Got something to sell? Have extra parts that need a good home? Have something that others would need to complete their kits? Post it up here and see if anyone else is searching for what you are selling. Guest may post replies to topics already here. All topics here will expire after 90 days of inactivity.
Post Reply
User avatar
Monstarr
100 W
100 W
Posts: 231
Joined: Apr 12, 2011 4:56 am
Location: The Netherlands

LG Chem 10S2P battery modules - 37V30Ah - 1100 wh [EU]

Post by Monstarr » Sep 05, 2017 8:56 am

New modules arrived.

These LG Chem built modules contain very high quality NMC pouch power parallel 15 ah cells from LG Chem configured in 37V30Ah - 10S2P order for 1100 Wh's of capacity. The rigid steel OEM casing provides excellent compression and has connection for watercooling system. It has a protective cover over the cell tabs and terminals and there is a direct balance lead connection and two connectors for the thermistors (blue wires) built in the pack.

Image
Image
Image
Image
Image
Balance pin-out of the 14 pin connector (Molex Microfit 3.0 - MX-43025-1400) - cable is not included.
1 X X X X 10 9
2 3 4 5 6 7 8

Cell 1 connect to - gives single cell voltage
Cell 10 connect to - gives full pack voltage

The same cells are also used for example in Opel Ampera/Chevy Volt/Renault Zoe packs. High discharge rating 10 C.
These modules are excellent for slim light-weight powerpacks in scooters, cargobikes etc.
Weighing around 10 KG.

The onboard electronics board is a cell voltage & temperature node and sends information by CAN bus to the pack's main hub.
It doesn't really have any value to DIY because you need to reverse engineer the whole protocol and CAN language. Besides, it will only tell you monitoring information. It can't shut down the power like a BMS can.

Dimensions:
130 mm wide
280 mm high
320 mm long (w/o coolant tubes 300 mm)

The modules currently have a storage voltage and are stored dry.
Modules are located in Breda, The Netherlands, Europe.
Shipping optional if possible. PM for more info.

Price:
1 module: € 175
2+ modules: € 150/pc
per 2 with original flexible high current interconnect for series connection.

As an example, in 1 of my projects I am using two of these modules in series in a Govecs (Gen4 @ 70A max discharge) scooter for more than 1,5 year now and they pack a punch. I only charge to 4,1 v/cel. Recently after a year of use I checked the voltages and they were all still perfectly balanced. Using almost daily for commuting. Few pleased customers already also are using these modules from previous sale threads.
For those interested: I also have the CAN operated EV Powerchargers IP67 chargers which came included with the packs. Charge voltage is a bit too high perhaps for ES -> 250 VDC - 420 VDC. They retail around 1200 €.
Price = € 200 / charger.


If any questions, feel free to ask.
Last edited by Monstarr on Nov 29, 2017 5:29 pm, edited 9 times in total.

User avatar
boisrondevens
100 W
100 W
Posts: 264
Joined: Jul 11, 2011 11:30 am
Location: Canada
Contact:

Re: LG Chem 10S2P modules - 37V30Ah - 1100 wh [EU]

Post by boisrondevens » Sep 05, 2017 1:56 pm

Can you ship to Canada?

User avatar
Monstarr
100 W
100 W
Posts: 231
Joined: Apr 12, 2011 4:56 am
Location: The Netherlands

Re: LG Chem 10S2P modules - 37V30Ah - 1100 wh [EU]

Post by Monstarr » Sep 05, 2017 2:48 pm

boisrondevens wrote:Can you ship to Canada?
No i am sorry. These modules can not be shipped by air unfortunately. At least afaik.

abahanad
10 W
10 W
Posts: 67
Joined: Apr 09, 2017 7:30 am

Re: LG Chem 10S2P modules - 37V30Ah - 1100 wh [EU]

Post by abahanad » Sep 06, 2017 4:17 am

hello,
they seem pretty good for my ebike build,
how much current can they handle (per pack)
will you ship to the UK?
nominal and max voltage per pack?

