Postby SamTexas » Thu May 05, 2011 10:26 pm

I have heard so much about the incredible self-balancing property of 18650v (apparently used in Makita packs) . Does anyone know where I can get a manufacturer's data sheet that describes that property? Thanks.

Sam

Edit: Original title "Data sheet for SELF-BALANCING 18650V" changed.
Last edited by SamTexas on Thu May 12, 2011 12:22 am, edited 3 times in total.
SamTexas
100 MW
100 MW
 
Posts: 2841
Joined: Wed Dec 29, 2010 5:34 am
Location: Houston, Texas

Re: Data sheet for SELF-BALANCING 18650V

Postby CamLight » Thu May 05, 2011 10:53 pm

SamTexas wrote:I have heard so much about the incredible self-balancing property of 18650v (apparently used in Makita packs) . Does anyone know where I can get a manufacturer's data sheet that describes that property? Thanks.

Sam

No cell can self-balance as no cell can be aware of the SOC and resting voltage of the other cells. Has never happened and never will. So you won't be able to find any data on this. :)

Having said that, there are some cells that are manufactured to tighter physical tolerances using chemicals also having tighter manufacturing control over their content (i.e., they're "purer"). These cells will, of course, go out of balance eventually but the tighter manufacturing control helps to extend the time they will take to get out of balance enough to be a problem.

Essentially, the cells that are purported to be "self-balancing" are just better matched due to tighter control during manufacture. They will all drift and age, but often at a slower rate than others and will tend to do so as a group and not all over the place as often happens when using other cells. But, of course, this is only true if pack assembly doesn't impact the cell-to-cell uniformity....which it does. :mrgreen:

Only testing can help each user to decide if a pack using these cells will stay balanced long enough to not exceed whatever limits we set for pack performance.
John M.
Owner
CamLight Systems
CamLight
10 kW
10 kW
 
Posts: 728
Joined: Sat Dec 13, 2008 8:51 pm
Location: New York City, USA

Re: Data sheet for SELF-BALANCING 18650V

Postby Doctorbass » Thu May 05, 2011 11:57 pm

Here is the TRUE specs i found on the internet back in 2007.

They was erased from the website few weeks after.

As far as i know.. .I remain the only source of these specs over the internet :lol:

They made a mistake.. at 1C the Wh IS 5.61Wh... not 3.61Wh... just pay attention to that to avoid confusion....

Here it is:
:wink:

Doc
Attachments
spec complet de la 18650V1 (des Makita).pdf
Konion 18650V ORIGINAL spec from BMZ
(154.45 KiB) Downloaded 125 times
________________
-Fastest speed record from now: 113 km/h measured on GPS
-Fastest ebike 106km/h on flat and managed to enter in the 19.875 sec on the 1/4 mile drag racing !
-0-70km/h in 5sec X5 5303 on 24"
TORQUE SETUP:
-Succeded to haul a 19200 pounds schoolbus!
-Team Konion Member
113kmh Giant___http://www.evalbum.com/3406
Mongoose____http://www.evalbum.com/1947
E-trike_______ http://www.evalbum.com/3776
http://twitter.com/DocbassMelancon
I speak FRENCH and english
User avatar
Doctorbass
100 GW
100 GW
 
Posts: 6607
Joined: Sun Apr 08, 2007 2:24 am
Location: Quebec, Canada East

Re: Data sheet for SELF-BALANCING 18650V

Postby SamTexas » Fri May 06, 2011 12:17 am

I have seen that specs before and there was nothing about self-balancing. I just looked again at the specs you attached and again no reference to SELF-BALANCING. What gives?
SamTexas
100 MW
100 MW
 
Posts: 2841
Joined: Wed Dec 29, 2010 5:34 am
Location: Houston, Texas

Re: Data sheet for SELF-BALANCING 18650V

Postby CamLight » Fri May 06, 2011 1:26 am

Umm...because they don't self-balance?
John M.
Owner
CamLight Systems
CamLight
10 kW
10 kW
 
Posts: 728
Joined: Sat Dec 13, 2008 8:51 pm
Location: New York City, USA

Re: Data sheet for SELF-BALANCING 18650V

Postby SamTexas » Fri May 06, 2011 1:36 am

CamLight wrote:Umm...because they don't self-balance?


