Postby amberwolf » Fri Feb 10, 2012 9:01 pm

methods wrote:They get hot, but not so hot that it takes your skin off. 100C

So at least I can make my tea with the thing. Just dip it in waterproofing first, then insert into my cup with a teabag, and wait. By the time balancing is done on some really big and badly abused pack, I can sit back and sip away. ;)
House Fire Updates Thread


Got a question that isn't personal or private? Post it in the forums, don't PM it. ;)

Wiki your techy info so it doesn't get old, lost and icky:
http://endless-sphere.com/w


Full-Suspension Semi Recumbent Cargo Bike - NuVinci MidDrive
Semi-Recumbent Recycled-Parts Cargo eBike: "CrazyBike2"
DayGlo Avenger, MkII
User avatar
amberwolf
100 GW
100 GW
 
Posts: 13717
Joined: Mon Aug 17, 2009 6:43 am
Location: Phoenix, AZ, USA, Earth, Sol, Local Bubble, Orion Arm, Milky Way, Local Group

Re: Battery Medic - how to ID the REAL vs FAKE

Postby FastDemise » Fri Feb 10, 2012 9:03 pm

While testing are you having any issues with the screen getting too hot. I would get black discoloratin from the heat after about a hour.
21" Hardtail, Docs Torque Arm, Lipo 20s2p, ebikes.ca 9C 8x8 and Lyen 6fet (both Mineral Oil cooled)
User avatar
FastDemise
100 W
100 W
 
Posts: 202
Joined: Thu Aug 18, 2011 8:28 pm
Location: Hillsboro, OR USA

Re: Battery Medic - how to ID the REAL vs FAKE

Postby methods » Fri Feb 10, 2012 10:51 pm

Not at all - but I am keeping mine with the screen facing down so the heat can escape.

If they are set down face up (which is the most intuitive thing to do...) the heat just pools under the LCD.
I am considering drilling holes in the front cover to help let heat out as I suspect most people will set them face up even if we tell them to set it face down.

Still working on ideas over here.
I sure would like to just populate the empty space on the PCB and then improve the efficiency of the cooling design. Even just a moth flapping its wings would make all the difference here....

Awesome would = 250mA - 500mA diode to send the power away in the form of photons
Awesome would = tiny surface mount pager motor with a counterweight that could work the energy away mechanically
Awesome would = 2W fan on every channel - self cooling power dissipation
Awesome would = tiny DC-DC that would take the 4.2V from one channel and funnel it back as 25.2V to the pack

Maybe Poly fuses can play a role here... resistors are linear but the poly fuses would allow more current to flow with better cooling

Maybe we could utilize the duty cycle with tiny little transformers :)

Ok - back to finding a clean way to dump power the good ol'fashioned american way

-methods
Jozzer wrote:Your already the guy to go to for the guys that other guys go to..

I sell stuff.... like little morsels of my integrity @ http://www.MethodsTechnology.com
User avatar
methods
10 GW
10 GW
 
Posts: 4403
Joined: Fri Aug 08, 2008 12:08 pm
Location: Santa Cruz CA

Re: Battery Medic - how to ID the REAL vs FAKE

Postby sn0wchyld » Fri Feb 10, 2012 11:05 pm

rojitor wrote:
rui_fujino wrote:thanks alot! I got 4 from ebay (cheap! and turns out they have RED PCB! WIN!)
http://www.ebay.co.uk/itm/260753810568?ssPageName=STRK:MEWNX:IT&_trksid=p3984.m1439.l2649
This is where i got them from!

yay! That's the one i ordered

I ordered from them too, got the yellow/green model... so no consistency with that seller... :cry:


edit

I really love the idea of a dc-dc converter to send the power back to the pack as a whole. how hard would it be to build?

Im using the axial resistors, but I have them mounted at a 90deg angle to the board, so they stand up above the board. Seems to work quite well, though I've always run 'em face down and with a fan blowing over 'em. I think ill build a new case to mount em in with a couple of fans to keep things cool.
Last edited by sn0wchyld on Fri Feb 10, 2012 11:28 pm, edited 2 times in total.
Got questions? hit up the wiki!
http://www.endless-sphere.com/w/index.php/Main_Page

My builds:
http://endless-sphere.com/forums/viewtopic.php?f=3&t=29373
Norko Aline Park DH - Clyte HT3525 - 24s lipo
http://endless-sphere.com/forums/viewtopic.php?f=28&t=33657&p=534823#p534823
'02ish Avanti D8 - 8085 170kv - 5s 40ah lipo - ple80 recution
abject failure in september
http://endless-sphere.com/forums/viewtopic.php?f=12&t=43143
RC driven Electric mountainboard - New vids up!
User avatar
sn0wchyld
100 kW
100 kW
 
Posts: 1243
Joined: Fri Mar 18, 2011 8:27 pm
Location: South Aus.

