Hybrid 7.2v 6.5Ah Nimh Battery Sticks

Got something to sell? Have extra parts that need a good home? Have something that others would need to complete their kits? Post it up here and see if anyone else is searching for what you are selling. Guest may post replies to topics already here. All topics here will expire after 90 days of inactivity.

Hybrid 7.2v 6.5Ah Nimh Battery Sticks

Postby peterperkins » Thu Oct 06, 2011 1:11 pm

I have a large stock of used good battery sticks from hybrid cars which are more than adequate for e-Bike/scooter projects especially recumbents or trikes where the extra weight is less of an issue.

They are very easy to assemble into packs using the screw terminals (bolts supplied) and include a ptc heat sensing strip to implement a simple overheating protection circuit. They can handle upto 100A discharge and 50A charge rates. They can be put into series for any voltage HV pack.

I have upwards of 100 sticks available at £10.00 each p&p extra or collection free from my address in North Yorkshire.

They are a doddle to charge overnight with a cheap fixed current 300-350ma psu meanwell led supply and no fancy BMS is reqd. The only proviso is that the self discharge rate will be higher than you are used to, so charge them within a few days of your expected use to get best results. For optimum performance just charge them prior to use. You can trickle charge them at very low currents for standby use if you wish.

I'll happily warranty the sticks for 6 months in any e-bike/scooter application and replace them for the cost of postage only.

PM me your requirements.
Last edited by peterperkins on Tue Oct 02, 2012 10:30 pm, edited 1 time in total.
Honda Insight MK1 lmpg 131mpg Imp
Lifepo4 40ah HiPower IMA Pack & 20ah A123 IMA Pack
BCM Fooler, BCM Interceptor, BCM Gauge, Li-Ion BMS System, OBDIIC&C, IMAC&C
http://www.150mpg.co.uk
peterperkins
100 W
100 W
 
Posts: 193
Joined: Fri Jun 06, 2008 2:10 am

Re: Hybrid 7.2v 6.5Ah Nimh Battery Sticks

Postby Kin » Thu Oct 06, 2011 2:48 pm

That's pretty cool. It doesnt quite work with what I've got going on. That said, you might also get some people interested at DIYElectriccar forums. But, perhaps, you're especially targeting ebikes for whatever reason. Might want to mention, do you know how much of the 6.5ah still works? Have you been able to test them?
New to endless-sphere? Notice a lot of signatures recommending Ebike.ca? That's because it's the best place for a quality and manageable, (but still 'real'), first build. Justin is a solid supporter of electric bike development, and a good source of equipment.

My hat off a thousand times to the green people that effectively run this forum. The ES Mods are superb.
Kin
100 kW
100 kW
 
Posts: 1193
Joined: Sat Mar 05, 2011 6:16 pm
Location: NC or MA, U.S

Re: Hybrid 7.2v 6.5Ah Nimh Battery Sticks

Postby peterperkins » Fri Oct 07, 2011 12:18 pm

After cycling on a decent charger like the Robotronic Overloader a few times to condition them after storage, most average out at about 6ah capacity at 15A ~2C+ discharge rate on the ones I have tested at random.

The Puekert effect does reduce capacity at high discharge rates. At 65A (10C) you would see about 3.5Ah.

I'm going to put some on e-bay and other forums.
Honda Insight MK1 lmpg 131mpg Imp
Lifepo4 40ah HiPower IMA Pack & 20ah A123 IMA Pack
BCM Fooler, BCM Interceptor, BCM Gauge, Li-Ion BMS System, OBDIIC&C, IMAC&C
http://www.150mpg.co.uk
peterperkins
100 W
100 W
 
Posts: 193
Joined: Fri Jun 06, 2008 2:10 am

Re: Hybrid 7.2v 6.5Ah Nimh Battery Sticks

Postby peterperkins » Sat Oct 08, 2011 12:47 am

Honda Insight MK1 lmpg 131mpg Imp
Lifepo4 40ah HiPower IMA Pack & 20ah A123 IMA Pack
BCM Fooler, BCM Interceptor, BCM Gauge, Li-Ion BMS System, OBDIIC&C, IMAC&C
http://www.150mpg.co.uk
peterperkins
100 W
100 W
 
Posts: 193
Joined: Fri Jun 06, 2008 2:10 am

Re: Hybrid 7.2v 6.5Ah Nimh Battery Sticks

Postby peterperkins » Tue Oct 11, 2011 11:12 am

Load testing a random stick.

http://www.youtube.com/watch?v=4PEflc_dW04

The sticks weigh 1075g each approx
Length inc two bolts is 400mm
Diameter is 35mm
Honda Insight MK1 lmpg 131mpg Imp
Lifepo4 40ah HiPower IMA Pack & 20ah A123 IMA Pack
BCM Fooler, BCM Interceptor, BCM Gauge, Li-Ion BMS System, OBDIIC&C, IMAC&C
http://www.150mpg.co.uk
peterperkins
100 W
100 W
 
Posts: 193
Joined: Fri Jun 06, 2008 2:10 am

Re: Hybrid 7.2v 6.5Ah Nimh Battery Sticks

Postby Doctorbass » Tue Oct 11, 2011 10:29 pm

peterperkins wrote:Load testing a random stick.

http://www.youtube.com/watch?v=4PEflc_dW04

The sticks weigh 1075g each approx
Length inc two bolts is 400mm
Diameter is 35mm


Where did you got your load tester shown in the video?