Exactly. So why do people buy and use these cells without a BMS? May be for the same reasons I do with my home built Lithium-Cobalt pack at this time. But I have no illusion that my pack would stay balanced for long.
SamTexas
100 MW
100 MW
 
Posts: 2841
Joined: Wed Dec 29, 2010 5:34 am
Location: Houston, Texas

Re: Data sheet for SELF-BALANCING 18650V

Postby Doctorbass » Fri May 06, 2011 1:44 am

These battery are known since 2006 and have been tested also by the Nasa Aerospace flight program.

They have been used in makita, Bosh and Bionx stuff

each of these conpagnt DONT have any balance lead or balancer in their battery

Only the new Makita 2011 have balance lead but they use the same cells.. they just decided to help prolong their pack like a bit and reduce the deffective pack duw to lower cells vs aging

I dont know why people sday they self balance... it'S not the afct...

They just DONT NEED balancing.. but they must be protected against over dishcarge and overcharge to avoid damaging them

They are as safe as A123 cells
________________
-Fastest speed record from now: 113 km/h measured on GPS
-Fastest ebike 106km/h on flat and managed to enter in the 19.875 sec on the 1/4 mile drag racing !
-0-70km/h in 5sec X5 5303 on 24"
TORQUE SETUP:
-Succeded to haul a 19200 pounds schoolbus!
-Team Konion Member
113kmh Giant___http://www.evalbum.com/3406
Mongoose____http://www.evalbum.com/1947
E-trike_______ http://www.evalbum.com/3776
http://twitter.com/DocbassMelancon
I speak FRENCH and english
User avatar
Doctorbass
100 GW
100 GW
 
Posts: 6607
Joined: Sun Apr 08, 2007 2:24 am
Location: Quebec, Canada East

Re: Data sheet for SELF-BALANCING 18650V

Postby Doctorbass » Fri May 06, 2011 1:48 am

________________
-Fastest speed record from now: 113 km/h measured on GPS
-Fastest ebike 106km/h on flat and managed to enter in the 19.875 sec on the 1/4 mile drag racing !
-0-70km/h in 5sec X5 5303 on 24"
TORQUE SETUP:
-Succeded to haul a 19200 pounds schoolbus!
-Team Konion Member
113kmh Giant___http://www.evalbum.com/3406
Mongoose____http://www.evalbum.com/1947
E-trike_______ http://www.evalbum.com/3776
http://twitter.com/DocbassMelancon
I speak FRENCH and english
User avatar
Doctorbass
100 GW
100 GW
 
Posts: 6607
Joined: Sun Apr 08, 2007 2:24 am
Location: Quebec, Canada East

Re: Data sheet for SELF-BALANCING 18650V

Postby SamTexas » Fri May 06, 2011 2:16 am

Doctorbass wrote:I dont know why people sday they self balance... it'S not the afct...

They just DONT NEED balancing..


Huh???
SamTexas
100 MW
100 MW
 
Posts: 2841
Joined: Wed Dec 29, 2010 5:34 am
Location: Houston, Texas

Re: NO such thing as SELF-BALANCING 18650V (Makita)

Postby CamLight » Fri May 06, 2011 3:57 am

All cells don't inherently require balancing. It all depends on the cells and how they're used. For example, if I have a hi-capacity A123 pack, keep all of the cells at the same low room temperature all year around, only charge them to 3.5V/cell at a 0.5C rate and only discharge them at 0.5C down to 3.3V/cell, those cells won't become anymore unbalanced for years.

If I'm using even lower internal-resistance cells with even tighter manufacturing tolerances, then I can abuse them a lot more and still not need balancing before the cells reach their end-of-life.

