The official "My Tidalforce S-750 frame creation" thread

Show off your E-bike creation here.

The official "My Tidalforce S-750 frame creation" thread

Postby oatnet » Sun Jul 26, 2009 10:53 pm

You have probably seen my thread in the For-Sale section for the Tidalforce S-750 Electric Bike frames. I had hoped to manufacture my own line of ebikes with them, but since I decided to sell them, I am instead living vicariously through people who bought them, encouraging them to post pictures of their creations on the for-sale thread. With the wide and varied imaginations of everyone here, I can't wait to see what people come up with.

Someone reminded me today that when I eventually run out of frames the for-sale thread will expire and scroll off the site, so I thought I'd make an 'official' thread that will be permanent, show the variety, and give people a place to exchange ideas. So I'll get the ball rolling by posting some of the pics I have seen, there are dozens and dozens and dozens of these frames out there now, so I hope everyone will post their builds, wild or mild, so we can see the results!

-JD

This is one of my favorite pictures of an early x5 prototype, taken at a local beach:
Image

Here is my old xtracycle prototype, freshly updated with a 2004 Rock Shox Boxxer fork
Image
Image

Here is ianmcnally2's version (ian you gotta dump that tape and run the cables through the channels inside the frame :D ) :
Image

Today I heard from a guy named Jerry who is living out my dream, and building ebikes for sale from the frames. Not only did he do a really clean build, but what really floored me were the Decals he made for the bikes. Apparently his 'day' job is doing graphics, and he was concerned about the legal ramifications of selling ebikes with the Tidalforce logo, so he came up with these amazing Decals that look good as well as covering up the logo. I don't think he is on Endless-Sphere at the moment, if you want to contact him to get some graphics made, drop me a PM with your email addy and I will forward it on to him.


(Note: yes, this does have a front motor on a suspension fork, which I DO NOT recommend or endorse or condone, as I have had an aluminum suspension fork fail on me, fast, and I was very lucky that I was doing a slow turn and had room to roll after the fall.

Jerry reports that he is using a STEEL suspension fork, I warned him I do not recommend using a hub motor on ANY suspension fork, but he feels comfortable with it. I don't have any experience with steel suspension forks, but just to be safe I would still recommend using only a rear motor or a strong, solid, steel, conventional fork without suspension. I still believe that using a hub motor with any suspension fork could result in injury or death, and I believe that Jerry will take my advice on his future builds.)

Image

Image



And as is typical, Ypedal takes the prize for the most imaginative setup to date, going the RC route using one of recumpence's absolutely BEAUTIFULLY machined 2-stage gear reductions to drive a Nuvinci hub on 20" wheel (instead of the 26" these frames were made for).

Image

Image




(ignore the shrunk copies below of full-size photos posted above.)
Attachments
wind-runner 1.jpg
wind-runner 2.jpg
Last edited by oatnet on Sun Aug 09, 2009 10:58 pm, edited 2 times in total.
Member 117 of 16,xxx

179v VW Camper © 164v Vectrix E-Moto © 72v Norco A-line/x5403 © 60v Specialized Enduro Comp/BMC © 72v x5tracycle © 48v TF IO/BMC © 36v Kepler Friction Drive © Spot-Welding a123 © Pelican Front Packs © Vectrix Battery Replacement © MORE !!


Image大鸡巴 Motors
Knowledge is acquired through experience, everything else is just information - Albert Einstein
"Cheater?" I'm not competing, I'm Commuting!
User avatar
oatnet
100 MW
100 MW
 
Posts: 2507
Joined: Thu Apr 26, 2007 3:03 pm
Location: SoCal, USA

Re: The official "My Tidalforce l S-750 frame creation" thread

Postby Ypedal » Mon Jul 27, 2009 6:18 am

Slight edit, ( I changed it already for you ) the rear wheel is 20", the front is 24 ! :wink:
ES site status page, for when "things" happen...
http://www.ypedal.com/ES/ES.htm
----------------
Always Staying Busy !!
http://www.ypedal.com/Projects.htm
User avatar
Ypedal
100 GW
100 GW
 