User avatar
Monstarr
100 W
100 W
Posts: 231
Joined: Apr 12, 2011 4:56 am
Location: The Netherlands

Re: LG Chem 10S2P modules - 37V30Ah - 1100 wh [EU]

Post by Monstarr » Sep 06, 2017 4:48 am

abahanad wrote:hello,
they seem pretty good for my ebike build,
how much current can they handle (per pack)
will you ship to the UK?
nominal and max voltage per pack?
Yeh, so most lithium chemistry's (NMC, NCA, LMO, LCO) range somewhat from 3 Volt empty to 4,2 Volt full. Some even higher, some a bit lower. LiFePO4 & LTO are another story, but that is not the case here.
Ideally, you want to charge to 4,0-4,1 Volt/cell most of the time to strongly increase cell longevity and don't discharge far below 3,5 Volt. There is very little energy left at that point anyway.
Image
More info on getting the most life of your cells as possible: http://batteryuniversity.com/learn/arti ... _batteries

So these cells offer 10 C according to LG Chem 15 Ah cell test reports. 10 C means 300 A @ 37 Volt which is pretty insane for a 10 KG package if you ask me.
That probably is the reason it has liquid cooling ;). Way way more current potential than any kind of LEV would need. So don't worry.

PHEV cells, which these are, are power cells. Which means their engineering emphasis lies on delivering high power instead of having a big wh per kg/energy ratio. This is because in PHEV the batterypack is relatively small compared to full electric vehicles but it still needs high power delivery capability to propel the mass of the car. These LG Chem cells are about 150 Wh/KG. In contrast modern Tesla Model S cells (NCA) are energy cells with 250 Wh / KG. This doesn't mean they are better, but they are different. Those Tesla cells don't offer very high C rating for example but rely on the packs cell masses for the super high ludicrous 1500 A current delivery.

I will send you a PM for the details on delivery.

mjar99
10 µW
10 µW
Posts: 6
Joined: Oct 22, 2014 9:33 am

Re: LG Chem 10S2P battery modules - 37V30Ah - 1100 wh [EU]

Post by mjar99 » Sep 11, 2017 2:17 am

Can they be reconfigured to 20s1p for ebike use?

User avatar
Monstarr
100 W
100 W
Posts: 231
Joined: Apr 12, 2011 4:56 am
Location: The Netherlands

Re: LG Chem 10S2P battery modules - 37V30Ah - 1100 wh [EU]

Post by Monstarr » Sep 11, 2017 2:56 am

mjar99 wrote:Can they be reconfigured to 20s1p for ebike use?
They are hard configured to 10s2p.
So no, not without any DIY effort.

Havin' said that, please check the second last photo. There you can see the parallel connections between the cellpairs.
You can pry these connection off of eachother and end up with 20 bare cells with long easy workable cell tabs. If you'd search in the large and famous A123 pouch cell topics from yesteryears you find out that a lot of hobbyists and inspiring professionals already figured out great solutions for these type of pouch cell battery builds.

Juwe
1 mW
1 mW
Posts: 12
Joined: Aug 05, 2017 11:55 am

Re: LG Chem 10S2P battery modules - 37V30Ah - 1100 wh [EU]

Post by Juwe » Sep 11, 2017 10:28 am

How much it is postage cost to Slovenia?

User avatar
Monstarr
100 W
100 W
Posts: 231
Joined: Apr 12, 2011 4:56 am
Location: The Netherlands

Re: LG Chem 10S2P battery modules - 37V30Ah - 1100 wh [EU]

Post by Monstarr » Sep 11, 2017 2:02 pm

Juwe wrote:How much it is postage cost to Slovenia?
Please pm how many modules. I will send you the price.

User avatar
wojtek
100 kW
100 kW
Posts: 1361
Joined: Nov 29, 2009 3:52 pm
Location: Luxembourg
Contact:

Re: LG Chem 10S2P battery modules - 37V30Ah - 1100 wh [EU]

Post by wojtek » Sep 14, 2017 4:13 pm

mjar99 wrote:Can they be reconfigured to 20s1p for ebike use?
+1
Would also be interested in plug and play 20s solution
WIRES AND CONNECTORS
https://endless-sphere.com/forums/vi ... 31&t=30176
https://endless-sphere.com/forums/viewto ... 31&t=32244

KMX Cobra with Xlyte 5403
Go-One Evo with Cromotor
BATMOBILE - Astro 3220 / Nuvinci in progress
Giant CRS Alliance - yes, just pushbike! frock you..
3Element Espire - SOLD
Custom built Specialized BigHit with BBS02 - SOLD
Velokraft e-VK3 SOLD
Steintrike Mungo Sport HS3540-SOLD
Scorpion FS HS3540-SOLD
Kona Dawg BMC v2-SOLD

999zip999
100 GW
100 GW
Posts: 8279
Joined: Jan 10, 2010 1:40 pm
Location: Dana Point So. Cal

Re: LG Chem 10S2P battery modules - 37V30Ah - 1100 wh [EU]

Post by 999zip999 » Sep 19, 2017 10:33 am

Would love a 20s 1p but think the tabs are laser welded and are shorted in the process. Looking for 15 -20 ah nmc cells 5c or better ?