So, some cells don't need balancing for a lot of applications. But, lots of cells need balancing for some applications. :)
John M.
Owner
CamLight Systems
CamLight
10 kW
10 kW
 
Posts: 728
Joined: Sat Dec 13, 2008 8:51 pm
Location: New York City, USA

Re: NO such thing as SELF-BALANCING 18650V (Makita)

Postby John in CR » Fri May 06, 2011 4:17 am

When a pack gets out of balance after a deep discharge, then you charge/discharge conservatively for a number of cycles, and the pack gets back into good balance, what do you call it other than self-balancing?
John in CR
100 GW
100 GW
 
Posts: 10491
Joined: Tue May 20, 2008 12:58 am
Location: Paradise

Re: NO such thing as SELF-BALANCING 18650V (Makita)

Postby John in CR » Fri May 06, 2011 4:26 am

I suspect the cause to be self discharge varying with voltage to an extent that is different from other batteries. ie Higher voltage has greater self discharge, causing the string to naturally come back into balance.
John in CR
100 GW
100 GW
 
Posts: 10491
Joined: Tue May 20, 2008 12:58 am
Location: Paradise

Re: NO such thing as SELF-BALANCING 18650V (Makita)

Postby trademybikes » Fri May 06, 2011 8:10 am

Its likely a chemical additive protecting from overcharge, results in balanced. This topic was posted last December, the General Motors Lifepo4 patent. Within the patent is ALL the other chemistries that also work. Its 5.5 years since all was known to the inventor group & put to paper. 5 years for patent approval.

How many years has the method been used & by whom? Did the university/GM enter agreements pre-patent? Stolen tech? Does the patent intent to eliminated copies? 20 grand cash bribes most formulas...in general.

Long term players will recall when specific battery types quit burning easily (hint LiFePo series). Recent posts indicate which "Li-ion" sources/suppliers its NOT in.

Dwell on it.
trademybikes
1 µW
1 µW
 
Posts: 1
Joined: Sun Apr 03, 2011 11:01 am

Re: NO such thing as SELF-BALANCING 18650V (Makita)

Postby liveforphysics » Fri May 06, 2011 11:26 am

The charge efficiency of the spinel chemistries decreases slightly as it approaches a high SOC. You can see the effect with a CC supply and a temp sensor as plain as day.

This is what causes them to self balance. (and what causes a lead acid to self balance, only they use electrolysis as the energy outlet)

It is not a designed-in feature, simply an inherent property that helps to self correct balance in packs.

In practice, you can start with a pack that is out of balance, run a number of cycles through it, and each time its finishing the CV mode, you see balance creep a little closer each time until it ends up back in roughly perfect balance after enough cycles.

The exceptions of course would be if you have a weak cell, or a very fresh cell with old cells, etc etc.
For ebike parts, don't be a douche, buy from http://www.ebikes.ca or http://www.MethTek.com

Justin saved the forum at great personal expense! The man is a legend and a hero!
User avatar
liveforphysics
100 GW
100 GW
 
Posts: 11008
Joined: Wed Oct 29, 2008 1:48 am
Location: Santa Cruz, CA, USA

Re: NO such thing as SELF-BALANCING 18650V (Makita)

Postby Doctorbass » Fri May 06, 2011 11:45 am

SamTexas wrote:I have heard so much about the incredible self-balancing property of 18650v (apparently used in Makita packs) . Does anyone know where I can get a manufacturer's data sheet that describes that property? Thanks.

Sam

Edit: Original thread title changed: "Data sheet for SELF-BALANCING 18650V"



You should remane your thread again...

In the industry these cells generally are NOT used with any balancer.. BionX and Makita are some of them

Few month ago Makita began to install cell monitoring on their pack to try increasing the life and refuce the deffecitve pack. Thanks John in Cr for mentioning that. I also got few of these new gen packs but from now had no time to test them as hard as i tested the most known gen.

Plus the experience of over 200-300 users of these makita on the E-S that dont use balancing feature is a valuable data.

The real history about " self balancing".. came from the fact that these big known manufactur DONT use balancer in their batteri desing.

What LFP said make sense to me.

no real need to search further...
________________
-Fastest speed record from now: 113 km/h measured on GPS
-Fastest ebike 106km/h on flat and managed to enter in the 19.875 sec on the 1/4 mile drag racing !
-0-70km/h in 5sec X5 5303 on 24"
TORQUE SETUP:
-Succeded to haul a 19200 pounds schoolbus!
-Team Konion Member
113kmh Giant___http://www.evalbum.com/3406
Mongoose____http://www.evalbum.com/1947
E-trike_______ http://www.evalbum.com/3776
http://twitter.com/DocbassMelancon
I speak FRENCH and english
User avatar
Doctorbass
100 GW
100 GW
 