Doc
________________
-Fastest speed record from now: 113 km/h measured on GPS
-Fastest ebike 106km/h on flat and managed to enter in the 19.875 sec on the 1/4 mile drag racing !
-0-70km/h in 5sec X5 5303 on 24"
TORQUE SETUP:
-Succeded to haul a 19200 pounds schoolbus!
-Team Konion Member
113kmh Giant___http://www.evalbum.com/3406
Mongoose____http://www.evalbum.com/1947
E-trike_______ http://www.evalbum.com/3776
http://twitter.com/DocbassMelancon
I speak FRENCH and english
User avatar
Doctorbass
100 GW
100 GW
 
Posts: 6525
Joined: Sun Apr 08, 2007 2:24 am
Location: Quebec, Canada East

Re: Hybrid 7.2v 6.5Ah Nimh Battery Sticks

Postby peterperkins » Mon Oct 17, 2011 6:44 pm

10 sold now ~90 sticks left :wink:

My load tester is an old farnell thing at least 20 years old+ Uses ~10 x 2N3055 in parallel if i remember correctly with some pwm going on. Capable of 120A at 30V adjustable CC or CV It gives cells a good workout :)
Honda Insight MK1 lmpg 131mpg Imp
Lifepo4 40ah HiPower IMA Pack & 20ah A123 IMA Pack
BCM Fooler, BCM Interceptor, BCM Gauge, Li-Ion BMS System, OBDIIC&C, IMAC&C
http://www.150mpg.co.uk
peterperkins
100 W
100 W
 
Posts: 193
Joined: Fri Jun 06, 2008 2:10 am

Re: Hybrid 7.2v 6.5Ah Nimh Battery Sticks

Postby peterperkins » Tue Oct 02, 2012 10:29 pm

I now have a further 100 of these. Demand was very high last time and i sold them all quite quickly.

I have a large quantity (100+) x 7.2V (6 x D Cell) sticks from ex Honda Hybrid cars in my garage.
These quality panasonic nimh sticks are designed for 50A charge and 100A discharge rates.

The sticks I have are no longer suitable for hybrid car use at those rates, but at more modest discharge upto 25A they are fine. Capacity is anything from 5.5-6.5ah at 20A discharge rate.

They have M6 bolt ends and are a doddle to connect together using bolts, or studs to screw sticks directly together end to end. Charging is easy using a simple led constant current 350ma power supply. The 48V led supplies on e-bay can charge anything from two to six sticks. The 90V ones can do up ten sticks. Five sticks is ideal and gives a simple 36V ~6ah pack that weighs 5kg.

Search for 300ma or 350ma led driver on ebay for a simple charger there are zillions.

Price is £10 a stick for a random stick from my stock. All my sticks are currently stored in my cool workshop.

Postage is extra or you can have as many as you want if you collect from my address in North Yorkshire.

I find the best way to use them is wake them up with a robotronic overloader type nimh charger/cycler then build them into a pack. I've used quite a few in my electric bike and other projects and they are great.

Here is a yt video of a random stick under torture/test on my electronic load.

6.5ah 7.2v Nimh Hybrid Battery Sticks 100A Load Testing. - YouTube

It shows what they look like and even these older sticks still perform so i'm being conservative with my ratings above.

Contact me at 150mpg(remove this)@gmail(remove this).com
Honda Insight MK1 lmpg 131mpg Imp
Lifepo4 40ah HiPower IMA Pack & 20ah A123 IMA Pack
BCM Fooler, BCM Interceptor, BCM Gauge, Li-Ion BMS System, OBDIIC&C, IMAC&C
http://www.150mpg.co.uk
peterperkins
100 W
100 W
 
Posts: 193
Joined: Fri Jun 06, 2008 2:10 am

Re: Hybrid 7.2v 6.5Ah Nimh Battery Sticks

Postby peterperkins » Fri Oct 05, 2012 3:06 pm

Price reduced to £7.00 a stick.
Honda Insight MK1 lmpg 131mpg Imp
Lifepo4 40ah HiPower IMA Pack & 20ah A123 IMA Pack
BCM Fooler, BCM Interceptor, BCM Gauge, Li-Ion BMS System, OBDIIC&C, IMAC&C
http://www.150mpg.co.uk
peterperkins
100 W
100 W
 
