Hey Guys,
Was thinking about a way to avoid the mess of spot welding copper.
What if I use 0.1mm thick copper tape over the serial connections of a battery pack?
0.1mm thickness is as conductive as 0.4mm pure nickel and the tape can sit pretty firm on the connections.
My only concern is that the glue of the tape will ruin the conductivity.
A link to the kind of tape:
https://www.aliexpress.com/item/25-...-conductive-heat-shield-tape/32822080932.html
What are your thoughts?