Dual rotor axial flux motor design

Electric Motors and Controllers

Re: Dual rotor axial flux motor design

Postby Miles » Wed Mar 21, 2012 5:41 am

OD increased from 92mm to 100mm
Electrical loading increased. Rm is now circa 4 milliohms.
Kv <150 rpm/V
Nominal speed 4000rpm
Flux frequency at nominal speed 533 Hz
Core volume 8.5222E4 cubic mm
Core mass 0.672 kg
User avatar
Miles
100 GW
100 GW
 
Posts: 9257
Joined: Fri Mar 16, 2007 4:15 pm
Location: London UK

Re: Dual rotor axial flux motor design

Postby fechter » Wed Mar 21, 2012 8:12 am

You might need some kind of housing to connect the two end plates together. Lamination stacks are not very rigid. There could be some eddy currents in the screws holding the lams together, but it should be fairly minimal. Normally they try to avoid having the fasteners in the teeth. It would be a lot of work, but it might be worth using some kind of adhesive between the laminations.
"One test is worth a thousand opinions"
User avatar
fechter
100 GW
100 GW
 
Posts: 9357
Joined: Sun Dec 31, 2006 3:23 pm
Location: California Bay Area, USA

Re: Dual rotor axial flux motor design

Postby Miles » Wed Mar 21, 2012 8:41 am

fechter wrote:It would be a lot of work, but it might be worth using some kind of adhesive between the laminations.
I definitely want to bond the laminations together. At the moment, the plan is to get the 75+ different lamination profiles laser cut and bonded into core modules. Haven't had a quote yet, though :mrgreen:
User avatar
Miles
100 GW
100 GW
 
Posts: 9257
Joined: Fri Mar 16, 2007 4:15 pm
Location: London UK

Re: Dual rotor axial flux motor design

Postby Miles » Wed Mar 21, 2012 9:07 am

Can I get a very rough approximation of the iron losses from the Watts per lb value given in the electrical steel specifications?

For Arnolds thin gauge GO 6mil (0.15mm) @ 15kG (1.5T); 400 Hz the losses are 9 Watts per lb.

My core weighs 1.48lbs. So, that's 13.5 Watts @ 1.5T; 400 Hz.

Say, 21 Watts at 533 Hz 1.5T.

Increase that to 25 Watts to allow for the greater flux density.

Increase again to 30 Watts to allow for stray, windage and bearing losses...
User avatar
Miles
100 GW
100 GW
 
Posts: 9257
Joined: Fri Mar 16, 2007 4:15 pm
Location: London UK

Re: Dual rotor axial flux motor design

Postby Miles » Wed Mar 21, 2012 9:40 am

This is what the above figures look like in Drive Calc...... :shock:
Attachments
Drive-Calc-graph-1.jpg
Drive-Calc-graph-1.jpg (135.34 KiB) Viewed 687 times
User avatar
Miles
100 GW
100 GW
 
Posts: 9257
Joined: Fri Mar 16, 2007 4:15 pm
Location: London UK

Re: Dual rotor axial flux motor design

Postby Miles » Wed Mar 21, 2012 2:58 pm

Couldn't resist... :)

Looks a bit "steampunk"
Attachments
Render-4.jpg
Render-4.jpg (207.42 KiB) Viewed 581 times
User avatar
Miles
100 GW
100 GW
 
Posts: 9257
Joined: Fri Mar 16, 2007 4:15 pm
Location: London UK

Re: Dual rotor axial flux motor design

Postby fechter » Wed Mar 21, 2012 9:49 pm

If the efficiency comes even close to the simulation it will be awesome. Most of us are dealing with 80% max.
"One test is worth a thousand opinions"
User avatar
fechter
100 GW
100 GW
 
Posts: 9357
Joined: Sun Dec 31, 2006 3:23 pm
Location: California Bay Area, USA

Re: Dual rotor axial flux motor design

Postby markobetti » Thu Mar 22, 2012 5:00 am

Miles wrote:Couldn't resist... :)

Looks a bit "steampunk"



i love it . Its going to make a beautiful BUH motor . By the way we have LAH 00000009 on board :)
markobetti
10 kW
10 kW
 
