my workshop burned down and then what happened

Liberatorbike

100 mW
Joined
Feb 3, 2012
Messages
38
https://www.youtube.com/watch?v=2y56uhCXLZM&t=4s

https://www.youtube.com/watch?v=xVFp2-BWdqo&t=44s


18238189_1361178703958941_7032692281227686052_o.jpg18237907_1368398999903578_7757301430952249487_o.jpg21270908_1489052261171584_791167646896082918_n.jpg21742909_1504048496338627_5940494942870217097_n.jpg
23722772_1557076954369114_3483950575916559634_n.jpg
 
Condolences. Looks like many creative art bike builds.
 
Was it during charge or in inactive state?
What kind of cells, BMS and manufacturer?

What a mess. My condolences.
 