Post by shinyballs » Jun 13, 2016 10:50 pm

Got a good deal for this scooter on Craigslist. The motor barely turns unloaded, I'm guessing the SLA battery is likely dead.
Planning to use 10s6P Panasonic 18650PF at 36V, which can easily fit in the case. Replace the front wheel with a 10" BLDC ungeared hub motor.
It's going to be built for torque - riding up steep hils, and limit the top speed to 20mph. I read that the band brake is weak and don't last, so will be using regen on the front motor. For now, will just use the stock motor.
Any recommendations for a 10" front hub motor? Also, where to find a good quality but cheap 36V dc brushed controller for the stock motor?
Attachments
00G0G_61eERp0aYDr_1200x900.jpg
Sale section etiquette, pls be courteous to other members, if you know of a better deal or do not agree with the sale price, do not shove links to similar products being sold by someone else in another member's post.. it's just not nice. If you suspect a scam pls FLAG the thread for moderation and it will be checked out... i know this is a tough one to call but put yourself in the seller's shoes and imagine how you would like it.

https://endless-sphere.com/forums/viewto ... 31&t=25446

User avatar
Dauntless
100 GW
100 GW
Posts: 6056
Joined: May 29, 2010 1:49 am
Location: Coordinates: 33°52′48″N 117°55′43″W

Re: Razor E300s upgrade

Post by Dauntless » Jun 14, 2016 1:04 am

Well, first off, you didn't give us any idea what you really wanted. I'd say with an 800w or higher hub, you can forget the motor that's on it. That's too small for anything particularly powerful.

http://www.aliexpress.com/item/10-800W- ... 78141.html
Any sufficiently advanced technology is INDISTINGUISHABLE FROM MAGIC!
- Arthur C. Clarke

User avatar
shinyballs
1 kW
1 kW
Posts: 386
Joined: Sep 29, 2007 2:43 am
Location: WA, USA

Re: Razor E300s upgrade

Post by shinyballs » Jun 21, 2016 10:49 pm

The Dropouts for that motor is 139mm - too wide, based from several sellers specs. The scooters' fork dropout width is 115mm. There's very limited choices for 10 inch hub motors that can fit. So, I'll be getting a 12" hub and will have to extend the fork by 1 inch. So far, I've found these -
http://www.aliexpress.com/item/high-spe ... .54.OCiczk
http://www.aliexpress.com/item/12-1-2-v ... .43.OCiczk

They are probably the same motor.
Attachments
IMG_0147 - Copy.JPG
IMG_0151.JPG
IMG_0151.JPG (22.8 KiB) Viewed 1245 times
Sale section etiquette, pls be courteous to other members, if you know of a better deal or do not agree with the sale price, do not shove links to similar products being sold by someone else in another member's post.. it's just not nice. If you suspect a scam pls FLAG the thread for moderation and it will be checked out... i know this is a tough one to call but put yourself in the seller's shoes and imagine how you would like it.

https://endless-sphere.com/forums/viewto ... 31&t=25446

User avatar
shinyballs
1 kW
1 kW
Posts: 386
Joined: Sep 29, 2007 2:43 am
Location: WA, USA

Re: Razor E300s upgrade

Post by shinyballs » Jun 27, 2016 7:56 pm

Seller Green E-motion from Aliexpress sent me some info about their 12" motor. It's made for the rear, but I don't see any problem using it on the front.
Attachments
LY12 hub motor.jpg
max 15N.m torque
Sale section etiquette, pls be courteous to other members, if you know of a better deal or do not agree with the sale price, do not shove links to similar products being sold by someone else in another member's post.. it's just not nice. If you suspect a scam pls FLAG the thread for moderation and it will be checked out... i know this is a tough one to call but put yourself in the seller's shoes and imagine how you would like it.

https://endless-sphere.com/forums/viewto ... 31&t=25446

some.bloke
10 µW
10 µW
Posts: 6
Joined: Feb 07, 2015 3:04 am

Re: Razor E300s upgrade

Post by some.bloke » Jun 29, 2016 12:13 am

those motors are cool. Do they have any with a bit more power? 500Watts plus?

User avatar
shinyballs
1 kW
1 kW
Posts: 386
Joined: Sep 29, 2007 2:43 am
Location: WA, USA

Re: Razor E300s upgrade

Post by shinyballs » Jul 18, 2016 1:27 am

The motor has arrived and will paint the insides and add vent holes; I may try Ferro Fluid. When ran as stock, I think no more than 500 watts is a safe limit for this motor.
Does anyone know of a good alternative to chromoly tubing that can be MIG welded? It seems that TIG is the preferred way to weld it - which I don't have.
Attachments
IMG_0158 - Copy.JPG
IMG_0160 - Copy.JPG
Sale section etiquette, pls be courteous to other members, if you know of a better deal or do not agree with the sale price, do not shove links to similar products being sold by someone else in another member's post.. it's just not nice. If you suspect a scam pls FLAG the thread for moderation and it will be checked out... i know this is a tough one to call but put yourself in the seller's shoes and imagine how you would like it.

https://endless-sphere.com/forums/viewto ... 31&t=25446

shortcircuit911
100 W
100 W
Posts: 205
Joined: Feb 19, 2010 1:24 pm
Location: Antioch, CA

Re: Razor E300s upgrade

Post by shortcircuit911 » Jul 18, 2016 10:38 am

I think standard mild steel is fine if you're mig welding, you could buy another set of e300 forks and cut them up. I'd also suggest putting a slug (solid steel rod with the same OD as the ID of the forks) in the fork tubes for added strength. Cool project can wait to see it run.