Re: Battery Medic - how to ID the REAL vs FAKE

Postby methods » Fri Feb 10, 2012 11:23 pm

That seller is probably offering two different models with a small price difference. :)
I suggest searching his offerings.

-methods
Jozzer wrote:Your already the guy to go to for the guys that other guys go to..

I sell stuff.... like little morsels of my integrity @ http://www.MethodsTechnology.com
User avatar
methods
10 GW
10 GW
 
Posts: 4403
Joined: Fri Aug 08, 2008 12:08 pm
Location: Santa Cruz CA

Re: Battery Medic - how to ID the REAL vs FAKE

Postby sn0wchyld » Fri Feb 10, 2012 11:28 pm

methods wrote:That seller is probably offering two different models with a small price difference. :)
I suggest searching his offerings.

-methods



hahaha now that you mention it I think I may have searched his listings thinking 'why the hell does he have two difference prices for the 'same' thing... though that may have been another seller, bought them a month or two ago so cant really remember.
Got questions? hit up the wiki!
http://www.endless-sphere.com/w/index.php/Main_Page

My builds:
http://endless-sphere.com/forums/viewtopic.php?f=3&t=29373
Norko Aline Park DH - Clyte HT3525 - 24s lipo
http://endless-sphere.com/forums/viewtopic.php?f=28&t=33657&p=534823#p534823
'02ish Avanti D8 - 8085 170kv - 5s 40ah lipo - ple80 recution
abject failure in september
http://endless-sphere.com/forums/viewtopic.php?f=12&t=43143
RC driven Electric mountainboard - New vids up!
User avatar
sn0wchyld
100 kW
100 kW
 
Posts: 1243
Joined: Fri Mar 18, 2011 8:27 pm
Location: South Aus.

Re: Battery Medic - how to ID the REAL vs FAKE

Postby FastDemise » Fri Feb 10, 2012 11:33 pm

Haha, imagine the noise of 6 cellphone motors going crazy. One can make a whole phone shake around the table. 6 would make a great back massage. Just gotta get long balance wires. :)
21" Hardtail, Docs Torque Arm, Lipo 20s2p, ebikes.ca 9C 8x8 and Lyen 6fet (both Mineral Oil cooled)
User avatar
FastDemise
100 W
100 W
 
Posts: 202
Joined: Thu Aug 18, 2011 8:28 pm
Location: Hillsboro, OR USA

Re: Battery Medic - how to ID the REAL vs FAKE

Postby sn0wchyld » Sat Feb 11, 2012 12:15 am




were these prices for a certain quantity? I just contacted the same guy to confirm the $1499 one was the high quality and he's saying they're $16 for the high end ones....
Got questions? hit up the wiki!
http://www.endless-sphere.com/w/index.php/Main_Page

My builds:
http://endless-sphere.com/forums/viewtopic.php?f=3&t=29373
Norko Aline Park DH - Clyte HT3525 - 24s lipo
http://endless-sphere.com/forums/viewtopic.php?f=28&t=33657&p=534823#p534823
'02ish Avanti D8 - 8085 170kv - 5s 40ah lipo - ple80 recution
abject failure in september
http://endless-sphere.com/forums/viewtopic.php?f=12&t=43143
RC driven Electric mountainboard - New vids up!
User avatar
sn0wchyld
100 kW
100 kW
 
Posts: 1243
Joined: Fri Mar 18, 2011 8:27 pm
Location: South Aus.

Re: Battery Medic - how to ID the REAL vs FAKE

Postby amberwolf » Sat Feb 11, 2012 1:59 am

methods wrote:NIf they are set down face up (which is the most intuitive thing to do...) the heat just pools under the LCD.
I am considering drilling holes in the front cover to help let heat out as I suspect most people will set them face up even if we tell them to set it face down.

How about a little wire frame that normally sits around the body of the unit, but can be folded back outward at the bottom to make it stand up when in use, like a DMM or a mirror typically has?