Posts: 11916
Joined: Wed Dec 27, 2006 12:55 pm
Location: Moncton NB, Canada

Re: The official "My Tidalforce S-750 frame creation" thread

Postby ambroseliao » Mon Aug 24, 2009 11:48 am

After many months of fits and starts interrupted by many life events, I was finally able to complete my Tidalforce S750 (S-750) front hub motor build using a eBikeKit.com front hub motor and a V.Power.hk 36V 20AH LiFEPo4 battery from eBay. The S750 frame came from Deerfencer1 and the components came mostly from Oatnet here on the EndlessSphere.com forums. I bought the frame right before Oatnet posted his ad for his S-750 components.

I've posted some pictures here:
http://picasaweb.google.com/ambroseliao/TFPix#
Click on the slideshow button near the upper left hand corner for easier viewing of the photos.

I've not ridden it much except last night as a test run after wiring up all of the electronics. It's very smooth and quiet. It feels a bit heavy because of the rear rack mounted 20 lb battery. I'm sure I'll get used to it. The Schwalbe Big Apple 2.35" tires give an exceptionally smooth quiet ride I may need to pump it up a bit more to give it a stiffer ride, actually. I plan to use the bike as my daily commuter to work.

Total cost for all parts and some assembly at the LBS are right around $1,000. Cost was a major factor. The challenge was another factor. I wanted to learn as much as possible from this build and to also build it exactly as I wanted it. I plan on updating it possibly with a rear hub motor in the future and perhaps a smaller/lighter battery. Considering that Tidalforce was selling this bike with an 8AH front hub battery and rear 750W motor for $2,800-2,900. I think this is quite a good deal for a solid ebike.

I want to thank Oatnet for posting his horde of parts since it made it very easy to get almost everything that I needed in one shot. His advice on the fork and other items was also very helpful. Thanks!

Comments welcome.

Ambrose
Attachments
IMG_0522.JPG
http://www.ebikes.ca/ for the best in ebike knowledge and equipment.

Tidalforce S-750, TidalForce iO Cruiser, 2x TidalForce M-750. Crystalyte HS3540 sensorless, 72V 45A Crystalyte SL controller, ebikes.ca DrainBrain & Cycle Analyst meters. GoPro HD Hero2 camera. A123 20Ah batteries. 88.2V 10Ah LiPO. My blog: http://ebikerider.blogspot.com
Remember LiFEPo4 HVC is 3.65V and LVC is 2.7V
User avatar
ambroseliao
100 kW
100 kW
 
Posts: 1230
Joined: Mon Apr 27, 2009 3:34 pm
Location: Washington, DC, USA area

Re: The official "My Tidalforce S-750 frame creation" thread

Postby oatnet » Sun Aug 30, 2009 8:33 pm

ambroseliao wrote:After many months of fits and starts interrupted by many life events, I was finally able to complete my Tidalforce S750 (S-750) front hub motor build using a eBikeKit.com front hub motor and a V.Power.hk 36V 20AH LiFEPo4 battery from eBay. The S750 frame came from Deerfencer1 and the components came mostly from Oatnet here on the EndlessSphere.com forums. I bought the frame right before Oatnet posted his ad for his S-750 components.


Nice Job, Ambrose! :D

Have you been able to start commuting on it? I know I get to work with a smile on my face from the ebike-commute. My knee has been bugging me for a few weeks, so I haven't been able to ride, I really miss it.

-JD
User avatar
oatnet
100 MW
100 MW
 
Posts: 2507
Joined: Thu Apr 26, 2007 3:03 pm
Location: SoCal, USA

Re: The official "My Tidalforce S-750 frame creation" thread

Postby aaronski » Mon Aug 31, 2009 12:01 am

oatnet wrote: My knee has been bugging me for a few weeks, so I haven't been able to ride, I really miss it.

