3kwh 20s40ah HK lipo going up in flames while charging.

Batteries, Chargers, and Battery Management Systems.

Re: 3kwh 20s40ah HK lipo going up in flames while charging.

Postby liveforphysics » Thu May 03, 2012 3:30 pm

methods wrote:
liveforphysics wrote:I would love to know what you think any amount of firefighters or army guys or anyone else would have done better.



Duh
He would have pulled out the 35lbs of powdered copper he keeps in his backpack for lithium fires :roll:

:mrgreen:

-methods



Lol.
For ebike parts, don't be a douche, buy from http://www.ebikes.ca or http://www.MethTek.com

Justin saved the forum at great personal expense! The man is a legend and a hero!
User avatar
liveforphysics
100 GW
100 GW
 
Posts: 10963
Joined: Wed Oct 29, 2008 1:48 am
Location: Santa Cruz, CA, USA

Re: 3kwh 20s40ah HK lipo going up in flames while charging.

Postby Stevil_Knevil » Thu May 03, 2012 5:12 pm

:idea: Mounting lipo packs with 5mm bungee cord would allow flaming packs - (as they melt through) to be ejected off the side(?)..

..not unlike a fuse..
User avatar
Stevil_Knevil
10 kW
10 kW
 
Posts: 766
Joined: Tue Jan 09, 2007 8:32 pm
Location: Up where the air is fresh and clean

Re: 3kwh 20s40ah HK lipo going up in flames while charging.

Postby El_Steak » Thu May 03, 2012 5:50 pm

My sympathies, that's a lot of Lipo to see going down in flames. Hopefully you'll be able to salvage some of it.

As the other said, LVC boards (Methods supplies them for cheap) are the way to go.

For a 20s pack, a duo of 1000W 10s RC chargers on separate power supplies is also a good way to charge with HVC cell-level protection and balancing.
TidalForce S-750 frame
Rear 2807 in a 24" wheel fed by a Methods 100V 100A controller
LiPo config: 24s3p 15ah
All the details here: viewtopic.php?f=6&t=17166
User avatar
El_Steak
10 kW
10 kW
 
Posts: 643
Joined: Tue Aug 11, 2009 8:33 pm
Location: Gatineau, Quebec

Re: 3kwh 20s40ah HK lipo going up in flames while charging.

Postby amberwolf » Fri May 04, 2012 12:17 am

Ypedal wrote:A few of my bikes have the packs hard mounted and i worry some day that this will happen and i got no way to quickly remove the pack to let it burn....... *ponders a quick release method........ :P

A little thermite or similar, mounted around the edges of the pack mountings. If the pack burns, it sets off the thermite and then you just knock the thing out of the frame. ;)

Assumign it doesn't melt your frame first.... :P
House Fire Updates Thread


Got a question that isn't personal or private? Post it in the forums, don't PM it. ;)

Wiki your techy info so it doesn't get old, lost and icky:
http://endless-sphere.com/w


Full-Suspension Semi Recumbent Cargo Bike - NuVinci MidDrive
Semi-Recumbent Recycled-Parts Cargo eBike: "CrazyBike2"
DayGlo Avenger, MkII
User avatar
amberwolf
100 GW
100 GW
 
Posts: 13697
Joined: Mon Aug 17, 2009 6:43 am
Location: Phoenix, AZ, USA, Earth, Sol, Local Bubble, Orion Arm, Milky Way, Local Group

Re: 3kwh 20s40ah HK lipo going up in flames while charging.

Postby Stevil_Knevil » Fri May 04, 2012 1:39 am

Bingo! Thermite enhanced bungee cord :twisted:
User avatar
Stevil_Knevil
10 kW
10 kW
 
Posts: 766
Joined: Tue Jan 09, 2007 8:32 pm
Location: Up where the air is fresh and clean

Re: 3kwh 20s40ah HK lipo going up in flames while charging.