Ok, a 5-minute version made from some solid copper house wiring I had out back. Would be better out of steel or something, but I cant' find any coat hangers or similar right now. I know I have some stainless thin wire that'd be perfect, long lever springs out of some copier or printer, but I have no idea where it's at.

There's a little hook on the left top piece that points toward the back, which makes it stay extended by sticking on the plastic. I actually meant to bend it *forwards) so it acts like a spring, but I screwed up. Still worked. :P

Of course, this only works for those charging their stuff on a table or other flat surface. :|
Attachments
DSC06082.JPG
DSC06082.JPG (46.86 KiB) Viewed 220 times
DSC06084.JPG
DSC06084.JPG (40.7 KiB) Viewed 220 times
DSC06087.JPG
DSC06087.JPG (41.57 KiB) Viewed 220 times
DSC06088.JPG
DSC06088.JPG (39.96 KiB) Viewed 220 times
DSC06089.JPG
DSC06089.JPG (73.32 KiB) Viewed 220 times
DSC06090.JPG
DSC06090.JPG (41.27 KiB) Viewed 220 times
House Fire Updates Thread


Got a question that isn't personal or private? Post it in the forums, don't PM it. ;)

Wiki your techy info so it doesn't get old, lost and icky:
http://endless-sphere.com/w


Full-Suspension Semi Recumbent Cargo Bike - NuVinci MidDrive
Semi-Recumbent Recycled-Parts Cargo eBike: "CrazyBike2"
DayGlo Avenger, MkII
User avatar
amberwolf
100 GW
100 GW
 
Posts: 13717
Joined: Mon Aug 17, 2009 6:43 am
Location: Phoenix, AZ, USA, Earth, Sol, Local Bubble, Orion Arm, Milky Way, Local Group

Re: Battery Medic - how to ID the REAL vs FAKE

Postby adrian_sm » Sat Feb 11, 2012 2:58 am

I have the Hobbyking Battery Medic, RED PCB, and it is ~20mV out. Enough for me to not trust it to balance correctly.

Here are the readings with Battery Medic, Cell Log, and a cheap Digital Multimeter.

6s LiPo

HobbyKing Battery Medic / HobbyKing Cell-Log / Cheap DMM
1 - 4.16 / 4.161 / 4.15
2 - 4.14 / 4.161 / 4.15
3 - 4.16 / 4.153 / 4.14
4 - 4.14 / 4.159 / 4.14
5 - 4.16 / 4.159 / 4.15
6 - 4.16 / 4.167 / 4.15
Build #1 ~28kg ~ 700w Avanti Hardtail Crystalyte 408, 48V10Ah Headway. ~5500 kms to date. (retired)
Build #2 ~30kg ~2000w Giant AC Dually Crystalyte 408, 48V10Ah Headway + 6s10Ah LiPo = 70V. ~15000 kms to date [SOLD]
Build #3 ~13kg ~2000w Commuter Booster <1kg Friction Drive in Beta testing (www.commuterbooster.com)
User avatar
adrian_sm
100 MW
100 MW
 
Posts: 2513
Joined: Mon Feb 23, 2009 12:54 am
Location: Melbourne, Australia

Re: Battery Medic - how to ID the REAL vs FAKE

Postby methods » Sat Feb 11, 2012 11:58 am

I bought a large lot - and why are you fussing over $1?
Chinese guys gotta eat..... it is this type of cheap consumer behavior (looking for the cheeeeeeeapest) that brings those garbage units to market. Just be grateful that you have the opportunity to buy a good one and pay what he asks.

-methods




sn0wchyld wrote:



were these prices for a certain quantity? I just contacted the same guy to confirm the $1499 one was the high quality and he's saying they're $16 for the high end ones....
Jozzer wrote:Your already the guy to go to for the guys that other guys go to..

I sell stuff.... like little morsels of my integrity @ http://www.MethodsTechnology.com
User avatar
methods
10 GW
10 GW
 
Posts: 4403
Joined: Fri Aug 08, 2008 12:08 pm
Location: Santa Cruz CA

Re: Battery Medic - how to ID the REAL vs FAKE

Postby methods » Sat Feb 11, 2012 12:01 pm

amberwolf wrote:Ok, a 5-minute version ...


I like that :mrgreen:

-methods
Jozzer wrote:Your already the guy to go to for the guys that other guys go to..

