Suggestions for 100A, 15 to 20AH pack

Post by IBScootn » Dec 29, 2017 9:26 pm

What would you suggest for a small but safe battery pack that comfortably delivers 100A and has a capacity of 15 to 20AH. Since it will have to be charged at work, outside near building, it needs to be fairly safe. Both DIY and purchased packs are being considered.

TIA
Last edited by IBScootn on Jan 02, 2018 6:42 pm, edited 1 time in total.
Motorcycles:
ZEV T7100, 84V, 60AH, 65+mph; Mods: TNC throttle, windshield, Cycle Analyst , Cell Log , and custom charger
Kymco GT300i - for long rides through the Rocky Mountains
Big EV Grin. :)

IBScootn
100 W
100 W
Posts: 230
Joined: Jan 30, 2012 11:47 pm
Location: Colorado, USA

Re: Suggestions for 100A, 15 to 20AH pack

Post by IBScootn » Dec 29, 2017 10:01 pm

Forgot to mention pack voltage: 87.6V currently but anything +/- 5% should do as charger is completely adjustable

Thanks
Motorcycles:
ZEV T7100, 84V, 60AH, 65+mph; Mods: TNC throttle, windshield, Cycle Analyst , Cell Log , and custom charger
Kymco GT300i - for long rides through the Rocky Mountains
Big EV Grin. :)

User avatar
amberwolf
100 GW
100 GW
Posts: 25040
Joined: Aug 17, 2009 6:43 am
Location: Phoenix, AZ, USA, Earth, Sol, Local Bubble, Orion Arm, Milky Way, Local Group
Contact:

Re: Suggestions for 100A, 15 to 20AH pack

Post by amberwolf » Dec 30, 2017 2:03 am

The EIG NMC cells in the for sale section (sorry I forget whose thread it is) would do that; they're 5C continuous cells (10C for 10sec), so a 20Ah pack could do 100A continuous. I don't know the history on what's in that thread, but I'd bet at least most of the cells are good (you'd have to talk to the seller).

I use these on my bike and trike; all of what I got was used already, and still works fine (have had one cell of all the ones I've used degrade significantly, and one in my lighting pack died from overdischarge so far I reversed it--but the other three that were in series with it still work--and they'd already been abused to just about zero once before and recovered).

The ones in teh for sale section are nice and modular, bolt together packs, I think what he's got are 2P packs (40Ah) but you could make different busbars that make them 1p (20Ah) packs, at whatever series number gives you the voltage you need.

They're 4.15v max cells (I use 4.1v max on the lighting pack, and 4v max for the trike's traction pack for typical charge, and 4.14v for "full" charge). I'm using 14s, and a 2p pack weighs around 35-ish lbs. So a 1p 21s pack (87.1v full @ 4.15v/cell) would be about 26-27lbs bare.

You could go 22s and only charge to 4v/cell to lengthen their lifespan, for an 88v full pack.

User avatar
dogman dan
100 GW
100 GW
Posts: 34672
Joined: May 17, 2008 12:53 pm
Location: Las Cruces New Mexico USA

Re: Suggestions for 100A, 15 to 20AH pack

Post by dogman dan » Dec 30, 2017 9:07 am

Yeah, 100 amps and safe, in that size, pretty hard to get with anything much else.

User avatar
wesnewell
100 GW
100 GW
Posts: 7196
Joined: Jan 31, 2011 6:25 pm
Location: Wylie, TX, USA