User avatar
Monstarr
100 W
100 W
Posts: 231
Joined: Apr 12, 2011 4:56 am
Location: The Netherlands

Re: LG Chem 10S2P battery modules - 37V30Ah - 1100 wh [EU]

Post by Monstarr » Oct 08, 2017 9:01 am

Bump.
Got a few modules left.

User avatar
wojtek
100 kW
100 kW
Posts: 1361
Joined: Nov 29, 2009 3:52 pm
Location: Luxembourg
Contact:

Re: LG Chem 10S2P battery modules - 37V30Ah - 1100 wh [EU]

Post by wojtek » Oct 21, 2017 5:05 am

MSGed you.
ps. how old are those modules?
WIRES AND CONNECTORS
https://endless-sphere.com/forums/vi ... 31&t=30176
https://endless-sphere.com/forums/viewto ... 31&t=32244

KMX Cobra with Xlyte 5403
Go-One Evo with Cromotor
BATMOBILE - Astro 3220 / Nuvinci in progress
Giant CRS Alliance - yes, just pushbike! frock you..
3Element Espire - SOLD
Custom built Specialized BigHit with BBS02 - SOLD
Velokraft e-VK3 SOLD
Steintrike Mungo Sport HS3540-SOLD
Scorpion FS HS3540-SOLD
Kona Dawg BMC v2-SOLD

User avatar
Monstarr
100 W
100 W
Posts: 231
Joined: Apr 12, 2011 4:56 am
Location: The Netherlands

Re: LG Chem 10S2P battery modules - 37V30Ah - 1100 wh [EU]

Post by Monstarr » Oct 21, 2017 9:59 am

wojtek wrote:MSGed you.
ps. how old are those modules?
prod date 8-2013
Vehicle itself was from 2015 (don't know exact month). It had around 50 k km on the clock.
I will reply to your message, thanks :)

User avatar
Monstarr
100 W
100 W
Posts: 231
Joined: Apr 12, 2011 4:56 am
Location: The Netherlands

Re: LG Chem 10S2P battery modules - 37V30Ah - 1100 wh [EU]

Post by Monstarr » Nov 02, 2017 4:24 am

Got some new modules :)
Several happy ES users bought these to full performance satisfaction.
Lowest price, € 0,14 per Wh !

galderdi
1 kW
1 kW
Posts: 313
Joined: Sep 08, 2015 8:17 pm

Re: LG Chem 10S2P battery modules - 37V30Ah - 1100 wh [EU]

Post by galderdi » Nov 07, 2017 12:16 am

Hi,

Can you confirm, Is 37V the nominal voaltage? From what you have said that makes the pack 42V when fully charged?

Do you have 8 modules available?

I know you said there is no air freight for these. Are you able to provide surface freight to Australia?

If so how much for 8 modules?

User avatar
Monstarr
100 W
100 W
Posts: 231
Joined: Apr 12, 2011 4:56 am
Location: The Netherlands

Re: LG Chem 10S2P battery modules - 37V30Ah - 1100 wh [EU]

Post by Monstarr » Nov 07, 2017 4:44 am

galderdi wrote:Hi,

Can you confirm, Is 37V the nominal voaltage? From what you have said that makes the pack 42V when fully charged?

Do you have 8 modules available?

I know you said there is no air freight for these. Are you able to provide surface freight to Australia?

If so how much for 8 modules?
Hey,
Thanks for your interest. Unfortunately no shipping possibility outside EU. I am sorry.
FYI, li-ion NMC cell -> fully charged around 4.2 Volt. But main discharge takes place around 3.7-3.8 Volt. That way the refer to the nominal voltage for calculating batterypack sizes. As this module is 10 series that means nominal voltage around 37 Volt. A 48 Volt li-ion batterypack for example is 13 S which is 13x3.7/3.8 = 48.1-49.4-ish Volt.

User avatar
Monstarr
100 W
100 W
Posts: 231
Joined: Apr 12, 2011 4:56 am
Location: The Netherlands

Re: LG Chem 10S2P battery modules - 37V30Ah - 1100 wh [EU] -

Post by Monstarr » Nov 10, 2017 9:04 am

All modules gone.

User avatar
Monstarr
100 W
100 W
Posts: 231
Joined: Apr 12, 2011 4:56 am
Location: The Netherlands

Re: LG Chem 10S2P battery modules - 37V30Ah - 1100 wh [EU] -SOLD

Post by Monstarr » Nov 27, 2017 9:40 am

1 module left!

Post Reply