LOW COST UNMANNED SOLAR AIRCRAFT. We did it!!!!!

Things that fly

LOW COST UNMANNED SOLAR AIRCRAFT. We did it!!!!!

Postby Ludo91 » Fri Sep 09, 2011 10:57 am

Hey my worldwide located electric powered friends!

Me and a my "crazy projects mate" (Stefano, aka giubi.s) made a solar plane

It is 3 yards of wingspan (2.3 meters to be precise), glassfirbe homemade fuselage and carbon/balsa wing.

28 panels are connect in 14s2p and are inside the wings and on the tail.

Motor is hacker b2015l + maxxon gear 4:1, esc is 18A from hacker.

The panels under the trasparent oracover indoor give us 25 watts on a great sunny day, barely enough to fly, so we have a 3s lipo with a ground controlled switching regulator to make the battery and the panels cooperate.

FLying with such low conspumptions requires an insane precision, so the plane is flown by ardupilot 2.6 (thermopiles version).

We worked on it for a bot over a year, biggest issue was to have the battery cooperate with the panels.

A few days ago we managed to keep it in the air for 142 minutes, wich we think is a great succes and will be improved since that day was very wind and the autopilot was not propely set yet (5 times up from almost ground to limit of visibility and back, a big waste of energy I`d say).

Here are some pics!

Image
Image
Image
Image
Image
Image
Image
Image
Image
Image
Image
Image
Image
Image
Image
Image
Image
Image
Image
Open source high power BLDC controller! ===> http://code.google.com/p/dc-brushless-open-source-controller/
User avatar
Ludo91
100 W
100 W
 
Posts: 123
Joined: Mon Feb 14, 2011 3:03 pm
Location: Milan, Italy

Re: LOW COST UNMANNED SOLAR AIRCRAFT. We did it!!!!!

Postby vanilla ice » Fri Sep 09, 2011 11:43 am

Sweet! I think there is a job for you at border partrol. :P

What kind of issues did you have with the panels not cooperating with the battery?
75# ebike, 190# scooter, 370# motorcycle, 1900# car, 4900# truck..
User avatar
vanilla ice
1.21 GW
1.21 GW
 
Posts: 3550
Joined: Wed Sep 05, 2007 9:15 pm
Location: socal dude

Re: LOW COST UNMANNED SOLAR AIRCRAFT. We did it!!!!!

Postby TylerDurden » Fri Sep 09, 2011 12:05 pm

Very cool! :mrgreen:
Have a Nice Day,

TD

Image
___________________________________________________________

FYI: Adding pictures?

Bored?... take a crack at the unanswered posts

Please post your Watts-at-speed in the survey.



Image
User avatar
TylerDurden
100 GW
100 GW
 
Posts: 8540
Joined: Thu Jan 04, 2007 5:50 pm
Location: Wear the fox hat.

Re: LOW COST UNMANNED SOLAR AIRCRAFT. We did it!!!!!

Postby grindz145 » Fri Sep 09, 2011 12:05 pm

That, is so badass:) /has nothing to do with ebikes , awsome. I still want to do a quadcopter :D
http://www.endless-sphere.com/forums/viewtopic.php?f=18&t=19548 - Ebike Nerd Podcast
Thanks to Justin @ ebikes.ca! Go there, buy stuff. Support the Revolution :D
User avatar
grindz145
100 MW
100 MW
 
Posts: 2673
Joined: Tue Apr 07, 2009 12:10 pm
Location: Rochester NY

Re: LOW COST UNMANNED SOLAR AIRCRAFT. We did it!!!!!

Postby el_walto » Fri Sep 09, 2011 12:07 pm

Looks pretty cool.
el_walto
10 kW
10 kW
 
Posts: 680
Joined: Fri Apr 25, 2008 3:48 pm
Location: Kamloops BC Canada

Re: LOW COST UNMANNED SOLAR AIRCRAFT. We did it!!!!!

Postby hydro-one » Fri Sep 09, 2011 12:18 pm

Cool!!! That is a very nice model! Excellent

What spec panels are you using, how much are you losing due to the covering, can you get a better cover material?

Can you get a lighter panel?

Micropilot was developed by a guy , my dad knows him well.

fold out more panels the higher you get? what are your goal in this project?

