TylerDurden wrote:you may find the night riding with electric power to be dreamlike


Hyena wrote:We're at the mercy of the chinese postal system at the moment but I'll have you zippying along with 199.9w of near silence very shortly







itchynackers wrote:Looks great. You may need some padding over that screw head inside the box. The screw could wear a hole in your batteries (bad news).


chairshaker wrote:Excellent looking job. Noticed that your mirrors look great. Are you happy with them and where did you get them.








Hyena wrote:ANOTHER bullet came off ? Damn that's some very poor QC on hobbyking's part, I'll be sure and give all the ones I use in future a good tug. One of those coming unstuck is a quick way to to burn out your cell level parallel harness - good think you're still waiting on 2!


Scruffoid wrote: if you have read it it takes 24 - 90 V input and they claim it draws 12W but the CA was saying 200W so needs some investigating.