Postby Lebowski » Fri May 04, 2012 2:06 am

I have brand new out of the box 5s 5Ah zippy packs for my bike. I'm ballanced charging using a iCharger1010+
to 4.1 V. For discharge I have beepers which observe every cell and are set to go off at 3.6V . Max charge
rate is 1C, discharge 1.5C

I am a Lipo newbe so, am I treating my packs right ? Would a fire like this be likely ?
User avatar
Lebowski
100 kW
100 kW
 
Posts: 1466
Joined: Tue Jun 28, 2011 1:38 am
Location: beautiful Zurich, Switzerland

Re: 3kwh 20s40ah HK lipo going up in flames while charging.

Postby amberwolf » Fri May 04, 2012 2:08 am

Only if you take more Wh out than you are putting in, and then recharge them. ;) Use a wattmeter to monitor charge and discharge, and cell-level LVC / HVC, and you shouldn't have any issues, once you've established that the packs are all good to start with. :)
House Fire Updates Thread


Got a question that isn't personal or private? Post it in the forums, don't PM it. ;)

Wiki your techy info so it doesn't get old, lost and icky:
http://endless-sphere.com/w


Full-Suspension Semi Recumbent Cargo Bike - NuVinci MidDrive
Semi-Recumbent Recycled-Parts Cargo eBike: "CrazyBike2"
DayGlo Avenger, MkII
User avatar
amberwolf
100 GW
100 GW
 
Posts: 13697
Joined: Mon Aug 17, 2009 6:43 am
Location: Phoenix, AZ, USA, Earth, Sol, Local Bubble, Orion Arm, Milky Way, Local Group

Re: 3kwh 20s40ah HK lipo going up in flames while charging.

Postby neptronix » Fri May 04, 2012 2:44 am

Lebowski wrote:I have brand new out of the box 5s 5Ah zippy packs for my bike. I'm ballanced charging using a iCharger1010+
to 4.1 V. For discharge I have beepers which observe every cell and are set to go off at 3.6V . Max charge
rate is 1C, discharge 1.5C

I am a Lipo newbe so, am I treating my packs right ? Would a fire like this be likely ?


That is being extremely nice to them.
You should be fine, unless you have a pack or 2 in there that is a *real* oddball.

I suggest that since you have the same charger setup as me, you check out logview, it works with the iCharger for charge / discharge graphing.

http://www.logview.info/vBulletin/
ES facebook group: http://facebook.com/#!/home.php?sk=group_125035107565566&ap=1

The all-arounder: 8T MAC motor on a Trek 4500.
The girlfriend bike: 350W front MAC on a 700c Trek.
The wheelie machine: 20" Rear Magic Pie II on a Trek 4300 MTB
The Bus: ??? on a 'da bomb' cargo bike frame

Pro-tips for noobs: Avoid BMS Battery like the plague | Charge RC Lipos to 4.15v, stop discharging at 3.5-3.6v | Use torque plates/arms! | Rear mounted hubs are always best
User avatar
neptronix
100 GW
100 GW
 
Posts: 10242
Joined: Tue Jun 15, 2010 5:56 pm
Location: Salt Lake City, Utah

Re: 3kwh 20s40ah HK lipo going up in flames while charging.

Postby amigafan2003 » Fri May 04, 2012 4:06 am

Ypedal wrote:A few of my bikes have the packs hard mounted and i worry some day that this will happen and i got no way to quickly remove the pack to let it burn....... *ponders a quick release method........ :P


Yeah - I had my 63v10ah lipo pack hardmounted in the frame in an alloy box. I now have it sitting in an ezee bag velcro'd to the rear rack. I can rip it off the bike real quick if required.
amigafan2003
100 W
100 W
 
Posts: 220
Joined: Thu Jul 14, 2011 10:05 am

Re: 3kwh 20s40ah HK lipo going up in flames while charging.

Postby dogman » Fri May 04, 2012 5:04 am

About how I treat my packs too Lebowski, except I charge to 4.2v I don't have a good reason to discharge them deep, so I rarely do. Most of the time I stop at about 3.8v

The key things are don't overdischarge, then recharge them in a place where fire would be a bummer. I've really heated up some packs overdischarging them by mistake, but no fires when I did that a to a few times.