Tell us more!

mikebike
hydro-one
10 kW
10 kW
 
Posts: 704
Joined: Fri Dec 19, 2008 2:02 pm
Location: winipeg Canada

Re: LOW COST UNMANNED SOLAR AIRCRAFT. We did it!!!!!

Postby gestalt » Fri Sep 09, 2011 12:27 pm

Great work on the solar uav!!! Guys like you give me great hope and inspiration. Imagine now what could be done with more efficient solar panels. I wish thin film solar was more powerful, it would be awesome just to integrate the cells as part of the structure of the wing itself. You would probably have some great weight savings as well.

grindz145 wrote:That, is so badass:) /has nothing to do with ebikes , awsome. I still want to do a quadcopter :D


There used to be a link link and img of a maned electric quadracopter on here somewhere. I think I even posted it, but it disappeared and no matter how much I troll the interwebz for it it is nowhere to be seen. But I still have it in my rusty steel trap of a mind. If I'm ever not living hand to mouth I'm going to have to give it a try. Hmmm, how many kwh of nanotech would it take to powers 4 joby motors in ducts? More than I'm worth to be sure.
Last edited by gestalt on Fri Sep 09, 2011 1:27 pm, edited 1 time in total.
- be seeing you
Image
User avatar
gestalt
10 kW
10 kW
 
Posts: 809
Joined: Mon Oct 19, 2009 10:55 pm
Location: Boston, MA

Re: LOW COST UNMANNED SOLAR AIRCRAFT. We did it!!!!!

Postby Doctorbass » Fri Sep 09, 2011 12:36 pm

realy cool project!!!

Could you paint in silver or white the surrounding border ( balsa) of the solar panel to maximize the solar ray to the solar panel? I see a little shadow that cove rlike 5-10% surface so it would help a bit as well

Doc
________________
-Fastest speed record from now: 113 km/h measured on GPS
-Fastest ebike 106km/h on flat and managed to enter in the 19.875 sec on the 1/4 mile drag racing !
-0-70km/h in 5sec X5 5303 on 24"
TORQUE SETUP:
-Succeded to haul a 19200 pounds schoolbus!
-Team Konion Member
113kmh Giant___http://www.evalbum.com/3406
Mongoose____http://www.evalbum.com/1947
E-trike_______ http://www.evalbum.com/3776
http://twitter.com/DocbassMelancon
I speak FRENCH and english
User avatar
Doctorbass
100 GW
100 GW
 
Posts: 6536
Joined: Sun Apr 08, 2007 2:24 am
Location: Quebec, Canada East

Re: LOW COST UNMANNED SOLAR AIRCRAFT. We did it!!!!!

Postby pelle242 » Fri Sep 09, 2011 1:10 pm

Fantastic!! Its not long ago NASA or such did this with million dollar budget. Now its wihin the realm of hobbyists!
pelle242
100 W
100 W
 
Posts: 180
Joined: Fri Oct 22, 2010 3:41 am
Location: Stockholm, Sweden

Re: LOW COST UNMANNED SOLAR AIRCRAFT. We did it!!!!!

Postby whatever » Thu Sep 29, 2011 1:59 am

HI Ludo91
have you published any detailed plans on your build?
of interest for me is clear material over cells that you used,
and those problems you had getting cells and batteries to work together.
whatever
10 kW
10 kW
 
Posts: 651
Joined: Thu Jun 03, 2010 2:16 am

Re: LOW COST UNMANNED SOLAR AIRCRAFT. We did it!!!!!

Postby ptd » Thu Sep 29, 2011 3:44 am

grindz145 wrote:has nothing to do with ebikes

maybe that's why it's in the AIRCRAFT section
woohoo, knightmb is gone, now where's his ill gotten gains ?
User avatar
ptd
100 W
100 W
 
Posts: 221
Joined: Wed Jun 15, 2011 7:27 pm
Location: california

Re: LOW COST UNMANNED SOLAR AIRCRAFT. We did it!!!!!

Postby Ludo91 » Sat Oct 01, 2011 7:27 pm

Yep! my nad my friend want to realease all the plans about the plane, but since we are enrolled in a damn hard college we are seriously struggling with time, but we consider our projcet ope source and as soon as we get some time to do this we`ll make a .zip file with everything in it ;)

Film is oracover (or oralite? i dont remember, will check in the orders` mail) lite, for indoor use, wich mean thermal shrinking but not adhesive, beacuse the glue on the inside of the film in out first attemp got yellowish after less that one hour in direct sun.....

having the battery work with the panels is a damn hard issue, basically you wnat a motor and a prob that matched 2gehter would work by themselves at the MPP of the cells (sound weird but we say this basing on several hours of testing with a lot of sensors) and then use a switching dc dc converter in voltage mode to increase the voltage of the whole system, relying on the battery, in order to get more power.