Posts: 6607
Joined: Sun Apr 08, 2007 2:24 am
Location: Quebec, Canada East

Re: NO such thing as SELF-BALANCING 18650V (Makita)

Postby fizzit » Fri May 06, 2011 11:49 am

Make any pack self-balancing! Just put an equal resistor across the tabs of each cell. Due to ohm's law, the cells with higher voltage will discharge faster, and the whole thing will act like a voltage divider. Just make sure not to let it sit for too long :lol:
-Colin
my first ebike, a freeride mountain bike, using a turnigy 80-85, castle hv160, and turnigy lipo:
viewtopic.php?f=28&t=21953&start=180#p607020
User avatar
fizzit
10 kW
10 kW
 
Posts: 774
Joined: Wed Mar 10, 2010 10:14 pm
Location: Seattle, WA

Re: NO such thing as SELF-BALANCING 18650V (Makita)

Postby liveforphysics » Fri May 06, 2011 12:09 pm

Doctorbass wrote:
SamTexas wrote:I have heard so much about the incredible self-balancing property of 18650v (apparently used in Makita packs) . Does anyone know where I can get a manufacturer's data sheet that describes that property? Thanks.

Sam

Edit: Original thread title changed: "Data sheet for SELF-BALANCING 18650V"



You should remane your thread again...

In the industry these cells generally are NOT used with any balancer.. BionX and Makita are some of them

Few month ago Makita began to install cell monitoring on their pack to try increasing the life and refuce the deffecitve pack. Thanks John in Cr for mentioning that. I also got few of these new gen packs but from now had no time to test them as hard as i tested the most known gen.

Plus the experience of over 200-300 users of these makita on the E-S that dont use balancing feature is a valuable data.

The real history about " self balancing".. came from the fact that these big known manufactur DONT use balancer in their batteri desing.

What LFP said make sense to me.

no real need to search further...


Our pre-release Nissan LEAF sample pack at work had no balancing capability in its pack because its a spinel chemistry. It can only monitor to watch for a cell failure/weak cell, but it uses the cells themself to stay in balance, and they do, perfectly.
For ebike parts, don't be a douche, buy from http://www.ebikes.ca or http://www.MethTek.com

Justin saved the forum at great personal expense! The man is a legend and a hero!
User avatar
liveforphysics
100 GW
100 GW
 
Posts: 11008
Joined: Wed Oct 29, 2008 1:48 am
Location: Santa Cruz, CA, USA

Re: NO such thing as SELF-BALANCING 18650V (Makita)

Postby John in CR » Fri May 06, 2011 1:13 pm

LFP,

Thanks for the explanation. Balancing a little bit each cycle on the way up makes perfect sense. How do you think charge current affects this phenomenon? I have 3 of my charger pairs, so now I can charge 3.5, 7, or 10.5A, so if slow or fast charging is better it would be nice to know. Of course I haven't run out of juice since you were down, so I haven't worried about balance at all.


Sam my man, gotta edit the subject line in your first post to "Self balance charging batteries do exist, even lead batts can do that." :mrgreen:
John in CR
100 GW
100 GW
 
Posts: 10491
Joined: Tue May 20, 2008 12:58 am
Location: Paradise

Re: NO such thing as SELF-BALANCING 18650V (Makita)

Postby CamLight » Fri May 06, 2011 9:36 pm

John in CR wrote:When a pack gets out of balance after a deep discharge, then you charge/discharge conservatively for a number of cycles, and the pack gets back into good balance, what do you call it other than self-balancing?

The pack was never out of balance.
The cells are just at different voltage levels because of differences in SOC between them. Bring them all back to the same SOC and they're at the same voltage (assuming relatively good condition cells, blah, blah, blah).

If there's some sort of self-balancing going on then it shouldn't need cycling to occur. The cells would somehow "see" each other and just go ahead and balance themselves. That is, wiring a 25% SOC cell into a group of 100% SOC cells should result in a pack that has cells all at the same voltage after letting them sit. That won't happen, even with cycling the pack.
John M.
Owner
CamLight Systems
CamLight
10 kW
10 kW
 
Posts: 728
Joined: Sat Dec 13, 2008 8:51 pm
Location: New York City, USA

Re: NO such thing as SELF-BALANCING 18650V (Makita)

Postby John in CR » Fri May 06, 2011 11:29 pm

CamLight wrote:
John in CR wrote:When a pack gets out of balance after a deep discharge, then you charge/discharge conservatively for a number of cycles, and the pack gets back into good balance, what do you call it other than self-balancing?