Posts: 769
Joined: Fri Jul 17, 2009 1:28 am

Re: Dual rotor axial flux motor design

Postby Doctor » Fri Mar 30, 2012 12:35 am

HI all,
Maybe I am wrong, but to me it looks like the laminate direction in this design is wrong: look at the Apex drive lab's stator pictures ( http://www.apexdrivelabs.com/brushless- ... mages.html ), each ply of the laminate is oriented in radial direction.
On other hand I know that in other types of axial flux machines (for instance, in Thorus topology) the laminate oriented perpendicularly to the radial direction. Why is it so?
Doctor
1 µW
1 µW
 
Posts: 4
Joined: Fri Mar 30, 2012 12:21 am

Re: Dual rotor axial flux motor design

Postby Miles » Fri Mar 30, 2012 1:43 am

Welcome Doc!

This is the orientation that corresponds to the lamination direction in a radial flux motor. Most axial flux motors have laminations running circumferentially (spiral wound). In the Schiller design, which has a segmented stator, the laminations run this way. AFAIK, it is the optimum orientation for the containment of eddy currents.

Surely the apparent twin cores in the Apex design must be contiguous (a "U" shape)? So, in their case, the laminate direction would be a compromise to achieve the topology.

Other motors (eg Lynch) have the laminations running radially, so it can't be too much of a compromise.

I'd like to know more about this, too!
User avatar
Miles
100 GW
100 GW
 
Posts: 9257
Joined: Fri Mar 16, 2007 4:15 pm
Location: London UK

Re: Dual rotor axial flux motor design

Postby Miles » Fri Mar 30, 2012 2:42 am

This is interesting...
http://www.set.ugent.be/docs/TO_HEAF_v2.pdf

That makes 3 ways to equalise the radial flux density:

- Equalise, per lamination, the ratio of the cross sections of the core "head" to core "neck" .

- Reduce magnet area as radius decreases (only applicable in the case where the no. of poles is less than no.of slots).

- Reduce the airgap distance as radius increases (Ghent university proposal).
User avatar
Miles
100 GW
100 GW
 
Posts: 9257
Joined: Fri Mar 16, 2007 4:15 pm
Location: London UK

Re: Dual rotor axial flux motor design

Postby Miles » Fri Mar 30, 2012 5:14 am

Axial-flux permanent-magnet machine modeling, design, simulation and analysis.
A. Mahmoudi*, N. A. Rahim and W. P. Hew
Attachments
Mahmoudi et al.pdf
(1.03 MiB) Downloaded 63 times
User avatar
Miles
100 GW
100 GW
 
Posts: 9257
Joined: Fri Mar 16, 2007 4:15 pm
Location: London UK

Re: Dual rotor axial flux motor design

Postby Miles » Fri Mar 30, 2012 6:37 am

Adopting the US vernacular....: Woot! :D

Comparison of Nonoriented and Grain-Oriented Material in an Axial Flux
Permanent-Magnet Machine

Damian Kowal, Peter Sergeant, Luc Dupré, and Alex Van den Bossche

V. CONCLUSION
For an AFPMSM whose stator flux is flowing in axial direction
in the major part of the stator, GO material was compared
with NO material. With GO material, the machine has about 7
times less iron loss at the same speed, and a 10% higher torque
for the same current. Nevertheless, the EMF at no-load is almost
the same for both materials. For a given torque, the GO material
causes a 10% higher torque-to-current ratio which makes
it possible to reduce the copper losses—quadratic with the current—
by about 20%. Alternatively, because of the lower iron
losses, it is possible with GO material to allow larger copper
losses without increasing the temperature of the machine. This
means a higher stator current and more torque.We conclude that
for the considered type of PMSM, it is worth the extra cost to
use GO material.
Attachments
GO vs NGO.pdf
(948.16 KiB) Downloaded 35 times
User avatar
Miles
100 GW
100 GW
 
Posts: 9257
Joined: Fri Mar 16, 2007 4:15 pm
Location: London UK

Re: Dual rotor axial flux motor design

Postby Miles » Fri Mar 30, 2012 7:06 am

Optimized Design Considering the Mass Influence of an Axial
Flux Permanent-Magnet Synchronous Generator
With Concentrated Pole Windings

Hendrik Vansompel, Peter Sergeant and Luc Dupré
Attachments
4101vans.pdf
(791.94 KiB) Downloaded 48 times
User avatar
Miles
100 GW
100 GW
 
Posts: 9257
Joined: Fri Mar 16, 2007 4:15 pm
Location: London UK

Re: Dual rotor axial flux motor design

Postby bearing » Fri Mar 30, 2012 7:45 am

Very nice finds!

