I've always wanted to try out the contiguous double-spiral strip idea that we discussed beforerhitee05 wrote:You must have something serious in mind with the copper strips in those windings.




Miles wrote:I've always wanted to try out the contiguous double-spiral strip idea that we discussed before

rhitee05 wrote:I can tell you've been thinking about this... you even have the laminations drawn in the right direction.
The idea was to brace the two rotors against each other as close to the inside of the core as possible so, the axial forces will be neutralised with respect to the bearings and things will be as rigid as possible around the rim...rhitee05 wrote:I'm curious what you have planned for the mechanical design (if you've thought that far ahead). If you use big magnets to match those coils, some serious thrust bearings and lateral stiffness of the rotor are in order!



Definitely laminations. The idea is to have the minimum of iron so that it's close to saturation at max. continuous torque. No dedicated flux return path, minimum cross-section and thinnest laminations = low parasitic torquepelle242 wrote:Any plans on how to get the stators made? Laminations or iron powder?

Miles wrote:The idea was to brace the two rotors against each other as close to the inside of the core as possible so, the axial forces will be neutralised with respect to the bearings and things will be as rigid as possible around the rim...
Miles wrote:Definitely laminations. The idea is to have the minimum of iron so that it's close to saturation at max. continuous torque. No dedicated flux return path, minimum cross-section and thinnest laminations = low parasitic torque
Miles wrote:There's not much of a conduction path through the core, though....

Miles wrote:Definitely laminations. The idea is to have the minimum of iron so that it's close to saturation at max. continuous torque. No dedicated flux return path, minimum cross-section and thinnest laminations = low parasitic torquepelle242 wrote:Any plans on how to get the stators made? Laminations or iron powder?

Yes, it would definitely be worth experimenting with that - especially in combination with opening up the case ends and sucking air in through the rotors, using some sort of integral axial fan arrangement.rhitee05 wrote: Perhaps a better idea would be to design the bracing structure for the rotors like a squirrel-cage fan and just pump lots of air between the coils?

That would be a great help, Eric. I'd also appreciate advice on calculating the right balance between the iron and copper volumes.rhitee05 wrote: If you want it, I can probably help you try to estimate those axial forces when you get closer to the design phase, unless you just want to over-engineer the snot out of it!![]()


Good point. I've know idea how detrimental that would be? I guess one could curve the laminations. Maybe even as part of the stamping process?liveforphysics wrote:Any concerns about flux lines cutting through at an angle to the lam stack, as the lam stack isn't curved but flat?

Thanks Marko. I'll look it up.markobetti wrote: Finally you started this , i think aial flux design is underrated today . i bought axel borg book - diy - nice chapters there - you should look it up . Laters Axel design was based on dual rotors with mags i think


liveforphysics wrote:Any concerns about flux lines cutting through at an angle to the lam stack, as the lam stack isn't curved but flat?


I seem to remember modelling something like that on the single rotor design. Unless there's a significant gain it would be nice to keep all the laminations identical. I should imagine it would be more beneficial if you were using SMC cores?rhitee05 wrote:If you wanted to be really fancy, you could shape the ends such that the flare is wider on the outside edge of the core and narrower on the inner, making the end somewhat more wedge shaped (looking axially). Again, not entirely certain how much benefit this would provide (this is a 3D geometry, so would be difficult to simulate using the freeware) and would make fabrication more difficult.

Miles wrote:I seem to remember modelling something like that on the single rotor design. Unless there's a significant gain it would be nice to keep all the laminations identical. I should imagine it would be more beneficial if you were using SMC cores?


rhitee05 wrote:liveforphysics wrote:Any concerns about flux lines cutting through at an angle to the lam stack, as the lam stack isn't curved but flat?
I suspect that this shouldn't be too significant so long as the pole count and radius are sufficiently large, so the angular size of each core is not very big. Looks like maybe 18 teeth/cores? Since Miles knows the dimensions, I'm sure he could figure out how much of a difference there is between the straight lams and the ideal arc. Probably not worth the trouble to do anything about, especially if the lams are made from thin electrical steel.
This is what it looks like with a 0.35mm lamination thickness (first two laminations from the inside):Miles wrote:It's only a 90mm motor. The minor diameter across the cores, as modelled, is 62mm. Major diameter 82.
Maximum deviation is 0.4mm across 10mm wide core.