Carbon fiber cloth. This is how carbon fiber bikes are done by DIY. Use several layers to create a very solid structure.
kfong
1 MW
1 MW
 
Posts: 1646
Joined: Tue Sep 02, 2008 11:34 am
Location: SE Michigan, USA

Re: New frame + Lipo

Postby gensem » Sat Feb 04, 2012 1:52 pm

Thanks, ll try if the glue fails...
The glued area is big, like 1,5inch x 4inch hoping it doesnt fail on me.
have a look

Image
A decent 25mph bike will cost around $1000.
A decent 35mph bike will cost around $2000.
A $1000 35mph bike will get you killed.
Justin we really appreciate what you did!
User avatar
gensem
100 kW
100 kW
 
Posts: 1488
Joined: Fri Apr 01, 2011 5:28 pm
Location: Sao Paulo - Brasil

Re: New frame + Lipo

Postby kfong » Sat Feb 04, 2012 1:58 pm

Looks like you are adding a piece of half round aluminim tubing to the section. That should work too. Just as long as it conforms well to the area. I think you need to mix the epoxy.
Last edited by kfong on Sat Feb 04, 2012 2:01 pm, edited 1 time in total.
kfong
1 MW
1 MW
 
Posts: 1646
Joined: Tue Sep 02, 2008 11:34 am
Location: SE Michigan, USA

Re: New frame + Lipo

Postby Doctorbass » Sat Feb 04, 2012 1:59 pm

looking at the surface aream, you can hold tons of force without problem

But, iyt all depend on the precision you cleaned and grinded the surface to be bond.

If yo apply epoxy to painted surface, it will be as strong as thej paint bonding itself.

If you correctly grinded the paint to remove it all and have fresh aluminum or steel to bond, result should be perfect.

Doc
________________
-Fastest speed record from now: 113 km/h measured on GPS
-Fastest ebike 106km/h on flat and managed to enter in the 19.875 sec on the 1/4 mile drag racing !
-0-70km/h in 5sec X5 5303 on 24"
TORQUE SETUP:
-Succeded to haul a 19200 pounds schoolbus!
-Team Konion Member
113kmh Giant___http://www.evalbum.com/3406
Mongoose____http://www.evalbum.com/1947
E-trike_______ http://www.evalbum.com/3776
http://twitter.com/DocbassMelancon
I speak FRENCH and english
User avatar
Doctorbass
100 GW
100 GW
 
Posts: 6519
Joined: Sun Apr 08, 2007 2:24 am
Location: Quebec, Canada East

Re: New frame + Lipo

Postby gensem » Sat Feb 04, 2012 2:09 pm

Tube was not perfectly round, but the result should be good. I made sure to clean the surface with a hand steel brush. deviation is 0,6mm and it was filled with DP420.

Image
Last edited by gensem on Sat Feb 04, 2012 2:43 pm, edited 1 time in total.
A decent 25mph bike will cost around $1000.
A decent 35mph bike will cost around $2000.
A $1000 35mph bike will get you killed.
Justin we really appreciate what you did!
User avatar
gensem
100 kW
100 kW
 
Posts: 1488
Joined: Fri Apr 01, 2011 5:28 pm
Location: Sao Paulo - Brasil

Re: New frame + Lipo

Postby kfong » Sat Feb 04, 2012 2:31 pm

Looks like a lot of contours to deal with giving you pockets of epoxy. I think I would of gone with layers of carbon fiber. But you have to isolate the carbon from aluminum due to electrolysis. A separating layer of fiberglass can be used. So it would be a coin toss as to what would work better. You can use carbon tow (rope) as a wrap to go around the bottom bracket. That would be a better way to structurally secure it.
kfong
1 MW
1 MW
 
Posts: 1646
Joined: Tue Sep 02, 2008 11:34 am
Location: SE Michigan, USA

Re: New frame + Lipo

Postby Doctorbass » Sat Feb 04, 2012 5:03 pm

It is preferable to use EC2216 epoxy for carbon fiber. but it is less strong with aluminum and steel... no real trade off for both carbon fiber and steel or aluminum.


The EC2216 is also a 3M scotchweld structural epoxy like the DP420 but is a little bit softer.

The 2216 is used by the aerospace since the 60'

Doc
________________
-Fastest speed record from now: 113 km/h measured on GPS
-Fastest ebike 106km/h on flat and managed to enter in the 19.875 sec on the 1/4 mile drag racing !
-0-70km/h in 5sec X5 5303 on 24"
TORQUE SETUP:
-Succeded to haul a 19200 pounds schoolbus!
-Team Konion Member
113kmh Giant___http://www.evalbum.com/3406
Mongoose____http://www.evalbum.com/1947
E-trike_______ http://www.evalbum.com/3776
http://twitter.com/DocbassMelancon
I speak FRENCH and english
User avatar
Doctorbass
100 GW
100 GW
 
Posts: 6519
Joined: Sun Apr 08, 2007 2:24 am
Location: Quebec, Canada East

Re: New frame + Lipo

Postby Doctorbass » Sat Feb 04, 2012 5:04 pm

I can say... no need of filling with carbon fiber.. the DP420 is REALLY strong!

