Batteries vs Cold ☃

General Discussion about electric vehicles.
User avatar
changeissimple
1 mW
1 mW
Posts: 10
Joined: Oct 18, 2017 3:26 pm

Re: Batteries vs Cold ☃

Post by changeissimple » Dec 06, 2017 5:43 pm

I have been riding in 40F temperatures and am a bit new to the E-Bike scene. I have seen a performance dip on the battery at that temp- I am not worried about the performance . However I am worried about hurting the battery long term. Will charging and riding in these temps (40F) hurt or degrade the battery and the life of the battery?

User avatar
DrkAngel
10 GW
10 GW
Posts: 4508
Joined: Dec 15, 2010 11:14 am
Location: Upstate-Western-Southern Tier NY. USA

Re: Batteries vs Cold ☃

Post by DrkAngel » Dec 09, 2017 8:06 am

No definite answer on damaging, by discharging battery when cold ... but definite suppressed battery performance!
Charging when cold is detrimental!

Allow to warm near room temperature, then charge.

Put warm battery on bike for good initial performance.
A little learning is a dangerous thing;
Drink deep, or taste not the Pierian spring:
There, shallow draughts intoxicate the brain,
And drinking largely, sobers us again.

I enjoy enlightening ... and enlivening the spirit of the innovators.

New & Improved - Acronym Definitions

Index - Homemade Battery Packs - Updated - November 2015

EBike Toolbox - Bargains! $

Endless Sphere Wiki

User avatar
changeissimple
1 mW
1 mW
Posts: 10
Joined: Oct 18, 2017 3:26 pm

Re: Batteries vs Cold ☃

Post by changeissimple » Dec 12, 2017 12:43 pm

I put my bike in the basement for the winter just last week because of the snow and ice here in Boston. Wondering if anyone has a recommendation for maintaining the battery until spring. It is a 48v 26.1ah panasonic 13650 lithium ion pack. I have a 4amp charger. Should I charge it once a week, one a month? should I run the motor and drain the battery periodically? I'd love help on this issue. Maybe there is thread on maintaining the battery for a few months - love some help/recommendations.

User avatar
tomjasz
1.21 GW
1.21 GW
Posts: 3696
Joined: Mar 29, 2014 1:45 pm
Location: Out riding, MN USA
Contact:

Re: Batteries vs Cold ☃

Post by tomjasz » Dec 12, 2017 12:49 pm

changeissimple wrote:
Dec 12, 2017 12:43 pm
I put my bike in the basement for the winter just last week because of the snow and ice here in Boston. Wondering if anyone has a recommendation for maintaining the battery until spring. It is a 48v 26.1ah panasonic 13650 lithium ion pack. I have a 4amp charger. Should I charge it once a week, one a month? should I run the motor and drain the battery periodically? I'd love help on this issue. Maybe there is thread on maintaining the battery for a few months - love some help/recommendations.
Best stored at refrigerator, NOT fewer temps. Best I can do is 55F. Store at 50% charge. 46.8V.
Attachments
Screen Shot 2017-12-12 at 11.50.45 AM.png
Screen Shot 2017-12-12 at 11.50.45 AM.png (90.19 KiB) Viewed 135 times
Thanks Justin_le we're here thanks to you. All the best to the mods for their tireless work keeping it on an even keel.

User avatar
tomjasz
1.21 GW
1.21 GW
Posts: 3696
Joined: Mar 29, 2014 1:45 pm
Location: Out riding, MN USA
Contact:

Re: Batteries vs Cold ☃

Post by tomjasz » Dec 12, 2017 12:52 pm

Here's the complete chart.
Attachments
Screen Shot 2017-12-04 at 2.35.19 PM.png
Thanks Justin_le we're here thanks to you. All the best to the mods for their tireless work keeping it on an even keel.

Post Reply