-JD


Hi JD, I just thought I'd chime in on the knee issue. I have torn the ligaments in my knees when I was much younger and they never got better. I got the ebike to mitigate the stresses biking puts on them. When I first started ebiking I had the seat about 1/2 inch too low and developed terrible knee pain over the course of the week. I moved the seat up 1/2 inch, back about 1/4 inch, and tilted it down about 5 degrees and the pain has vanished. it also seems to help me if I try and keep the knees close to the bike as I pedal. Just my two cents to try and help someone out. I was shocked that sizing the bike that slight difference could make such an change!
Broken bike and electric bits everywhere. Some times it's a bike and I ride it.
Have:bmc 9c, bafang, lifepo4,lipo, konions, infineon ctrlrs
Smoked:bmc,9c,bafang, lifepo4,lipo, infineons
Konions appear to be bulletproof...
aaronski
1 kW
1 kW
 
Posts: 362
Joined: Thu Jul 09, 2009 4:43 am
Location: San Francisco,ca

Re: The official "My Tidalforce S-750 frame creation" thread

Postby ambroseliao » Tue Sep 01, 2009 1:05 pm

Hi JD,

Yes, I've been commuting on it since yesterday. It is indeed a blast. My commute is just about perfect for me. It's 8 miles slightly downhill on the way in to Washington, DC and it's uphill (of course) on the way home. I think I overestimated my power requirements so have a huge 20AH battery when I only use about 4AH on my way in and about 4.5 on my way home. I'm thinking of getting a 48V 10AH battery to increase the top speed and reduce the weight of the bike which is a bit top heavy.

I'm also thinking about bike lighting since daylight is ending sooner and morning light is coming later. I see you have some small lights on your bike. Do they work well for you?

Ambrose
http://www.ebikes.ca/ for the best in ebike knowledge and equipment.

Tidalforce S-750, TidalForce iO Cruiser, 2x TidalForce M-750. Crystalyte HS3540 sensorless, 72V 45A Crystalyte SL controller, ebikes.ca DrainBrain & Cycle Analyst meters. GoPro HD Hero2 camera. A123 20Ah batteries. 88.2V 10Ah LiPO. My blog: http://ebikerider.blogspot.com
Remember LiFEPo4 HVC is 3.65V and LVC is 2.7V
User avatar
ambroseliao
100 kW
100 kW
 
Posts: 1230
Joined: Mon Apr 27, 2009 3:34 pm
Location: Washington, DC, USA area

Re: The official "My Tidalforce S-750 frame creation" thread

Postby oatnet » Tue Sep 01, 2009 7:34 pm

ambroseliao wrote:Hi JD,

Yes, I've been commuting on it since yesterday. It is indeed a blast. My commute is just about perfect for me. It's 8 miles slightly downhill on the way in to Washington, DC and it's uphill (of course) on the way home. I think I overestimated my power requirements so have a huge 20AH battery when I only use about 4AH on my way in and about 4.5 on my way home. I'm thinking of getting a 48V 10AH battery to increase the top speed and reduce the weight of the bike which is a bit top heavy.

I'm also thinking about bike lighting since daylight is ending sooner and morning light is coming later. I see you have some small lights on your bike. Do they work well for you?

Ambrose


Cool, glad you are getting out there, one more car off the road <grin>

Because of that top-heavy effect, I don't use rack-top mounted packs. I like to put my batteries in side panniers, with the pack split in half for balance. This puts the mass right above the axle. It still leaves the bike tail-heavy, but unless you do a triangle pack or a Tidalforce in-front-wheel battery, that's the way it is.

The lights you see above are 1w LED lights I used to buy at a local swapmeet. They are just OK, and I use rechargable cells in them. I've heard good things about Justin's (ebikes.ca) lights, that can handle up to 100v so you can wire in parallel with your main battery pack, good illumination with no batteries required.

-JD
User avatar
oatnet
100 MW
100 MW
 
Posts: 2507
Joined: Thu Apr 26, 2007 3:03 pm
Location: SoCal, USA

Re: The official "My Tidalforce S-750 frame creation" thread

Postby oatnet » Tue Sep 01, 2009 7:45 pm

Here are pics of more builds by Jerry, who reports:

"Here's the BMC 400 watt version with the Topeak bag/rack system. Its finally feeling like the solid town vehicle/commuter that I envisioned at the start. I am very happy with the performance of the motor. Its an excellent hill climber that's much quieter than my Heinzmann."