Re: Suggestions for 100A, 15 to 20AH pack

Post by wesnewell » Dec 30, 2017 3:39 pm

I've been using 24s 10ah 10C and 20C rc lipo packs for years without any problems. A 15ah 20C pack would be rated for 300A, 450A burst.and certainly wouldn't have a problem at only 100A.
Need Advice? https://endless-sphere.com/forums/viewt ... =3&t=66302
Mongoose 26" Ledge 2.1 mtb bike $99, yescomusa.com 48V 1000W rear hub kit $200, Hua Tong 72V 40A controller $35, 10ah 24s lipo $217=~43mph, range=45 miles @ 20mph. 25K miles and still going strong.
Huffy Fortress 3.0 with MXUS 3000 4T motor, 24s lipo, 96V 60A controller. Total cost with extras <$700. Top speed ~50mph
My videos https://www.youtube.com/channel/UC0KW4U ... _G2wQhptMg

IBScootn
100 W
100 W
Posts: 230
Joined: Jan 30, 2012 11:47 pm
Location: Colorado, USA

Re: Suggestions for 100A, 15 to 20AH pack

Post by IBScootn » Dec 31, 2017 7:43 pm

Amberwolf, great suggestion! I like the cell stacking and ease of bussing.

Now what BMS would someone suggest for 21 or 22 cell pack? Prefer a centralized BMS where if a balance lead breaks, a fault is generated.
Motorcycles:
ZEV T7100, 84V, 60AH, 65+mph; Mods: TNC throttle, windshield, Cycle Analyst , Cell Log , and custom charger
Kymco GT300i - for long rides through the Rocky Mountains
Big EV Grin. :)

999zip999
100 GW
100 GW
Posts: 8354
Joined: Jan 10, 2010 1:40 pm
Location: Dana Point So. Cal

Re: Suggestions for 100A, 15 to 20AH pack

Post by 999zip999 » Jan 01, 2018 2:51 pm

Eig cells are great but had a hard time finding out the cycle life on the cells in the used section ? He didn't know a way of shipping.

999zip999
100 GW
100 GW
Posts: 8354
Joined: Jan 10, 2010 1:40 pm
Location: Dana Point So. Cal

Re: Suggestions for 100A, 15 to 20AH pack

Post by 999zip999 » Jan 01, 2018 4:54 pm

Powervelocity. Com has big high power batteries. You would need to email to find out.
Found a link https://endless-sphere.com/forums/viewt ... 0#p1298017

IBScootn
100 W
100 W
Posts: 230
Joined: Jan 30, 2012 11:47 pm
Location: Colorado, USA

Re: Suggestions for 100A, 15 to 20AH pack

Post by IBScootn » Jan 02, 2018 6:39 pm

zip,
Thanks for the suggestion.
Motorcycles:
ZEV T7100, 84V, 60AH, 65+mph; Mods: TNC throttle, windshield, Cycle Analyst , Cell Log , and custom charger
Kymco GT300i - for long rides through the Rocky Mountains
Big EV Grin. :)

IBScootn
100 W
100 W
Posts: 230
Joined: Jan 30, 2012 11:47 pm
Location: Colorado, USA

Re: Suggestions for 100A, 15 to 20AH pack

Post by IBScootn » Jan 02, 2018 7:22 pm

Wesnewell,

Thanks for the suggestion, but I don’t feel comfortable recommending standard hobby king RC packs for the final user of this system. I’ve heard too many stories of a cell in the middle of one of those pack failing and puffing. He doesn’t have the skills or tools to fully and continually verify each cell in each pack. The pack will need a BMS with sufficient balancing so the whole pack can be bank charged.
Motorcycles:
ZEV T7100, 84V, 60AH, 65+mph; Mods: TNC throttle, windshield, Cycle Analyst , Cell Log , and custom charger
Kymco GT300i - for long rides through the Rocky Mountains
Big EV Grin. :)

999zip999
100 GW
100 GW
Posts: 8354
Joined: Jan 10, 2010 1:40 pm
Location: Dana Point So. Cal

Re: Suggestions for 100A, 15 to 20AH pack

Post by 999zip999 » Jan 02, 2018 7:57 pm

Si yes I understand but I don't run lipo I don't run 18650 yet except from a free Pedego 48 volt slim fish pack. I find the highest energy output Samsung 25r address the issue from there