Working with Lamination Steel

Post by rjhzxc » Dec 28, 2017 3:48 pm

Hi all, I'm completely new to this so please bear with me.

If I were to get some laminations cut for me by a 'laser' guy I know would any burrs produced be a problem? If I was to remove these burrs with, say, a file would the bare metal then need to be coated with an insulating varnish or something?


Best Regards
Rob

User avatar
fechter
100 GW
100 GW
Posts: 12417
Joined: Dec 31, 2006 3:23 pm
Location: California Bay Area, USA

Re: Working with Lamination Steel

Post by fechter » Dec 28, 2017 9:03 pm

No, insulating the edges is not necessary but you would want to paint it to prevent rust.
"One test is worth a thousand opinions"

e-beach
10 MW
10 MW
Posts: 2497
Joined: Jan 10, 2012 9:48 pm
Location: Any Los Angeles area beach I am at. Or Santa Monica or possibly the south bay beaches.

Re: Working with Lamination Steel

Post by e-beach » Dec 28, 2017 9:10 pm

I say it depends on what you are using the laminations for. Are you building a motor? A transformer?

What are you making?

:D
Favorite Quote: "This is L.A., sugar. There is no 'over the top." --- Chris Erskine

Current build: Liahona w/ cheap front suspension and suspension seat post. Yescomusa 36v 800w generic front hub motor. 15ah Headway triangle mounted pack. Tronsung 30 amp,

Previous Build:1992 Trek Antelope 800 - Bone Crusher (no suspension) - Yescomusa 800 watt 36 volt front wheel kit. Don't do it! Get suspension!!!

rjhzxc
1 µW
1 µW
Posts: 2
Joined: Dec 28, 2017 3:41 pm

Re: Working with Lamination Steel

Post by rjhzxc » Dec 29, 2017 6:20 pm

These would be for building up the stator of a pm type alternator/generator.

e-beach
10 MW
10 MW
Posts: 2497
Joined: Jan 10, 2012 9:48 pm
Location: Any Los Angeles area beach I am at. Or Santa Monica or possibly the south bay beaches.

Re: Working with Lamination Steel

Post by e-beach » Dec 29, 2017 7:24 pm

Then my answer would be, yes de-burr the cut laminates if they are ruff. You don't want to scratch any enamel off of your winding. A print shop burnishing tool might be useful. So would a Dremel tool.

:D
Favorite Quote: "This is L.A., sugar. There is no 'over the top." --- Chris Erskine

Current build: Liahona w/ cheap front suspension and suspension seat post. Yescomusa 36v 800w generic front hub motor. 15ah Headway triangle mounted pack. Tronsung 30 amp,

Previous Build:1992 Trek Antelope 800 - Bone Crusher (no suspension) - Yescomusa 800 watt 36 volt front wheel kit. Don't do it! Get suspension!!!

e-beach
10 MW
10 MW
Posts: 2497
Joined: Jan 10, 2012 9:48 pm
Location: Any Los Angeles area beach I am at. Or Santa Monica or possibly the south bay beaches.

Re: Working with Lamination Steel

Post by e-beach » Dec 29, 2017 10:33 pm

Also, you may not need to do anything to the edges if the cuts are well done.

:D
Favorite Quote: "This is L.A., sugar. There is no 'over the top." --- Chris Erskine

Current build: Liahona w/ cheap front suspension and suspension seat post. Yescomusa 36v 800w generic front hub motor. 15ah Headway triangle mounted pack. Tronsung 30 amp,

Previous Build:1992 Trek Antelope 800 - Bone Crusher (no suspension) - Yescomusa 800 watt 36 volt front wheel kit. Don't do it! Get suspension!!!

User avatar
fechter
100 GW
100 GW
Posts: 12417
Joined: Dec 31, 2006 3:23 pm
Location: California Bay Area, USA

Re: Working with Lamination Steel

Post by fechter » Dec 29, 2017 10:41 pm

Ideally you don't want any electrical contact between the laminations, but in many things I've torn apart, they don't seem to be too careful about this, especially if it's away from the windings. My guess is a little contact here and there isn't significant. It will make the most difference where the magnetic flux is changing the most, like in the stator teeth.
"One test is worth a thousand opinions"