-JD
Attachments
IMG_0283.JPG
IMG_0288.JPG
IMG_0302.JPG
IMG_0305.JPG
User avatar
oatnet
100 MW
100 MW
 
Posts: 2507
Joined: Thu Apr 26, 2007 3:03 pm
Location: SoCal, USA

Re: The official "My Tidalforce S-750 frame creation" thread

Postby ambroseliao » Sat Sep 05, 2009 8:39 am

Thanks JD for the info on your lights. I was looking at small add-on bike lights but decided on the Dealextreme.com 900 lumen P7 light for $70. These are very bright and come with a Li-ion battery pack and charger. They were initially very suspect, but they have improved their quality and fixed a couple of issues recently. I'm waiting for it to arrive soon.
http://www.dealextreme.com/details.dx/sku.25149

I'm also looking at these for tail lights.
http://www.dealextreme.com/details.dx/sku.3639

Lastly, I'm looking at a Planet Bike Superflash light for my helmet.
http://www.rei.com/product/756360
these are on sale this weekend at REI.

I WANT TO BE VISIBLE! :-)

*I'm not associated with any of these companies. Just a happy customer.
http://www.ebikes.ca/ for the best in ebike knowledge and equipment.

Tidalforce S-750, TidalForce iO Cruiser, 2x TidalForce M-750. Crystalyte HS3540 sensorless, 72V 45A Crystalyte SL controller, ebikes.ca DrainBrain & Cycle Analyst meters. GoPro HD Hero2 camera. A123 20Ah batteries. 88.2V 10Ah LiPO. My blog: http://ebikerider.blogspot.com
Remember LiFEPo4 HVC is 3.65V and LVC is 2.7V
User avatar
ambroseliao
100 kW
100 kW
 
Posts: 1230
Joined: Mon Apr 27, 2009 3:34 pm
Location: Washington, DC, USA area

Re: The official "My Tidalforce S-750 frame creation" thread

Postby El_Steak » Mon Sep 28, 2009 2:23 pm

I don't know if this bike was created by an ES member, I just found the picture while going a google image search for inspiration.

I really like the road bike handles look on a MTB frame
2 motors ???
BIG front crank
What is that thing on the front? a mudguard?

Image
TidalForce S-750 frame
Rear 2807 in a 24" wheel fed by a Methods 100V 100A controller
LiPo config: 24s3p 15ah
All the details here: viewtopic.php?f=6&t=17166
User avatar
El_Steak
10 kW
10 kW
 
Posts: 643
Joined: Tue Aug 11, 2009 8:33 pm
Location: Gatineau, Quebec

Re: The official "My Tidalforce S-750 frame creation" thread

Postby StudEbiker » Mon Sep 28, 2009 5:20 pm

I remember seeing that bike somewhere on the web. IIRC, he took some part off of a scooter and is using it as a fender, but is also using it to house the controller. I may be wrong, but there was definitely some reason he was doing it. Can't say I really enjoy the look of it though.......probably worth a couple of 40ozs. on here for sure. :lol:
TidalForce S-750-(build #2) w/9C rear w/EV Components Headway 36v 10ah LiFePo4 pack: http://endless-sphere.com/forums/viewtopic.php?f=6&t=15443&hilit=+headway+rack+pack

Bike-E (Build #3, mostly done)- 400W Kollmorgen mid-drive: http://endless-sphere.com/forums/viewtopic.php?f=28&t=25980#p375646
My Bike E Facebook group: http://www.facebook.com/groups/165756106813440/

"Facts do not cease to exist because they are ignored" - Aldous Huxley
User avatar
StudEbiker
10 MW
10 MW
 
Posts: 2260
Joined: Mon Apr 13, 2009 2:15 pm
Location: Ashland, OR, USA

Re: The official "My Tidalforce S-750 frame creation" thread

Postby El_Steak » Tue Sep 29, 2009 8:18 pm

Alright, it still a work in progress, but I've started building my Tidalforce S-750 bike. I went with an entry-level Marzochi fork. It's heavier than others and might not take a 6-foot drop too keenly but for urban riding it should be great. Plus the colors are a good match for the frame ;)

I also went with 2.5" x 26" Hookworms and a decent Mavic 321 front wheel.