I sell stuff.... like little morsels of my integrity @ http://www.MethodsTechnology.com
User avatar
methods
10 GW
10 GW
 
Posts: 4403
Joined: Fri Aug 08, 2008 12:08 pm
Location: Santa Cruz CA

Re: Battery Medic - how to ID the REAL vs FAKE

Postby methods » Sat Feb 11, 2012 12:05 pm

It has already been shown that the Hobby City PCB is *different*
Yes, it is red, but it is a totally different design than those I reviewed above.

Lets get away from talking about RED vs YELLOW PCB's as this is not a good way to differentiate them.
Better to talk about where we sourced them from - or maybe some other method.

Why would you not trust it?
Accuracy and reliability are not necessarily related. A pack balanced to +/- 20mV is better than an unbalanced pack.
Reality is... most electronics are that sloppy. People just dont know it.

-methods




adrian_sm wrote:I have the Hobbyking Battery Medic, RED PCB, and it is ~20mV out. Enough for me to not trust it to balance correctly.

Here are the readings with Battery Medic, Cell Log, and a cheap Digital Multimeter.

6s LiPo

HobbyKing Battery Medic / HobbyKing Cell-Log / Cheap DMM
1 - 4.16 / 4.161 / 4.15
2 - 4.14 / 4.161 / 4.15
3 - 4.16 / 4.153 / 4.14
4 - 4.14 / 4.159 / 4.14
5 - 4.16 / 4.159 / 4.15
6 - 4.16 / 4.167 / 4.15
Jozzer wrote:Your already the guy to go to for the guys that other guys go to..

I sell stuff.... like little morsels of my integrity @ http://www.MethodsTechnology.com
User avatar
methods
10 GW
10 GW
 
Posts: 4403
Joined: Fri Aug 08, 2008 12:08 pm
Location: Santa Cruz CA

Re: Battery Medic - how to ID the REAL vs FAKE

Postby adrian_sm » Sat Feb 11, 2012 4:41 pm

methods wrote:Why would you not trust it?
Accuracy and reliability are not necessarily related. A pack balanced to +/- 20mV is better than an unbalanced pack. Reality is... most electronics are that sloppy. People just dont know it.


Fair call. I just balance with my charger now, which agrees with my Cell-Log & DMM.

Maybe once I start bulk charging more often, I'll stop being so anal about 0.02V.
Build #1 ~28kg ~ 700w Avanti Hardtail Crystalyte 408, 48V10Ah Headway. ~5500 kms to date. (retired)
Build #2 ~30kg ~2000w Giant AC Dually Crystalyte 408, 48V10Ah Headway + 6s10Ah LiPo = 70V. ~15000 kms to date [SOLD]
Build #3 ~13kg ~2000w Commuter Booster <1kg Friction Drive in Beta testing (www.commuterbooster.com)
User avatar
adrian_sm
100 MW
100 MW
 
Posts: 2513
Joined: Mon Feb 23, 2009 12:54 am
Location: Melbourne, Australia

Re: Battery Medic - how to ID the REAL vs FAKE

Postby methods » Sat Feb 11, 2012 6:29 pm

I used to fuss over my cell voltages - but after bulk charging about 500 times it is the last thing on my mind. I don't even really care if cells are at 4.3V... just so long as they are not below 3.0V with smoke coming out :)

-methods
Jozzer wrote:Your already the guy to go to for the guys that other guys go to..

I sell stuff.... like little morsels of my integrity @ http://www.MethodsTechnology.com
User avatar
methods
10 GW
10 GW
 
Posts: 4403
Joined: Fri Aug 08, 2008 12:08 pm
Location: Santa Cruz CA

Re: Battery Medic - how to ID the REAL vs FAKE

Postby sn0wchyld » Sat Feb 11, 2012 8:34 pm

nah your right that I shouldn't sweat a few $... more that I'd be pissed to end up with lower quality units if I'd paid extra, and getting a different price didn't fill me with confidence... I missed that you'd gotten a bulk discount too. nvm

how closely do you keep yours in balance anyhow? I generally don't worry about it till it gets over about 30-40mv, but I'd be interested to know the thoughts of someone with more lipo experience. 4.3v seems kinda high, but then I am a bit paranoid since my bike is usually inside.

methods wrote:I bought a large lot - and why are you fussing over $1?.......
Got questions? hit up the wiki!
http://www.endless-sphere.com/w/index.php/Main_Page

My builds:
http://endless-sphere.com/forums/viewtopic.php?f=3&t=29373
Norko Aline Park DH - Clyte HT3525 - 24s lipo
http://endless-sphere.com/forums/viewtopic.php?f=28&t=33657&p=534823#p534823
'02ish Avanti D8 - 8085 170kv - 5s 40ah lipo - ple80 recution
abject failure in september
http://endless-sphere.com/forums/viewtopic.php?f=12&t=43143
RC driven Electric mountainboard - New vids up!
User avatar
sn0wchyld
100 kW
100 kW
 
Posts: 1243
Joined: Fri Mar 18, 2011 8:27 pm
Location: South Aus.