The DP420 is also a structural adhesive

Doc
________________
-Fastest speed record from now: 113 km/h measured on GPS
-Fastest ebike 106km/h on flat and managed to enter in the 19.875 sec on the 1/4 mile drag racing !
-0-70km/h in 5sec X5 5303 on 24"
TORQUE SETUP:
-Succeded to haul a 19200 pounds schoolbus!
-Team Konion Member
113kmh Giant___http://www.evalbum.com/3406
Mongoose____http://www.evalbum.com/1947
E-trike_______ http://www.evalbum.com/3776
http://twitter.com/DocbassMelancon
I speak FRENCH and english
User avatar
Doctorbass
100 GW
100 GW
 
Posts: 6519
Joined: Sun Apr 08, 2007 2:24 am
Location: Quebec, Canada East

Re: New frame + Lipo

Postby fabiograssi » Sat Feb 04, 2012 5:18 pm

+1 on only 420. That adhesive is a beast!

Doctorbass wrote:I can say... no need of filling with carbon fiber.. the DP420 is REALLY strong!

The DP420 is also a structural adhesive

Doc
User avatar
fabiograssi
100 W
100 W
 
Posts: 266
Joined: Sun Jun 14, 2009 9:42 am
Location: Bauru, Sao Paulo, Brazil

Re: New frame + Lipo

Postby gensem » Sun Feb 05, 2012 8:21 am

More dp420 to fix Doc torque arms.

Image

Image
A decent 25mph bike will cost around $1000.
A decent 35mph bike will cost around $2000.
A $1000 35mph bike will get you killed.
Justin we really appreciate what you did!
User avatar
gensem
100 kW
100 kW
 
Posts: 1488
Joined: Fri Apr 01, 2011 5:28 pm
Location: Sao Paulo - Brasil

Re: New frame + Lipo

Postby GCinDC » Mon Feb 06, 2012 10:30 am

replacement frame - sweet!

is this the old frame w/ cromotor from that thread?
Image
if so, what happened to the frame? looks like it got crushed..

did you just send a pic of swing arm crack to seller to get the replacement? awesome...
Youtube channel, 2011 Highlights vid. Ebike Nerdcast.
Giant DH Comp: 20s lipo (10Ah), hs3540, 72V 45A 12FET, 900W BMSBattery charger.
GT I-Drive, 20s lipo, 9C, 72V 45A 12FET.
User avatar
GCinDC
1 GW
1 GW
 
Posts: 3459
Joined: Fri Jan 23, 2009 11:19 am
Location: Washington, DC

Re: New frame + Lipo

Postby gensem » Mon Feb 06, 2012 10:39 am

Yes, its the same frame only the color differs.
I ended welding some pieces to the frame to find out the heat plus a very small pressure cracked the swingarm bushing.
Its looking bad because I sorta beat the frame when I saw the crack.
I was willing to pay for a new frame but the seller asked just a hundred bucks for shipping and that was after I told him the frame was modded and thats why it cracked.


GCinDC wrote:replacement frame - sweet!

is this the old frame w/ cromotor from that thread?
Image
if so, what happened to the frame? looks like it got crushed..

did you just send a pic of swing arm crack to seller to get the replacement? awesome...
A decent 25mph bike will cost around $1000.
A decent 35mph bike will cost around $2000.
A $1000 35mph bike will get you killed.
Justin we really appreciate what you did!
User avatar
gensem
100 kW
100 kW
 
Posts: 1488
Joined: Fri Apr 01, 2011 5:28 pm
Location: Sao Paulo - Brasil

Re: New frame + Lipo

Postby gensem » Sat Feb 11, 2012 10:57 am

Sneak peek

Image

Should have something running(testing) tomorrow.
You know what a big fork and 24" makes me think..... alot of room for batteries under the down tube, might worth testing later,
A decent 25mph bike will cost around $1000.
A decent 35mph bike will cost around $2000.
A $1000 35mph bike will get you killed.
Justin we really appreciate what you did!
User avatar
gensem
100 kW
100 kW
 
Posts: 1488
Joined: Fri Apr 01, 2011 5:28 pm
Location: Sao Paulo - Brasil

Re: New frame + Lipo

Postby BATFINK » Sat Feb 11, 2012 6:36 pm

Looking good gens em, what made you decide to weld that battery holder plate straight onto the headset instead of the clamps like what Oatnet did with his? I think I'm going to do a similar mount of my batteries but I will try to think of a way to do it so the battery box is removable for charging.