I've ordered a rear 2806 from Justin at ebikes.ca (re-laced properly to eliminate the offset). I took a 7 speed cassette (with axle washers) and a threaded chinese disk brake. I have some doubts that it will all fit between the rear dropouts, especially for the disk brake as I think it might rub on the big square torque arm "notch" on the frame. Was anybody here able to use a rear disc brake with that frame and a 9c motor ?

Image
TidalForce S-750 frame
Rear 2807 in a 24" wheel fed by a Methods 100V 100A controller
LiPo config: 24s3p 15ah
All the details here: viewtopic.php?f=6&t=17166
User avatar
El_Steak
10 kW
10 kW
 
Posts: 643
Joined: Tue Aug 11, 2009 8:33 pm
Location: Gatineau, Quebec

Re: The official "My Tidalforce S-750 frame creation" thread

Postby Ypedal » Wed Sep 30, 2009 12:35 am

Attachments
RCdone.JPG
RCdone.JPG (74.69 KiB) Viewed 3916 times
ES site status page, for when "things" happen...
http://www.ypedal.com/ES/ES.htm
----------------
Always Staying Busy !!
http://www.ypedal.com/Projects.htm
User avatar
Ypedal
100 GW
100 GW
 
Posts: 11916
Joined: Wed Dec 27, 2006 12:55 pm
Location: Moncton NB, Canada

Re: The official "My Tidalforce S-750 frame creation" thread

Postby will_newton » Thu Nov 26, 2009 4:59 pm

OK, so it didn't become an e-bike, but it is my daughter's xmas gift this year!
Attachments
s750.jpg
s750.jpg (22.67 KiB) Viewed 3617 times
Adult sized E-kick Scooter- Self-made frame, NC1606 front hub, 48V 10 ah lipo (12S) Hidden build thread in the E-S Beer section!
-highly stalled build-- Electric Big Dummy ---
Methods/9c/e-bikekit rear, Methods 100V/100A controller, 12S 10ah Flightmax lipos for testing only-final pack TBA
E-Cannondale MTB/commuter w/front WE BD36, 35A controller, 44V 20 ah lipos (11s). yeah, it's brushed, but it goes EVERY time I hit the throttle, K.I.S.S!
User avatar
will_newton
1 kW
1 kW
 
Posts: 381
Joined: Sat May 02, 2009 11:51 am
Location: nc, usa

Re: The official "My Tidalforce S-750 frame creation" thread

Postby Amonk » Sat Nov 28, 2009 6:50 pm

I wanted to post a few pictures of what I have done with the frame so far.An E-bikekit front hub is on the way.I also wanted to thank Oatnet.He has been great to deal with.Very good comunication and fast shipping.
IMG_0118.JPG
IMG_0118.JPG (221.8 KiB) Viewed 3897 times
Attachments
IMG_0119.JPG
IMG_0119.JPG (209.01 KiB) Viewed 3878 times
IMG_0120.JPG
IMG_0120.JPG (235.75 KiB) Viewed 3877 times
Amonk
10 mW
10 mW
 
Posts: 30
Joined: Fri Jun 26, 2009 8:36 am
Location: Nashville.TN.

Re: The official "My Tidalforce S-750 frame creation" thread

Postby Amonk » Sun Dec 20, 2009 4:22 pm

Here are the newest pictures of my TidalForce S-750 build.I used a E-bikeKit 6*10 (2806) front hub.It seems like it is going to be a good hill climber.
Attachments
IMG_0121.JPG
IMG_0121.JPG (166.29 KiB) Viewed 1641 times
IMG_0122.JPG
IMG_0122.JPG (181.85 KiB) Viewed 1781 times
IMG_0123.JPG
IMG_0123.JPG (188.05 KiB) Viewed 1778 times
Amonk
10 mW
10 mW
 
Posts: 30
Joined: Fri Jun 26, 2009 8:36 am
Location: Nashville.TN.