Posts: 193
Joined: Fri Jun 06, 2008 2:10 am

Re: Hybrid 7.2v 6.5Ah Nimh Battery Sticks

Postby JoramsWeapon » Fri Oct 05, 2012 4:18 pm

I need a shipping quote please. Check your email.
JoramsWeapon
100 W
100 W
 
Posts: 145
Joined: Wed Feb 16, 2011 12:11 am

Re: Hybrid 7.2v 6.5Ah Nimh Battery Sticks

Postby peterperkins » Fri Oct 05, 2012 5:15 pm

Sorry I should have made it clear this is UK only as overseas shipping is too expesnive.
Honda Insight MK1 lmpg 131mpg Imp
Lifepo4 40ah HiPower IMA Pack & 20ah A123 IMA Pack
BCM Fooler, BCM Interceptor, BCM Gauge, Li-Ion BMS System, OBDIIC&C, IMAC&C
http://www.150mpg.co.uk
peterperkins
100 W
100 W
 
Posts: 193
Joined: Fri Jun 06, 2008 2:10 am

Re: Hybrid 7.2v 6.5Ah Nimh Battery Sticks

Postby darren1678 » Sat Oct 06, 2012 6:56 pm

hay peter check email
darren1678
1 W
1 W
 
Posts: 52
Joined: Thu Aug 30, 2012 8:58 pm

Re: Hybrid 7.2v 6.5Ah Nimh Battery Sticks

Postby peterperkins » Mon Nov 12, 2012 12:21 am

Price reduced to £1 a cell (£6.00 a stick) trying to clear out my garage.
Honda Insight MK1 lmpg 131mpg Imp
Lifepo4 40ah HiPower IMA Pack & 20ah A123 IMA Pack
BCM Fooler, BCM Interceptor, BCM Gauge, Li-Ion BMS System, OBDIIC&C, IMAC&C
http://www.150mpg.co.uk
peterperkins
100 W
100 W
 
Posts: 193
Joined: Fri Jun 06, 2008 2:10 am

Re: Hybrid 7.2v 6.5Ah Nimh Battery Sticks

Postby Electricmike » Sat Nov 17, 2012 1:57 pm

How many of these sticks do you have left?
Electricmike
1 µW
1 µW
 
Posts: 2
Joined: Sat Nov 17, 2012 1:45 pm

Re: Hybrid 7.2v 6.5Ah Nimh Battery Sticks

Postby peterperkins » Tue Nov 20, 2012 12:45 am

I get more in most weeks so have about 100 sticks again now.
Honda Insight MK1 lmpg 131mpg Imp
Lifepo4 40ah HiPower IMA Pack & 20ah A123 IMA Pack
BCM Fooler, BCM Interceptor, BCM Gauge, Li-Ion BMS System, OBDIIC&C, IMAC&C
http://www.150mpg.co.uk
peterperkins
100 W
100 W
 
Posts: 193
Joined: Fri Jun 06, 2008 2:10 am

Re: Hybrid 7.2v 6.5Ah Nimh Battery Sticks

Postby peterperkins » Sun Nov 25, 2012 3:21 am

Last reduction £5 a stick.

Sorry this is UK only but thanks for the overseas enqs.
Honda Insight MK1 lmpg 131mpg Imp
Lifepo4 40ah HiPower IMA Pack & 20ah A123 IMA Pack
BCM Fooler, BCM Interceptor, BCM Gauge, Li-Ion BMS System, OBDIIC&C, IMAC&C
http://www.150mpg.co.uk
peterperkins
100 W
100 W
 
Posts: 193
Joined: Fri Jun 06, 2008 2:10 am

Re: Hybrid 7.2v 6.5Ah Nimh Battery Sticks

Postby pdarnett » Sat Dec 01, 2012 4:07 pm

Any of these left? I wouldnt mind 10 to buld two 36v packs for my ezee Sprint
pdarnett
1 mW
1 mW
 
Posts: 10
Joined: Sat Dec 01, 2012 3:28 pm

Re: Hybrid 7.2v 6.5Ah Nimh Battery Sticks

Postby peterperkins » Sun Dec 02, 2012 11:32 pm

Yes still got some left but going fast.
Honda Insight MK1 lmpg 131mpg Imp
Lifepo4 40ah HiPower IMA Pack & 20ah A123 IMA Pack
BCM Fooler, BCM Interceptor, BCM Gauge, Li-Ion BMS System, OBDIIC&C, IMAC&C
http://www.150mpg.co.uk
peterperkins
100 W
100 W
 
Posts: 193
Joined: Fri Jun 06, 2008 2:10 am


Return to Items for Sale - Used

Who is online

Users browsing this forum: emiyata and 1 guest