Considering the amount of academic research done on axial flux motors, and the obvious advantages they have, I'm a bit confused to why there are so few axial flux motors available/produced/used commercially.
bearing
1 kW
1 kW
 
Posts: 449
Joined: Wed Dec 24, 2008 2:14 am

Re: Dual rotor axial flux motor design

Postby kenkad » Fri Mar 30, 2012 8:14 am

Miles,
The end of the third paragraph on the Ghent papers says:
"contentrated pole windings----A disadvantage is that for a three-phase machine several windings should be connected in series. When connecting n concentrated windings in series, the total electromotive force is not n times the voltage of a single winding, because of phase shift in the neighboring windings. An atlternative is to make a machine with many phases [3]."

This is what I had tried to bring up earlier. I had see this paper before but had not copied it at that time. Thank you for posting it here so now I can make a copy and give it to the PhD student that hopefully will do my modeling/simulation soon. I believe that a nine phase motor cited in the reference above is bsically the same as three separate three-phase windings. I do know in my design that it reduces the required drive of each three-phase group.
kenkad
kenkad
10 W
10 W
 
Posts: 73
Joined: Mon Oct 12, 2009 9:36 pm
Location: Union Grove, AL, USA

Re: Dual rotor axial flux motor design

Postby bearing » Fri Mar 30, 2012 8:28 am

When connecting n concentrated windings in series, the total electromotive force is not n times the voltage of a single winding, because of phase shift in the neighboring windings


This is the so called "winding factor". In a good design the phase difference won't be very big. I think Miles had about 0.95, so it won't do much to increase it to 1.
bearing
1 kW
1 kW
 
Posts: 449
Joined: Wed Dec 24, 2008 2:14 am

Re: Dual rotor axial flux motor design

Postby Miles » Fri Mar 30, 2012 8:30 am

Have you seen this one, Ken?
Attachments
90-39T.pdf
(742.98 KiB) Downloaded 50 times
User avatar
Miles
100 GW
100 GW
 
Posts: 9257
Joined: Fri Mar 16, 2007 4:15 pm
Location: London UK

Re: Dual rotor axial flux motor design

Postby Miles » Fri Mar 30, 2012 8:32 am

bearing wrote:
When connecting n concentrated windings in series, the total electromotive force is not n times the voltage of a single winding, because of phase shift in the neighboring windings


This is the so called "winding factor". In a good design the phase difference won't be very big. I think Miles had about 0.95, so it won't do much to increase it to 1.

As they say:
Although a multiphase system for concentrated pole windings
is proposed in [5], a regular three-phase system is used in
this paper. In order to obtain a high winding factor, the number
of teeth is set to 15 resulting in a winding factor of 0.951 for the
16-pole machine
User avatar
Miles
100 GW
100 GW
 
Posts: 9257
Joined: Fri Mar 16, 2007 4:15 pm
Location: London UK

Re: Dual rotor axial flux motor design

Postby kenkad » Fri Mar 30, 2012 8:39 am

Miles,
Yes, I had this copy. This is a paper that the PhD students Professor cited to me as a probable issue of the harmonics. Of course, that is something to find out. I am not a motor designer as you and I have discussed before. There are a lot of tradeoffs in any design problem. I was trying to find a way create a motor design that would allow shutting down of some of the three-phase groups when a vehicle is crusing. At that point, cogging effects as less of an issue, etc. Sort of like running an 8-cyl engine on 4 cylinders to save fuel. It really makes a difference in finding a full bridge driver for each three-phase group! As usual, it will all come out in the end one way or another. If the simulation is of any consequence, then we go on to a prototype, if I live long enough or if we live through Dec 21, 2012 (ha ha).
kenkad
kenkad
10 W
10 W
 
Posts: 73
Joined: Mon Oct 12, 2009 9:36 pm
Location: Union Grove, AL, USA

Re: Dual rotor axial flux motor design

Postby Miles » Fri Mar 30, 2012 8:43 am

kenkad wrote:I was trying to find a way create a motor design that would allow shutting down of some of the three-phase groups when a vehicle is crusing. At that point, cogging effects as less of an issue, etc. Sort of like running an 8-cyl engine on 4 cylinders to save fuel.
I still can't see the logic of that one. I don't think it's an appropriate analogy. Switching off phase groups will lower the efficiency.
User avatar
Miles
100 GW
100 GW
 
