DC carries more power for a given time than AC.
0.1mm cu is doable with a .3ni capable machine
Slots are a given, and discussed elsewhere in detail
Thicker than .1mm cu requires so much power you are approaching the limit of the can to survive. Any minor misalignment etc results in a hole perforating your cell, though It can be done with techniques other than spotwelding.