Re: The official "My Tidalforce S-750 frame creation" thread

Postby Kevinator » Fri Mar 12, 2010 2:00 am

Lots of great builds, but I especially enjoyed Ypedal's video with the RC motor ride. That was inspiring. :mrgreen:
Kevin's "K7 Clown Bike" - 2009 Dahon Boardwalk S1 on steroids, crack, and mountain dew.

Build thread: http://www.bikeforums.net/showthread.ph ... ner!/page2
Kevinator
100 W
100 W
 
Posts: 170
Joined: Tue Feb 02, 2010 1:21 pm

Re: The official "My Tidalforce S-750 frame creation" thread

Postby Kevinator » Fri Mar 12, 2010 10:48 pm

I did some work on my silver frame today. I installed a Suntour Raidon 120mm air fork, headset, stem, and handlebars. I was lucky and had enough headset spacers to install everything without having to cut the steer tube. I borrowed the 26" wheels from another bike to get a better idea of sizing.

IMGA0463.JPG
TF1
IMGA0463.JPG (126.76 KiB) Viewed 1387 times

IMGA0465.JPG
TF2
IMGA0465.JPG (122.11 KiB) Viewed 1387 times

IMGA0468.JPG
TF3
IMGA0468.JPG (118.24 KiB) Viewed 1387 times
Kevin's "K7 Clown Bike" - 2009 Dahon Boardwalk S1 on steroids, crack, and mountain dew.

Build thread: http://www.bikeforums.net/showthread.ph ... ner!/page2
Kevinator
100 W
100 W
 
Posts: 170
Joined: Tue Feb 02, 2010 1:21 pm

Re: The official "My Tidalforce S-750 frame creation" thread

Postby StudEbiker » Sat Mar 20, 2010 11:24 pm

God I've been waiting so long to post to this thread. Not quite done yet, but I did take it for a ride today so I think I will put up some pics. 8)

almostdone1.JPG


almostdone3.JPG
almostdone3.JPG (246.02 KiB) Viewed 1356 times
TidalForce S-750-(build #2) w/9C rear w/EV Components Headway 36v 10ah LiFePo4 pack: http://endless-sphere.com/forums/viewtopic.php?f=6&t=15443&hilit=+headway+rack+pack

Bike-E (Build #3, mostly done)- 400W Kollmorgen mid-drive: http://endless-sphere.com/forums/viewtopic.php?f=28&t=25980#p375646
My Bike E Facebook group: http://www.facebook.com/groups/165756106813440/

"Facts do not cease to exist because they are ignored" - Aldous Huxley
User avatar
StudEbiker
10 MW
10 MW
 
Posts: 2260
Joined: Mon Apr 13, 2009 2:15 pm
Location: Ashland, OR, USA

Re: The official "My Tidalforce S-750 frame creation" thread

Postby oatnet » Sun Mar 21, 2010 10:20 pm

Hey congrats stud, that build is looking great! Isn't it nice to get it out and about? BTW - it is NEVER finished. :shock: :oops: :D

-JD
User avatar
oatnet
100 MW
100 MW
 
Posts: 2507
Joined: Thu Apr 26, 2007 3:03 pm
Location: SoCal, USA

Re: The official "My Tidalforce S-750 frame creation" thread

Postby El_Steak » Wed Mar 24, 2010 8:56 pm

Here's mine.