I think I will always prefer charging my RC lipo off the bike. That's when the fireworks are likely, or in a crash or other event that shorts them.
THE LIPO RULES. NEVER ABOVE 4.3V NEVER BELOW 2.7V DON'T PUNCTURE

Ideal charging /discharging range for Lipo, 3.65v minimum 4.1v maximum

See battery technology section, FAQ thread at the top of the page for lipo noob info.
User avatar
dogman
100 GW
100 GW
 
Posts: 21992
Joined: Sat May 17, 2008 12:53 pm
Location: Las Cruces New Mexico USA

Re: 3kwh 20s40ah HK lipo going up in flames while charging.

Postby miuan » Fri May 04, 2012 6:28 am

methods wrote:I bet that if you had a meter on all of the individual banks you would have seen that the damaged banks where showing a much higher voltage than all the rest.


I recently tested one of these hardcases specifically to find out what happens to 0V cells that either wouldn't hold charge anymore, or were just puffed but behaved normally. Upon 1.5C charge, the bad cells held a voltage of about 2V while charging, but dropped back to zero in a matter of seconds after I stopped the charge. So each cell was dissipating 15W heat, but eventually they'd start holding some of the charge I gave them, and got to 3.5V by the time the good ones in series already got over 4V. The weak cells were dangerously hot and puffed, but didn't pop. Then I let them sit and watched ALL of them lose voltage, the leakers and keepers alike. About 10mV per minute.
It seems that using these cells would soon result in a situation where they'd get to 0V while others were fully charged, thus overcharging all the other cells, or popping the weak cells from heat. Though they proved to be quite heat resistant, an enclosed pack of stacked cells would've helped them pop much sooner.

methods wrote:$3 for one of those cheap ass Hobby City beepers - buy 3 or 4 of those and plug them in.
That will save your ass next time
Just dont leave them plugged in all the time (while storing)


While they're handy little devices, it's not a good idea to slap them on all the riding time, then bulk charge. They tend to unbalance cells quite badly. Treat and know your cells so you can trust them and not just worry all the time.
I've had much more luck with conservative pack level LVC and cell level monitoring before and during charging (about mid charge).

I also use these on all my (and friends') builds.
http://www.ebay.com/itm/Digital-Voltmet ... 0904901912
...and stop at 3.7V per cell unloaded.
miuan
10 kW
10 kW
 
Posts: 729
Joined: Thu Nov 26, 2009 4:16 am
Location: Slovakia

Re: 3kwh 20s40ah HK lipo going up in flames while charging.

Postby Lebowski » Fri May 04, 2012 6:39 am

dogman wrote:About how I treat my packs too Lebowski, except I charge to 4.2v I don't have a good reason to discharge them deep, so I rarely do. Most of the time I stop at about 3.8v

The key things are don't overdischarge, then recharge them in a place where fire would be a bummer. I've really heated up some packs overdischarging them by mistake, but no fires when I did that a to a few times.

I think I will always prefer charging my RC lipo off the bike. That's when the fireworks are likely, or in a crash or other event that shorts them.


I had a look at the graphs neptronix posted in another thread and had the impression there was not a lot
of Ah to be had between 4.1 and 4.2 ? I chose 3.6 as the underlimit, the beepers measure when the pack
is delivering upto 1.5C so the 3.6 is my idea of 3.7 but take away 0.1 due to the current drawn (the beepers
only have a resolution of 0.1V for the alarm, else I'd have gone with 3.65)
User avatar
Lebowski
100 kW
100 kW
 
Posts: 1466
Joined: Tue Jun 28, 2011 1:38 am
Location: beautiful Zurich, Switzerland

Re: 3kwh 20s40ah HK lipo going up in flames while charging.

Postby whatever » Fri May 04, 2012 7:20 am

cell logs when riding will show duds
I charge in lots of 24v packs also, much safer.
whatever
10 kW
10 kW
 
Posts: 650
Joined: Thu Jun 03, 2010 2:16 am

Re: 3kwh 20s40ah HK lipo going up in flames while charging.