Re: Battery Medic - how to ID the REAL vs FAKE

Postby Arlo1 » Sat Feb 11, 2012 8:39 pm

methods wrote:I used to fuss over my cell voltages - but after bulk charging about 500 times it is the last thing on my mind. I don't even really care if cells are at 4.3V... just so long as they are not below 3.0V with smoke coming out :)

-methods

Uhmm what about 0v with no smoke? I have 48 cells that are at 0v lol. :oops: Left my pack plugged into my bike while I was out of my shop for ~2 months in the cold... I would say it might have got to -5 degC but I think Either my controller was what drained it or I accidently left the power on and the CA drained them.
Dam! I did get ~400 cycles before this so not bad but I would have liked to get ~1000 cycles then better and cheaper batteries would be out. For my new pack I will be using methods LVC HVC system. I pounded my pack into the ground <1v a cell with full power trying to help a guy who I thought was my friend who crashed my brothers ebmx I just finished and lost his keys so I found them then had to search for buddy in the meenwhile I killed my lipo and when he crashed my bothers bike he wrecked some shit and never offered to pay for it so I asked if he would help at my shop to make up for it and he said he would need money for that :shock: :| IM done with that looser! End rant. Moral of story Use methods shit so you dont end up like me!
Thanks Justin of http://www.ebikes.ca/
Also a thanks to Methy at http://www.methtek.com/ :)
And Dave who has some good deals on STUF
RC lipo and most other types of Lithium batteries you MUST know your individual cell voltages while charging and discharging.
Batteries of all kinds need respect they can burn your house down, so don't sleep with them under your bed or any other were you cant afford smoke or fire!
[color=#FF0000][b][size=150]Never above 4.2v never below 2.7v EVER!!!
User avatar
Arlo1
100 GW
100 GW
 
Posts: 5225
Joined: Sun Apr 26, 2009 10:36 pm
Location: Nanaimo BC Canada

Re: Battery Medic - how to ID the REAL vs FAKE

Postby Hyena » Sat Feb 11, 2012 10:23 pm

methods wrote:Ok - here is prototype number 3

6.8ohm axial resistors
in parallel with stock resistors
4.2ohms total impedance
700mA balance current (after duty cycle)
1W developed on the external resistors

That's my preferred method - not having to mess with SMD components existing or otherwise is a big plus in my book.
Quick and easy and 700ma of balance current is pretty good for the majority of applications.

methods wrote:I used to fuss over my cell voltages - but after bulk charging about 500 times it is the last thing on my mind.

Yep, I used to be an adventurer like you, but then I took an arrow... hang on, wait :P
I'm the same, I used to carefully watch the balance but then after 100 bulk charges when nothing ever needed balancing I stopped bothering even checking! I bulk charge twice a day and every few months I check but I don't bother balancing unless they're more than 50mv out of whack. I bulk charge to 4.18v/cell average and sometimes the cells get up to 4.22 while others are 4.15 but meh, it's trivial. I rarely take my pack past 80% discharge so in practise it's of little consequence. Mind you, I tell noobs and others others to carefully check the balance. Do as I say, not as I do :P

Oh, and that supplier that you suggested methy is the same one I've been buying from for months. An alignment in the force across the globe, no doubt :P
www.HyenaElectricBikes.com
Aussie high powered and custom e-bike kits
My build and HD video thread__. My youtube channel
My bike is writing cheques my body can't cash...
User avatar
Hyena
10 GW
10 GW
 
Posts: 4152
Joined: Wed Aug 13, 2008 9:10 am
Location: Sydney, Australia

Re: Battery Medic - how to ID the REAL vs FAKE

Postby methods » Sun Feb 12, 2012 12:01 am

That is an alignment in the force...

He is a good guy. His English comes through Google Translate - and it is terrible - but he is smart and honest. Can't ask for more than that. I think we should cultivate him into our new Kenny/Keywin replacement. Both of those guys stuck it in my butt the last time we did business - and I am still a little sore.

