;s up to you .....

Best Regards :(

User avatar
oatnet
100 MW
100 MW
Posts: 2930
Joined: Apr 26, 2007 3:03 pm
Location: SoCal, USA

Re: Group Buy? Dr.Bass Steveo found 7s3p Module! Awesome Pri

Post by oatnet » May 13, 2012 11:21 am

cwah wrote:Yeah, but I suppose the group buy would be in US. For me in europe it's not that interesting. So probably have to go for cells only.

Had a quote for 29.75$/cell... damn.. I better go lipo lol
Victpower's new single-cells are great, and $25/cell delivered - and are rated for 3000 cycles.
Member 117 of 26,000+

153v DUNE BUGGY © 164v Vectrix E-Moto © 72v Norco A-line/x5403 © 60v Specialized Enduro Comp/BMC © 72v x5tracycle © 48v TF IO/BMC © 36v Kepler FrictionDrive © Spot-Welding a123 © Pelican Front Packs © Vectrix Battery Replacement © MORE !!


Image大鸡巴 Motors
Knowledge is acquired through experience, everything else is just information - Albert Einstein
"Cheater?" I'm not competing, I'm Commuting!

totinen
10 mW
10 mW
Posts: 31
Joined: Apr 02, 2012 12:11 pm
Location: Finland

Re: Group Buy? Dr.Bass Steveo found 7s3p Module! Awesome Pri

Post by totinen » May 13, 2012 2:08 pm

drdmdmd wrote:xin wang <victpowersales@victpower.cn> wrote:

Dear:"........

Thx for ur mail

Im sorry , we dont any guarantees for those modules

And no after sell service

Buy or not , it;s up to you .....

Best Regards :(
So, she is honest.

totinen
10 mW
10 mW
Posts: 31
Joined: Apr 02, 2012 12:11 pm
Location: Finland

Re: Group Buy? Dr.Bass Steveo found 7s3p Module! Awesome Pri

Post by totinen » May 13, 2012 2:24 pm

deVries wrote:
cwah wrote:Anyone from UK interested in a group buy? This seems to be a good deal if we can receive good cells
Read the recent posts starting with "page" 24 to understand the odds of getting a good module. Also, if you just need 1-2 modules, then waiting for a group buy won't save you much money. If they sell the modules for $155, then it would be a very good deal. IMO. :twisted: :idea:
Or then there should be someone checking modules prior shipment.

Post Reply