Postby Ypedal » Fri May 04, 2012 7:32 am

http://www.youtube.com/watch?v=5F3hWc0x1B8



In that video, the cell on the left did not burst into flames, even tho it was over-discharged and puffed and vented gas, but it was only 2 cells.... run a 100v pack and do this... it will release flames.
ES site status page, for when "things" happen...
http://www.ypedal.com/ES/ES.htm
----------------
Always Staying Busy !!
http://www.ypedal.com/Projects.htm
User avatar
Ypedal
100 GW
100 GW
 
Posts: 11911
Joined: Wed Dec 27, 2006 12:55 pm
Location: Moncton NB, Canada

Re: 3kwh 20s40ah HK lipo going up in flames while charging.

Postby kfong » Fri May 04, 2012 8:19 am

Bummer, that's a lot of batteries to loose. For those who have batteries mounted into the frame. You should enclose them in metal or carbon fiber with a vent. That way they can burn out without much damage to the bike or surroundings. I never bulk charge if possible, too many unknown variables such as damage to packs after a ride, over discharging, loose connections, wrong charging voltage, bad cells, broken wires. A good RC charger will at least address some of these problems by monitoring the packs through the balance ports. I like the Hyperion chargers, very well designed and reliable. Draining your packs too close to the knee is going to give you unbalanced packs, so balance charging afterwards is a must. If something is wrong, the algorithm on the charger will stop the charge process and indicate the problem. A good way to double check during the charge process with the Hyperions is to look at the balance voltages. It even gives you max difference. Most lipo fires happen during the charge process, since you are forcing energy into the pack vs removing energy during use.

Was any packs saved? Seemed unlikely with such big packs.
Last edited by kfong on Fri May 04, 2012 8:50 pm, edited 3 times in total.
kfong
1 MW
1 MW
 
Posts: 1646
Joined: Tue Sep 02, 2008 11:34 am
Location: SE Michigan, USA

Re: 3kwh 20s40ah HK lipo going up in flames while charging.

Postby Ypedal » Fri May 04, 2012 8:25 am

nevermind the pack... how's the bike ?..
ES site status page, for when "things" happen...
http://www.ypedal.com/ES/ES.htm
----------------
Always Staying Busy !!
http://www.ypedal.com/Projects.htm
User avatar
Ypedal
100 GW
100 GW
 
Posts: 11911
Joined: Wed Dec 27, 2006 12:55 pm
Location: Moncton NB, Canada

Re: 3kwh 20s40ah HK lipo going up in flames while charging.

Postby neptronix » Fri May 04, 2012 11:24 am

Lebowski wrote:
dogman wrote:About how I treat my packs too Lebowski, except I charge to 4.2v I don't have a good reason to discharge them deep, so I rarely do. Most of the time I stop at about 3.8v

The key things are don't overdischarge, then recharge them in a place where fire would be a bummer. I've really heated up some packs overdischarging them by mistake, but no fires when I did that a to a few times.

I think I will always prefer charging my RC lipo off the bike. That's when the fireworks are likely, or in a crash or other event that shorts them.


I had a look at the graphs neptronix posted in another thread and had the impression there was not a lot
of Ah to be had between 4.1 and 4.2 ? I chose 3.6 as the underlimit, the beepers measure when the pack
is delivering upto 1.5C so the 3.6 is my idea of 3.7 but take away 0.1 due to the current drawn (the beepers
only have a resolution of 0.1V for the alarm, else I'd have gone with 3.65)


My graph is deceiving. Those cells were charged up to 4.15v or so.

I avoid charging above 4.175v/cell average though, because i like to bulk charge 99% of the time. You do need a little room for error.
ES facebook group: http://facebook.com/#!/home.php?sk=group_125035107565566&ap=1

The all-arounder: 8T MAC motor on a Trek 4500.
The girlfriend bike: 350W front MAC on a 700c Trek.
The wheelie machine: 20" Rear Magic Pie II on a Trek 4300 MTB
The Bus: ??? on a 'da bomb' cargo bike frame

Pro-tips for noobs: Avoid BMS Battery like the plague | Charge RC Lipos to 4.15v, stop discharging at 3.5-3.6v | Use torque plates/arms! | Rear mounted hubs are always best
User avatar
neptronix
100 GW
100 GW
 
Posts: 10242
Joined: Tue Jun 15, 2010 5:56 pm
Location: Salt Lake City, Utah

Previous

Return to Battery Technology