You can get more pics and info in this thread: viewtopic.php?f=6&t=17166

Image
TidalForce S-750 frame
Rear 2807 in a 24" wheel fed by a Methods 100V 100A controller
LiPo config: 24s3p 15ah
All the details here: viewtopic.php?f=6&t=17166
User avatar
El_Steak
10 kW
10 kW
 
Posts: 643
Joined: Tue Aug 11, 2009 8:33 pm
Location: Gatineau, Quebec

Re: The official "My Tidalforce S-750 frame creation" thread

Postby Amonk » Sat May 08, 2010 7:04 pm

Here are some pics of my new Tidalforce build with one of the rear geared E-bikekits.I really like the front and rear disc brakes(no mods to the frame or the caliper mount).Thanks Again Oatnet for the great deal on the frames. :D
Attachments
IMG_0139.JPG
IMG_0139.JPG (184.57 KiB) Viewed 1383 times
IMG_0140.JPG
IMG_0140.JPG (203.05 KiB) Viewed 1386 times
IMG_0138.JPG
IMG_0138.JPG (207.92 KiB) Viewed 1383 times
IMG_0137.JPG
IMG_0137.JPG (151.76 KiB) Viewed 1386 times
Amonk
10 mW
10 mW
 
Posts: 30
Joined: Fri Jun 26, 2009 8:36 am
Location: Nashville.TN.

Re: The official "My Tidalforce S-750 frame creation" thread

Postby ambroseliao » Tue May 11, 2010 12:38 pm

That is a very stealthy little motor. How does it perform? Can you compare it to any other motors out there? Does it make much noise?

Thanks,
Ambrose
http://www.ebikes.ca/ for the best in ebike knowledge and equipment.

Tidalforce S-750, TidalForce iO Cruiser, 2x TidalForce M-750. Crystalyte HS3540 sensorless, 72V 45A Crystalyte SL controller, ebikes.ca DrainBrain & Cycle Analyst meters. GoPro HD Hero2 camera. A123 20Ah batteries. 88.2V 10Ah LiPO. My blog: http://ebikerider.blogspot.com
Remember LiFEPo4 HVC is 3.65V and LVC is 2.7V
User avatar
ambroseliao
100 kW
100 kW
 
Posts: 1230
Joined: Mon Apr 27, 2009 3:34 pm
Location: Washington, DC, USA area

Re: The official "My Tidalforce S-750 frame creation" thread

Postby Amonk » Tue May 11, 2010 6:56 pm

The motor is actually very quite.This is my first rear installation and also my first geared hub.It seems to have pretty good take off and pulls hills reasonably well ,about the same as my 2807 front hub(@ 36 v).The top end with the controller that came with this kit is about 17.5 mph.I Have plans to upgrade later to a stock E-bikekit(infineon 22A) controller.I think then I would get similar performance to the 2807 hub,and this would also allow me to run it at 48v.I will try to give a comparison once I upgrade it and get a CA on this bike. P.S One pleasant suprise was the ease of installation.I was able to mount BB7 disc brakes and rotor(6")with no mods to the frame, caliper mount ,or hub.All I had to do was mount the torque washer on the inside of the frame with the tabs facing out,and I think that I have room for a 7sd freewheel. :D
Amonk
10 mW
10 mW
 
Posts: 30
Joined: Fri Jun 26, 2009 8:36 am
Location: Nashville.TN.

Re: The official "My Tidalforce S-750 frame creation" thread

Postby El Duderino X » Tue May 18, 2010 5:02 am

IMG_0003b.jpg
(160.95 KiB) Downloaded 3 times


99.9% done!
One Tidalforce S-750 frame equipped with Salsa Cromo 29" front fork, a 700C eZee geared front hub, Shimano Alfine rear hub and Avid BB7 disc brakes all around (and no frame trimming). I've tidied it up a bit since this pic was taken adding a full front fender, Cygolite Dual Cross Pro front LED lights and a whole lot of zap straps.

Thanks again for the frames, JD, this has been a heck of a learning experience. Next up: The Tidalforce S-750/BionX bike!

B!
El Duderino X
10 µW
10 µW
 
Posts: 5
Joined: Mon Feb 02, 2009 8:18 pm

Next

Return to E-Bike Photos & Video

Who is online

Users browsing this forum: Brute, craigjh, cruzxia, Hyena and 12 guests