Posts: 9257
Joined: Fri Mar 16, 2007 4:15 pm
Location: London UK

Re: Dual rotor axial flux motor design

Postby Arlo1 » Fri Mar 30, 2012 9:02 am

Miles wrote:
kenkad wrote:I was trying to find a way create a motor design that would allow shutting down of some of the three-phase groups when a vehicle is crusing. At that point, cogging effects as less of an issue, etc. Sort of like running an 8-cyl engine on 4 cylinders to save fuel.
I still can't see the logic of that one. I don't think it's an appropriate analogy. Switching off phase groups will lower the efficiency.

Yeah electric motors don't work that way. Instead the controller only puts the required power to move the motor for the load and speed required. The controller uses PWM to control this so in essence at cruise it is turning all the phases on and off really fast to save energy.
And ICE with cylinder deactivation on the other hand will not just stop putting fuel into the deactivated cylinders it will also close the valves so the pressure inside those cylinders will neutralize and become an air spring for the piston to bounce off of on the end of each stroke. So if you wanted to simulate this with an electric motor (which will not likely gain you anything at all) you would have to find a way to remove the eddy current losses and Hysteresis losses from the non powered coils.
Thanks Justin of http://www.ebikes.ca/
Also a thanks to Methy at http://www.methtek.com/ :)
And Dave who has some good deals on STUF
RC lipo and most other types of Lithium batteries you MUST know your individual cell voltages while charging and discharging.
Batteries of all kinds need respect they can burn your house down, so don't sleep with them under your bed or any other were you cant afford smoke or fire!
[color=#FF0000][b][size=150]Never above 4.2v never below 2.7v EVER!!!
User avatar
Arlo1
100 GW
100 GW
 
Posts: 5227
Joined: Sun Apr 26, 2009 10:36 pm
Location: Nanaimo BC Canada

Re: Dual rotor axial flux motor design

Postby bearing » Fri Mar 30, 2012 9:15 am

Yes, a better approach to decrease idle losses could be to make the rotor discs able to move further apart at light loads, which weakens the field and decreases iron losses. But it will only help at very light loads, since that would decrease the torque constant, hence increase resistive losses.

Maybe it's more beneficial in a performance/cost relationship to buy better steel, than to make the rotor discs moveable.
bearing
1 kW
1 kW
 
Posts: 449
Joined: Wed Dec 24, 2008 2:14 am

Re: Dual rotor axial flux motor design

Postby Miles » Sat Mar 31, 2012 10:50 am

Regarding access to the center of the motor for the three phase wires.....
The copper winding strip is 14mm x 1mm so that's 14 sq. mm in cross sectional area. Equivalent to a 4.2mm diameter round wire...... Compromising a bit on the total cross sectional area, I could use 2.6mm dia. wire in a loop, sharing the current. There's just room for this to pass between the core heads and the coils, at each end.

But.........How seriously will this proximity to the coil/core unbalance the electromagnetics?

Should I feed in from the other side of the core modules to maintain the coil winding direction?
This will reinforce the armature field on 2 of the 6 modules, for each phase?

Should I reconsider the original idea of linking the coils on the outside of the motor?
Attachments
Terminal-wire-routing.jpg
Terminal-wire-routing.jpg (171.75 KiB) Viewed 359 times
User avatar
Miles
100 GW
100 GW
 
Posts: 9257
Joined: Fri Mar 16, 2007 4:15 pm
Location: London UK

Re: Dual rotor axial flux motor design

Postby fechter » Sat Mar 31, 2012 12:51 pm

If the wire passes through the slot, it will be 1/2 turn, negating 1/2 turn of the strip. Running it the other way will add 1/2 turn, which would probably be better but you have to be sure it won't fight the BEMF from the other windings. Making the connection on the outside to maintain an even turns count would be the best bet.
"One test is worth a thousand opinions"
User avatar
fechter
100 GW
100 GW
 
Posts: 9357
Joined: Sun Dec 31, 2006 3:23 pm
Location: California Bay Area, USA

PreviousNext

Return to Motor Technology

Who is online

Users browsing this forum: snath, Velcro01 and 2 guests