Sent using Endless-Sphere Mobile app
User avatar
BATFINK
10 kW
10 kW
 
Posts: 593
Joined: Sun Aug 07, 2011 5:17 pm

Re: New frame + Lipo

Postby BATFINK » Sat Feb 11, 2012 6:37 pm

How many volts and amps can you fit into that pelican case?

Sent using Endless-Sphere Mobile app
User avatar
BATFINK
10 kW
10 kW
 
Posts: 593
Joined: Sun Aug 07, 2011 5:17 pm

Re: New frame + Lipo

Postby gensem » Sat Feb 11, 2012 7:37 pm

BATFINK wrote:Looking good gens em, what made you decide to weld that battery holder plate straight onto the headset instead of the clamps like what Oatnet did with his? I think I'm going to do a similar mount of my batteries but I will try to think of a way to do it so the battery box is removable for charging.

Sent using Endless-Sphere Mobile app


Its not welded, it was glued with DP420. I think they weight would mess with the bike handling.
I did not think about doing a removable mount, but I might come with something diferent at a later date.
A decent 25mph bike will cost around $1000.
A decent 35mph bike will cost around $2000.
A $1000 35mph bike will get you killed.
Justin we really appreciate what you did!
User avatar
gensem
100 kW
100 kW
 
Posts: 1488
Joined: Fri Apr 01, 2011 5:28 pm
Location: Sao Paulo - Brasil

Re: New frame + Lipo

Postby gensem » Sat Feb 11, 2012 7:40 pm

BATFINK wrote:How many volts and amps can you fit into that pelican case?

Sent using Endless-Sphere Mobile app



im fitting 24s 2p of zippy 8000mah (hobbyking lipo)
90v x 16a = ~1500wh
1100-1200wh usable 80%DOD
A decent 25mph bike will cost around $1000.
A decent 35mph bike will cost around $2000.
A $1000 35mph bike will get you killed.
Justin we really appreciate what you did!
User avatar
gensem
100 kW
100 kW
 
Posts: 1488
Joined: Fri Apr 01, 2011 5:28 pm
Location: Sao Paulo - Brasil

Re: New frame + Lipo

Postby BATFINK » Sat Feb 11, 2012 7:42 pm

Thanks that's great. Keep up the god work

Sent using Endless-Sphere Mobile app
User avatar
BATFINK
10 kW
10 kW
 
Posts: 593
Joined: Sun Aug 07, 2011 5:17 pm

Re: New frame + Lipo

Postby oatnet » Mon Feb 13, 2012 11:37 am

gensem wrote:Its not welded, it was glued with DP420.


What a great idea gensem! :shock: Here I have been toying with the idea of welding a block like yours onto my second frame, weighing concerns about deforming the headtube and the need for heat treating, and I never once considered using the DP420 epoxy Doc has been recommending for his torque plates. Gensem, you just advanced the design of front-mount batteries again. :D Heck, instead of needing a double-crown fork for mounting, a single-crown fork will let you mount the box even closer.

Thanks!
-JD <--------- pondering the implications
Member 117 of 16,xxx

179v VW Camper © 164v Vectrix E-Moto © 72v Norco A-line/x5403 © 60v Specialized Enduro Comp/BMC © 72v x5tracycle © 48v TF IO/BMC © 36v Kepler Friction Drive © Spot-Welding a123 © Pelican Front Packs © Vectrix Battery Replacement © MORE !!


Image大鸡巴 Motors
Knowledge is acquired through experience, everything else is just information - Albert Einstein
"Cheater?" I'm not competing, I'm Commuting!
User avatar
oatnet
100 MW
100 MW
 
Posts: 2507
Joined: Thu Apr 26, 2007 3:03 pm
Location: SoCal, USA

Re: New frame + Lipo

Postby gensem » Mon Feb 13, 2012 5:28 pm

oatnet wrote:
gensem wrote:Its not welded, it was glued with DP420.


What a great idea gensem! :shock: Here I have been toying with the idea of welding a block like yours onto my second frame, weighing concerns about deforming the headtube and the need for heat treating, and I never once considered using the DP420 epoxy Doc has been recommending for his torque plates. Gensem, you just advanced the design of front-mount batteries again. :D Heck, instead of needing a double-crown fork for mounting, a single-crown fork will let you mount the box even closer.

Thanks!
-JD <--------- pondering the implications


Hehe... Dont weld it, I dont think all the headaches are worth... try DP420, I think its strong enough, and ll find ouy next weekend. :)
Wont deny I have a steel cable hooked up just in case my lipos decide to fly.
To be truth I like the box far because it good against wheelies, but It odd to not see the front wheel. I need to finish the bicycle assembly so test it further. If I find it bad while riding I ll swap the fork for a single crown.