Basically our panels give their best at about 5.5 volts under load, with them still doing a great part of the work with the voltage raised up to 6.something volts by the dc dc converter... so having the battery stepping in to get a bit more extra power from the motor doesnt spoil the soalr nature of our toy (esc is always full chat, we change gas setpoint by changing the power rail voltage).

cheers!!! :D
Open source high power BLDC controller! ===> http://code.google.com/p/dc-brushless-open-source-controller/
User avatar
Ludo91
100 W
100 W
 
Posts: 123
Joined: Mon Feb 14, 2011 3:03 pm
Location: Milan, Italy

Re: LOW COST UNMANNED SOLAR AIRCRAFT. We did it!!!!!

Postby SamTexas » Sat Oct 01, 2011 9:08 pm

What a project! More detailed info please.

Ludo91 wrote:The panels under the trasparent oracover indoor give us 25 watts on a great sunny day, barely enough to fly,

So how much power is needed to keep it in the air? At what speed and altitude? Assuming a non-windy day of course.
How much does it weigh?
SamTexas
100 MW
100 MW
 
Posts: 2832
Joined: Wed Dec 29, 2010 5:34 am
Location: Houston, Texas

Re: LOW COST UNMANNED SOLAR AIRCRAFT. We did it!!!!!

Postby Ludo91 » Sun Oct 02, 2011 7:45 am

it is 1.6 kg rady to fly, it stays in the air with 25 watts when flying straight and perfectly flat, average consumption on a flight is about 30W, +/- 1.5W (yeah we have crappy current sensors).

We keept it at about 80 yard height

Now the plane is in a box beacuse italy is northen enough on the planet to make the october sun almost useless for panels under a plastic film (it reflect most of the light if it is not perpendicular) and also we really need to upgrade the autopilot to ardupilot mega, in order to have the barometric sensor (way better height control) and the Derivative term in the PID, so right now we are looking for a sponsor :wink:

I want so bad the release the .zip with all the info in it!!!
Open source high power BLDC controller! ===> http://code.google.com/p/dc-brushless-open-source-controller/
User avatar
Ludo91
100 W
100 W
 
Posts: 123
Joined: Mon Feb 14, 2011 3:03 pm
Location: Milan, Italy

Re: LOW COST UNMANNED SOLAR AIRCRAFT. We did it!!!!!

Postby SamTexas » Sun Oct 02, 2011 10:59 am

Thanks for the detailed info. What is the typical air speed at 80 yard altitude?

Best of luck on finding a sponsor and keep up with the good, interesting work.
SamTexas
100 MW
100 MW
 
Posts: 2832
Joined: Wed Dec 29, 2010 5:34 am
Location: Houston, Texas

Re: LOW COST UNMANNED SOLAR AIRCRAFT. We did it!!!!!

Postby Ludo91 » Mon Oct 03, 2011 7:14 am

Typical airspeed is about 20 mph, it is an indicative value since here in northen italy clear sunny days are always really windy ;)

If you know someone or somewhere to get sponsorship please tell us! :D
Open source high power BLDC controller! ===> http://code.google.com/p/dc-brushless-open-source-controller/
User avatar
Ludo91
100 W
100 W
 
Posts: 123
Joined: Mon Feb 14, 2011 3:03 pm
Location: Milan, Italy

Re: LOW COST UNMANNED SOLAR AIRCRAFT. We did it!!!!!

Postby Ludo91 » Sun Feb 12, 2012 6:52 am

Hey guys! working hard on our finals, truly hoping to (finally!) release the data in a month and a half or so :)
Open source high power BLDC controller! ===> http://code.google.com/p/dc-brushless-open-source-controller/
User avatar
Ludo91
100 W
100 W
 
Posts: 123
Joined: Mon Feb 14, 2011 3:03 pm
Location: Milan, Italy


Return to Electric Aircraft

Who is online

Users browsing this forum: No registered users and 0 guests