The pack was never out of balance.
The cells are just at different voltage levels because of differences in SOC between them. Bring them all back to the same SOC and they're at the same voltage (assuming relatively good condition cells, blah, blah, blah).

If there's some sort of self-balancing going on then it shouldn't need cycling to occur. The cells would somehow "see" each other and just go ahead and balance themselves. That is, wiring a 25% SOC cell into a group of 100% SOC cells should result in a pack that has cells all at the same voltage after letting them sit. That won't happen, even with cycling the pack.


Of course it was out of balance, and it was still out of balance after the initial recharge. After about 10 days of 1 or 2 cycles a day then the pack returned to normal. The last time I did accidentally did a 100% discharge, was just over a year ago, when LFP was down. He even commented on the crap capacity of that initial recharge, which I think was just 7ah for the 11-12ah pack. In less than 2 weeks, the pack was back to normal accepting full capacity.

LFP already explained the mechanism, so why still argue? These Konion packs definitely get out of whack from very deep discharges just like with other lithium chemistries, and they don't return to balance at top of charge on the first recharge. It's not just a voltage difference between the cells at the bottom SOC, and the self balancing charge effect isn't strong enough to self balance charge the first go round.
John in CR
100 GW
100 GW
 
Posts: 10491
Joined: Tue May 20, 2008 12:58 am
Location: Paradise

Re: NO such thing as SELF-BALANCING 18650V (Makita)

Postby liveforphysics » Sat May 07, 2011 12:43 am

CamLight wrote:
John in CR wrote:When a pack gets out of balance after a deep discharge, then you charge/discharge conservatively for a number of cycles, and the pack gets back into good balance, what do you call it other than self-balancing?

The pack was never out of balance.
The cells are just at different voltage levels because of differences in SOC between them. Bring them all back to the same SOC and they're at the same voltage (assuming relatively good condition cells, blah, blah, blah).

If there's some sort of self-balancing going on then it shouldn't need cycling to occur. The cells would somehow "see" each other and just go ahead and balance themselves. That is, wiring a 25% SOC cell into a group of 100% SOC cells should result in a pack that has cells all at the same voltage after letting them sit. That won't happen, even with cycling the pack.



Nope, perfectly matched brand new cells, at different states charge, will self balance after enough charge cycles with the spinel chemistries. They decrease charge energy efficiency and shed it as heat once they get above 4.1-4.2v or so. This makes the cells that were below this threshold get a bit of catch-up on each charge cycle until the pack finds balance.
For ebike parts, don't be a douche, buy from http://www.ebikes.ca or http://www.MethTek.com

Justin saved the forum at great personal expense! The man is a legend and a hero!
User avatar
liveforphysics
100 GW
100 GW
 
Posts: 11008
Joined: Wed Oct 29, 2008 1:48 am
Location: Santa Cruz, CA, USA

Re: NO such thing as SELF-BALANCING 18650V (Makita)

Postby CamLight » Sat May 07, 2011 3:41 am

John in CR wrote:LFP already explained the mechanism, so why still argue? These Konion packs definitely get out of whack from very deep discharges just like with other lithium chemistries, and they don't return to balance at top of charge on the first recharge. It's not just a voltage difference between the cells at the bottom SOC, and the self balancing charge effect isn't strong enough to self balance charge the first go round.

LOL, not arguing at all. I think there's some confusion as to the terminology used here. :mrgreen:
I completely agree with your statement above and was never trying to state otherwise.

LFP explained his position further and I will comment there.
John M.
Owner
CamLight Systems
CamLight
10 kW
10 kW
 
Posts: 728
Joined: Sat Dec 13, 2008 8:51 pm
Location: New York City, USA

Re: NO such thing as SELF-BALANCING 18650V (Makita)

Postby CamLight » Sat May 07, 2011 3:46 am

liveforphysics wrote:Nope, perfectly matched brand new cells, at different states charge, will self balance after enough charge cycles with the spinel chemistries. They decrease charge energy efficiency and shed it as heat once they get above 4.1-4.2v or so. This makes the cells that were below this threshold get a bit of catch-up on each charge cycle until the pack finds balance.