User avatar
shinyballs
1 kW
1 kW
Posts: 386
Joined: Sep 29, 2007 2:43 am
Location: WA, USA

Re: Razor E300s upgrade

Post by shinyballs » Aug 13, 2016 6:34 pm

Opened the motor, the inside looks crappy. The magnets are dirty and corroded, rusted bearings, some oxidation on the windings and 2 magnets on the rotor are chipped.
Did they sent me a used motor?! The seller is Green E-motion. I'll dispute the transaction. Has anyone tried AliExpress dispute with good results?
Attachments
IMG_0197.JPG
IMG_0199.JPG
IMG_0200.JPG
IMG_0203.JPG
Sale section etiquette, pls be courteous to other members, if you know of a better deal or do not agree with the sale price, do not shove links to similar products being sold by someone else in another member's post.. it's just not nice. If you suspect a scam pls FLAG the thread for moderation and it will be checked out... i know this is a tough one to call but put yourself in the seller's shoes and imagine how you would like it.

https://endless-sphere.com/forums/viewto ... 31&t=25446

User avatar
Ianhill
100 kW
100 kW
Posts: 1129
Joined: Sep 25, 2015 5:55 pm
Location: Wales UK

Re: Razor E300s upgrade

Post by Ianhill » Aug 13, 2016 9:28 pm

Has it spent its life by the sea in storage for many a year ?, By the pics looks like the magnet adhesive has corroded the alloy so the magnets can't be held on the best, thats gutting never nice when a project goes a bit wonky, when you get there with your hub motor it be worth the weight, the razor is a good frame set up its super light and a nice feeling ride and the battery box fits 3 × 4s 16ah multistars with a bit of space left over.

User avatar
shinyballs
1 kW
1 kW
Posts: 386
Joined: Sep 29, 2007 2:43 am
Location: WA, USA

Re: Razor E300s upgrade

Post by shinyballs » Oct 02, 2017 4:03 am

Everything about this scooter is crap except the frame. Cleaned, painted and vented the motor ; just warm when ran continuously for 1Kw. The fork broke twice. So, I inserted a pipe inside the tube and welded the bottom edge and drilled 2 self-tapping screws on the front and back. Have been riding it for more than 5,000 miles.

Top speed: 20mph
Battery: 10s7p Panasonic PF ; no bms
Combined Peak power: 59 Amps 2,049 Watts 33.5V sag

Motor setup#1: aftermarket 24V brushed, stock controller, twist throttle
Motor setup#2: Kelly KBS72101 w/ regen, 12" bldc hub, thumb throttle

Charger: 2 Lenovo psu, Meanwell ELN-30-5 in series @ 41.6V, 5A - onboard

Rear tire: Primo Durotrap Foam Filled Wheelchair tire, size: 10 x 3 in. (3.00-4)

Others:
Turnigy Watt meter
XT90-S Anti-Spark Connector
80 tooth sprocket
36V led headlight
Sunlite wire basket mounted to a modified bike rear rack
Maxi-fuse and holder
Attachments
IMG_0209 - Copy.JPG
IMG_0209 - Copy.JPG (170.09 KiB) Viewed 568 times
IMG_0210 - Copy.JPG
IMG_0210 - Copy.JPG (213.84 KiB) Viewed 568 times
IMG_0213 - Copy.JPG
IMG_0213 - Copy.JPG (173.81 KiB) Viewed 568 times
IMG_0214 - Copy.JPG
IMG_0214 - Copy.JPG (167.87 KiB) Viewed 568 times
IMG_0344 - Copy.JPG
IMG_0344 - Copy.JPG (199.3 KiB) Viewed 568 times
IMG_0391 - Copy.JPG
IMG_0391 - Copy.JPG (190.52 KiB) Viewed 568 times
IMG_0464 - Copy.JPG
IMG_0464 - Copy.JPG (181.82 KiB) Viewed 568 times
IMG_0468 - Copy.JPG
IMG_0468 - Copy.JPG (183.68 KiB) Viewed 568 times
Sale section etiquette, pls be courteous to other members, if you know of a better deal or do not agree with the sale price, do not shove links to similar products being sold by someone else in another member's post.. it's just not nice. If you suspect a scam pls FLAG the thread for moderation and it will be checked out... i know this is a tough one to call but put yourself in the seller's shoes and imagine how you would like it.

https://endless-sphere.com/forums/viewto ... 31&t=25446

User avatar
wineboyrider
100 MW
100 MW
Posts: 2929
Joined: Sep 30, 2009 9:08 am
Location: Tularosa, New Mexico
Contact:

Re: Razor E300s upgrade

Post by wineboyrider » Oct 28, 2017 1:10 pm

Do you still use the brushed motor too?
ES IS SAVED! THANK YOU JUSTIN.

User avatar
fechter
100 GW
100 GW
Posts: 11992
Joined: Dec 31, 2006 3:23 pm
Location: California Bay Area, USA

Re: Razor E300s upgrade

Post by fechter » Oct 28, 2017 2:30 pm

If you could fit another identical hub motor on the rear, that thing could really fly.
"One test is worth a thousand opinions"

User avatar
ElectricGod
100 kW
100 kW
Posts: 1447
Joined: Nov 01, 2015 5:24 pm

Re: Razor E300s upgrade

Post by ElectricGod » Oct 28, 2017 9:06 pm

Or since it's already set up with a chain drive to the back wheel, just buy an inrunner that will fit in the space of the original motor.
ElectricGod...it's a joke...don't take things so seriously folks!

XB-502 Moped:
https://endless-sphere.com/forums/viewt ... 0#p1222730

Currie scooter:
https://endless-sphere.com/forums/viewt ... 7#p1227407

Post Reply