-methods
Jozzer wrote:Your already the guy to go to for the guys that other guys go to..

I sell stuff.... like little morsels of my integrity @ http://www.MethodsTechnology.com
User avatar
methods
10 GW
10 GW
 
Posts: 4403
Joined: Fri Aug 08, 2008 12:08 pm
Location: Santa Cruz CA

Re: Battery Medic - how to ID the REAL vs FAKE

Postby nicobie » Sun Feb 12, 2012 2:07 pm

It would be nice to have a replacement for those 2 characters. I got a kick when the 9c motors took off. Prices sure went down, didn't they... :|
Image

May your tote always stay tight and your edge eversharp :wink:

my eTownie build thread: viewtopic.php?f=6&t=23701
User avatar
nicobie
1 MW
1 MW
 
Posts: 1816
Joined: Thu Aug 07, 2008 1:48 pm
Location: Central Coast CA,USA

Re: Battery Medic - how to ID the REAL vs FAKE

Postby neptronix » Sun Feb 12, 2012 2:47 pm

IMHO...

A quality battery balancer, capable of balancing within 10+/- mV, and doing so fairly quickly, is worth well over double the cost of these units to me.

http://www.electrifly.com/miscproducts/gpmm3210.html

This is the closest i've came to that ideal. Super accurate, but painfully slow.

I'd happily fork over for a well calibrated battery medic with some uber resistors on it. About $50 is where i'd start to cry though. :)
ES facebook group: http://facebook.com/#!/home.php?sk=group_125035107565566&ap=1

The all-arounder: 8T MAC motor on a Trek 4500.
The girlfriend bike: 350W front MAC on a 700c Trek.
The wheelie machine: 20" Rear Magic Pie II on a Trek 4300 MTB
The Bus: ??? on a 'da bomb' cargo bike frame

Pro-tips for noobs: Avoid BMS Battery like the plague | Charge RC Lipos to 4.15v, stop discharging at 3.5-3.6v | Use torque plates/arms! | Rear mounted hubs are always best
User avatar
neptronix
100 GW
100 GW
 
Posts: 10292
Joined: Tue Jun 15, 2010 5:56 pm
Location: Salt Lake City, Utah

Re: Battery Medic - how to ID the REAL vs FAKE

Postby texaspyro » Sun Feb 12, 2012 3:58 pm

Make the stand out of shape memory alloy. The unit sits vertical when cool and you can read the screen. Turns LED side down when it heats up.
texaspyro
1 MW
1 MW
 
Posts: 1539
Joined: Wed May 12, 2010 6:53 pm

Re: Battery Medic - how to ID the REAL vs FAKE

Postby izeman » Thu Feb 16, 2012 4:55 am

chroot wrote:... I bought 14 dollars with free shipping from ebay under HKRC (seller name). He is excellent guy and easy communication.


thanks. that saved me from buying a bad one. just ordered one from HKRC. really good price and ww p&p included.
bmc trailfox, mac12t, 12s lipo: viewtopic.php?f=6&t=32267
klein mantra, hs3540, 24s lifepo4, 20" rims: http://endless-sphere.com/forums/viewto ... =3&t=38848
User avatar
izeman
10 kW
10 kW
 
Posts: 916
Joined: Tue Jun 21, 2011 8:25 am
Location: vienna, austria

Re: Battery Medic - how to ID the REAL vs FAKE

Postby rojitor » Thu Feb 16, 2012 7:10 am

Seems hobbyking has stock again.
User avatar
rojitor
10 kW
10 kW
 
Posts: 566
Joined: Wed Mar 23, 2011 6:39 pm
Location: vigo spain

Re: Battery Medic - how to ID the REAL vs FAKE

Postby izeman » Thu Feb 16, 2012 9:06 am

rojitor wrote:Seems hobbyking has stock again.

yep. but they don't send for free. which is a great benefit it you don't have a big order where you can add something like a small battery medic.
bmc trailfox, mac12t, 12s lipo: viewtopic.php?f=6&t=32267
klein mantra, hs3540, 24s lifepo4, 20" rims: http://endless-sphere.com/forums/viewto ... =3&t=38848
User avatar
izeman
10 kW
10 kW
 
Posts: 916
Joined: Tue Jun 21, 2011 8:25 am
Location: vienna, austria

PreviousNext

Return to Battery Technology