Sounds like a solid plan to me Kurt. Many do permanently paralell thier packs in to pairs or whatever. You can connect them permanently in the method of your choice, be it solder, paralell adapters, whatever.

I leave mine seperated and use andersons for the connections so I have the maximum adaptability. I run the same batts on all kinds of different bikes, and constantly experiment with new ones.

I think the 12s configuration is nearly perfect for a bike to be ridden daily. Very simple to rig up to connect in series to ride, then disconnect and use the same plugs to charge in 6s by putting the appropriate connector on your two chargers. Only slightly more complicated than a typical lifepo4 charger.

Link to one decent way to rig two chargers. What charger you use is not the key, but rather buying something that can use most of the capacity of the commonly avaliable 350 watt power supplies. So two 150 watt chargers works good, or a 300 watt charger than can do 12s, etc.

viewtopic.php?f=14&t=25005

Link to a good charger store in the US.

http://epbuddy.com/index.php?main_page= ... h9lp913q46
THE LIPO RULES. NEVER ABOVE 4.3V NEVER BELOW 2.7V DON'T PUNCTURE

Ideal charging /discharging range for Lipo, 3.65v minimum 4.1v maximum

See battery technology section, FAQ thread at the top of the page for lipo noob info.
User avatar
dogman
100 GW
100 GW
 
Posts: 22045
Joined: Sat May 17, 2008 12:53 pm
Location: Las Cruces New Mexico USA

Re: lipo noob questions

Postby chroot » Wed Feb 09, 2011 12:35 pm

I am going rid anderson connectors for good. I am tired when the initial spark *GUARANTEED* the anderson contact will melt or molten, and it will destroy themselve. ARGH! I may have follow GCinDC's style using 4mm or 5mm bullet connectors. These capable support 100A since my setup is pretty over 100A very often cause destroyed anderson connectors 4th times so far. :( :x :roll:

Only I would use anderson if it's minimal ampere like under 45A should be ok but not 100A.

PS. GCinDC setup is pretty much same setup on my ebike.
Thank you Justin Lemire-Elmore - You are a HERO!

Tidalforce, Yuba Mundo V4 Cargo bike, Juiced Riders ODK V1 Cargo bike
English is my secondary language - ASL (American Sign Language) is my primary.
chroot
100 kW
100 kW
 
Posts: 1481
Joined: Sun Nov 29, 2009 4:03 pm

Re: lipo noob questions

Postby dogman » Wed Feb 09, 2011 3:44 pm

Yeah, andersons for 100 amps requires too expensive connectors compared to others. Gold plated bullets are fairly cheap, and have tons of contact area.

BTW Kurt, that charger store has lots of neat paralell harnesses. Maybe use that for the balance wires, and you could unplug it and monitor individual cells from time to time. In practice, you tend to know though, it's the puffy cell every time. Break em in first too, before soldering up stuff. If you should get a stinker, you haven't wasted time, and could even get warantee if bought from the us warehouse.
THE LIPO RULES. NEVER ABOVE 4.3V NEVER BELOW 2.7V DON'T PUNCTURE

Ideal charging /discharging range for Lipo, 3.65v minimum 4.1v maximum

See battery technology section, FAQ thread at the top of the page for lipo noob info.
User avatar
dogman
100 GW
100 GW
 
Posts: 22045
Joined: Sat May 17, 2008 12:53 pm
Location: Las Cruces New Mexico USA

Re: lipo noob questions

Postby amberwolf » Wed Feb 09, 2011 3:58 pm

Well, if you use a connector designed for 45A max at 100A, I'd expect to have problems. ;)

Anderson also makes both Powerpoles and Multipoles for use at higher currents, up to several hundred amps, but they are physically larger to handle that current.

The bullet connectors aren't as physically large because their contact surface is not a flat plane, which is what makes the Andersons larger for similar current ratings.
House Fire Updates Thread


Got a question that isn't personal or private? Post it in the forums, don't PM it. ;)

Wiki your techy info so it doesn't get old, lost and icky:
http://endless-sphere.com/w


Full-Suspension Semi Recumbent Cargo Bike - NuVinci MidDrive
Semi-Recumbent Recycled-Parts Cargo eBike: "CrazyBike2"
DayGlo Avenger, MkII
User avatar
amberwolf
100 GW
100 GW
 
Posts: 13719
Joined: Mon Aug 17, 2009 6:43 am
Location: Phoenix, AZ, USA, Earth, Sol, Local Bubble, Orion Arm, Milky Way, Local Group

Re: lipo noob questions

Postby Emoto » Sun Jun 10, 2012 2:06 pm

Dogman, or any one, ive been reading but cant find my answer if i had 6s 5000 mah 20c lipo in a 18s 10ah 2p cofig [ 6 6s 5000 mah 20c's ] if a 20c a single 6s can deliver 100 amps.

So if i construct the 18s pack can i divide the amp draw say 60amps buy 3 or 2.
Edit my guess 2
Just a quick flight http://vimeo.com/30385026
User avatar
Emoto
100 W
100 W
 
Posts: 136
Joined: Mon Jun 13, 2011 9:31 am
Location: Australia

Previous

Return to Battery Technology

Who is online

Users browsing this forum: Bing [Bot], DrkAngel and 6 guests