Btw the pelican is somehow removable now, and lipos ll probably be perma paralleled because I dont have room inside the box for all thoses wires.

Regards
Last edited by gensem on Wed Feb 22, 2012 8:46 am, edited 1 time in total.
A decent 25mph bike will cost around $1000.
A decent 35mph bike will cost around $2000.
A $1000 35mph bike will get you killed.
Justin we really appreciate what you did!
User avatar
gensem
100 kW
100 kW
 
Posts: 1488
Joined: Fri Apr 01, 2011 5:28 pm
Location: Sao Paulo - Brasil

Re: New frame + Lipo

Postby gensem » Tue Feb 14, 2012 8:28 pm

Couple more cell phone pictures. Folks, please remind me to not do everything custom next time... Its alot more work that I could dream off.

Image

Image
A decent 25mph bike will cost around $1000.
A decent 35mph bike will cost around $2000.
A $1000 35mph bike will get you killed.
Justin we really appreciate what you did!
User avatar
gensem
100 kW
100 kW
 
Posts: 1488
Joined: Fri Apr 01, 2011 5:28 pm
Location: Sao Paulo - Brasil

Re: New frame + Lipo

Postby fabiograssi » Tue Feb 14, 2012 8:38 pm

Hey, Gensem, that's a "honda CG" horn in your machine???? Oh, what a dream if I was in traffic at Rebouças avenue and a cromota beast pass by horning insanely!!!!!

Nice build, my friend!!!!

:mrgreen:
User avatar
fabiograssi
100 W
100 W
 
Posts: 266
Joined: Sun Jun 14, 2009 9:42 am
Location: Bauru, Sao Paulo, Brazil

Re: New frame + Lipo

Postby gensem » Fri Feb 17, 2012 10:39 pm

small update... did my first run today using a 12fet controller 100v and 50phase amps... even with a shitload of weight in the fork I keep seeing the sky easily aside that the throttle is too frocking sensible, like a wild animal. I was a short ride, but was breath taking...
Will try to use capacitive throttle later and fix some other stuff I just found out.
Last edited by gensem on Wed Feb 22, 2012 8:56 am, edited 1 time in total.
A decent 25mph bike will cost around $1000.
A decent 35mph bike will cost around $2000.
A $1000 35mph bike will get you killed.
Justin we really appreciate what you did!
User avatar
gensem
100 kW
100 kW
 
Posts: 1488
Joined: Fri Apr 01, 2011 5:28 pm
Location: Sao Paulo - Brasil

Re: New frame + Lipo

Postby oatnet » Sat Feb 18, 2012 11:35 am

gensem wrote:small update... did my first run today using a 12fet controller 100v and 50phase amps... even with a shitload of weight in the fork I keep seeing the sky easily aside that the throttle is too frocking sensible, like a wild animal. I was a short ride, but was breath taking...
Will try to use capacitive throttle tmr and fix some other stuff I just found out.


Yep, that is why I wanted the 13kv winding instead of the 9kv. Once you reduce rim diameter enough to get the 9kv into a Moto tire that is safe at the speeds it can generate, the torque is enough to impact drivability for my style of riding. OTOH, there are a lot of people who like having the front wheel off the ground as much as possible, this winding is great for them.

Throttle response can often be attributed to the controller. Kelly controllers have a setting to reduce throttle response, that helps. As an alternative, you could try reducing power. :cry:

-JD
Member 117 of 16,xxx

179v VW Camper © 164v Vectrix E-Moto © 72v Norco A-line/x5403 © 60v Specialized Enduro Comp/BMC © 72v x5tracycle © 48v TF IO/BMC © 36v Kepler Friction Drive © Spot-Welding a123 © Pelican Front Packs © Vectrix Battery Replacement © MORE !!


Image大鸡巴 Motors
Knowledge is acquired through experience, everything else is just information - Albert Einstein
"Cheater?" I'm not competing, I'm Commuting!
User avatar
oatnet
100 MW
100 MW
 
Posts: 2507
Joined: Thu Apr 26, 2007 3:03 pm
Location: SoCal, USA

Re: New frame + Lipo

Postby BATFINK » Sat Feb 18, 2012 1:18 pm

Hello gensem, can you tell me what voltage that electric horn is? is it just a standard 12 motorcycle horn? did you use some sort of converter to step the voltage down for it or are you running a separate battery for the horn? I have 48 Volt battery pack is there any electric horns that will work on that voltage?
Thanks
User avatar
BATFINK
10 kW
10 kW
 
Posts: 593
Joined: Sun Aug 07, 2011 5:17 pm

PreviousNext

Return to E-Bike General Discussion

Who is online

Users browsing this forum: EdwardNY, Google [Bot], guting, mikebikerad, rp3, triggeraa and 8 guests