Ahhh...Interesting. Sounds very similar to charging the Nickel chemistries at over 100% SOC using low charge rates to help balance the pack. The terminology mismatch I was referring to above comes out of my thinking that the cells themselves aren't self-balancing, it's the charge that's bled off as heat that allows the other cells to catch up. The charge and charger balances them, not the cells all on their own ("self"). I guess one could argue that NiCd and NiMH cells are self-balancing too?

But, the Li stuff we're talking about is just terminology differences. The effect/end result is the same and I'll have no problems deferring to the accepted terminology used here. :D
John M.
Owner
CamLight Systems
CamLight
10 kW
10 kW
 
Posts: 728
Joined: Sat Dec 13, 2008 8:51 pm
Location: New York City, USA

Re: NO Self-Balancing 18650V (Makita) by design.

Postby GGoodrum » Sat May 07, 2011 11:27 am

As usual, Luke has nailed it. :) The slight loss of charging efficiency, as the cell gets full, is the trait of these spinel-type Lithium-Magenese cells that provide a similar balancing function that occurs with lead acid and NiCds. The latter two chemistries use aqueous-type electrolytes that have side reactions that can absorb some charge current, if the voltage they are charged to is slightly above the "full" point. This can be thought of as a slight loss of charging efficiency, just like what happens with the spinel LiMn cells. The net effect is the same. some current is absorbed for a full cell, allowing the next cell in series to use that same amount of current to finish charging. This is exactly the function of most BMS shunt balancing circuits provide for other Lithium chemistries that don't have this loss of efficiency trait.

This efficiency loss is very slight, however, which is why it will take multiple charge cycles for the cells to get back in balance. As John's experience has shown, eventually they will.

-- Gary
User avatar
GGoodrum
100 MW
100 MW
 
Posts: 2980
Joined: Thu Sep 20, 2007 2:03 pm
Location: South Orange County, CA

Re: NO such thing as SELF-BALANCING 18650V (Makita)

Postby flathill » Mon Apr 30, 2012 8:08 pm

liveforphysics wrote:
CamLight wrote:
John in CR wrote:When a pack gets out of balance after a deep discharge, then you charge/discharge conservatively for a number of cycles, and the pack gets back into good balance, what do you call it other than self-balancing?

The pack was never out of balance.
The cells are just at different voltage levels because of differences in SOC between them. Bring them all back to the same SOC and they're at the same voltage (assuming relatively good condition cells, blah, blah, blah).

If there's some sort of self-balancing going on then it shouldn't need cycling to occur. The cells would somehow "see" each other and just go ahead and balance themselves. That is, wiring a 25% SOC cell into a group of 100% SOC cells should result in a pack that has cells all at the same voltage after letting them sit. That won't happen, even with cycling the pack.



Nope, perfectly matched brand new cells, at different states charge, will self balance after enough charge cycles with the spinel chemistries. They decrease charge energy efficiency and shed it as heat once they get above 4.1-4.2v or so. This makes the cells that were below this threshold get a bit of catch-up on each charge cycle until the pack finds balance.



Bring this thread back from the dead as self balancing is such a great feature, but I've read more than one theory explaining how it works.

I've been doing more research on the mechanism behind this...AEA licensed the cathode to Sony and AEA's theory is cell's with a higher SOC will also have higher self discharge. This means that cells JUST SITTING THERE will also eventually self balance given enough time :D

The theory is confirmed:
"Tests ~8 yrs ago showed Sony HC do not imbalance
AEA developed a theory (ESPC 2002)
− Self-discharge (SD) decreases with state-of-charge (SOC)
− Cells diverge to a state of dynamic equilibrium
− Equilibrium spread depends on cell SD uniformity
Balancing model verified against test data":::::::::::

http://ntrs.nasa.gov/archive/nasa/casi. ... 015867.pdf
flathill
10 kW
10 kW
 
Posts: 630
Joined: Tue Jul 06, 2010 9:26 pm

Next

Return to Battery Technology

Who is online

Users browsing this forum: No registered users and 8 guests