14ga to 12ga Spoke Upgrade

Get all your technical information about electric bikes here.

14ga to 12ga Spoke Upgrade

Postby DrkAngel » Thu Mar 15, 2012 1:34 pm

My experience has been with the EZip type non-hubmotor wheels. (EZip Wheel Re-builds)

Most all my recommendations are somewhat applicable to all wheels.

Redrilling Spoke Holes

#1 Size of hub holes 1/8".

#2 Size of wheel holes 3/16".

Spoke "Lacing"

#1 Plan on a pattern that puts the torque on the outside spokes.

#2 Take into consideration torque on front wheel with disc brake(directionally opposed to motored front wheel.)

#3 Ignore disc brake on rear motored wheel
Motor on rear wheel should take precedence over disc brake considerations, rear wheel (dual braking) supplies only 20% braking power of front wheel

#4 "Rim" brakes should be ignored, as a spoke factor.

#5 "Important" - Lace all spokes into hub and align ... BEFORE beginning to insert into nipples.
12ga spokes do not "flex", they will bend
I did one side then positioned by making a run with electrical tape, a wrap at each spoke cross.
Then did similar with the opposite side.
Then began threading into nipples

#6 Coarse alignment - Equally thread nipples, I threaded till the thread was covered.
Then I tightened each nipple an equal number of turns.
Repeat until nearly tight
(I used a quality variable speed cordless drill with a straight bit. )
Note: put dot of "white out" or similar , on straight bit - easier to count turns!
Only if you have proper size spokes! Typically, each side uses different lengths!

#7 Final adjustment should be done on the bike it will be used with

Bonus Section!

#1 Spokes are now stronger than wheel?

You might pull the stronger spokes right through the wheel?
So ... washers!
#10 SAE "stamped" washers have a nice concave side, that works nicely with 12ga nipples.
Aluminum alloy wheels don't particularly like steel, even zinc coated steel washers, against them, so I ran 2 wraps of duct tape between.

Image

I planned ahead ordered spokes of +2mm length ... not necessary, as it turned out, plenty of threads with shorter length!

#2 Spokes keep breaking at elbow, hub flange too thin, ... too much spoke "flex"? #4 SAE washers work nicely, and look impressive!

Image

Stainless steel washers recommended!

SAPIM STAINLESS 12G SPOKE
Product #435925
$0.35
Last edited by DrkAngel on Thu Mar 22, 2012 3:21 pm, edited 1 time in total.
A little learning is a dangerous thing;
Drink deep, or taste not the Pierian spring:
There, shallow draughts intoxicate the brain,
And drinking largely, sobers us again.

I enjoy enlightening ... and enlivening the spirit of the innovators.

New & Improved - Acronym Definitions

Index - Homemade Battery Packs

Endless Sphere Wiki
User avatar
DrkAngel
100 kW
100 kW
 
Posts: 1214
Joined: Wed Dec 15, 2010 11:14 am
Location: Upstate NY. USA

Re: 14ga to 12ga Spoke Upgrade

Postby DrkAngel » Thu Mar 22, 2012 8:50 am

Washers for strength, alignment etc.

12ga spokes:
can use #10 or #12 washers, for nipples.(check wheel width, for washer "fit")
can use #4 or #6 washers on hub.

14ga spokes:
can use #10 washers, for nipples.
can use #4 washers on hub.
Possibly smaller - not tested.

(Test your spokes against locally available washers - before quantity purchases)

Stainless washers are, typically, thinner.
If necessary, 2 washers could be used, for optimal spoke positioning?
A little learning is a dangerous thing;
Drink deep, or taste not the Pierian spring:
There, shallow draughts intoxicate the brain,
And drinking largely, sobers us again.

I enjoy enlightening ... and enlivening the spirit of the innovators.

New & Improved - Acronym Definitions

Index - Homemade Battery Packs

Endless Sphere Wiki
User avatar
DrkAngel
100 kW
100 kW
 
Posts: 1214
Joined: Wed Dec 15, 2010 11:14 am
Location: Upstate NY. USA

Re: 14ga to 12ga Spoke Upgrade

Postby jateureka » Thu Mar 22, 2012 5:28 pm

DrkAngel wrote:My experience has been with the EZip type non-hubmotor wheels. (EZip Wheel Re-builds)

Spoke "Lacing" #1 Plan on a pattern that puts the torque on the outside spokes.



Can you elaborate on how to achieve this? Should the outside spokes be leading or trailing?

Is this what you are talking about? http://www.peterverdone.com/wiki/index.php?title=Disc_wheel_Lacing

EDIT: ok I read your post here http://endless-sphere.com/forums/viewtopic.php?f=2&t=37728 Thanks
Last edited by jateureka on Thu Mar 22, 2012 6:44 pm, edited 4 times in total.
Bafang; Mac; Ezee; Easy2Ride; PowerPed; Nope; Condor; Aprilia; eLation V2; Razor
jateureka
1 kW
1 kW
 
Posts: 423
Joined: Tue Apr 06, 2010 7:18 pm
Location: Brisbane QLD Australia

Re: 14ga to 12ga Spoke Upgrade

Postby DAND214 » Thu Mar 22, 2012 6:01 pm

I did just the oppsite!

The 12g were breaking so went to the 14g Sapim with a new wheel. At least you can get tension adjustment with a 14g spoke, not like the China crap 12g.

Spokes aren't breaking anymore :?

And I don't get as much growl from the hub?

Dan
It sure would be nice to know where we are all located, ON THIS WORLD.
Fill in your profile. It doesn't hurt.
I know some worry about being found.
I wish someone would find me.
DAND214
100 kW
100 kW
 
Posts: 1263
Joined: Sun Aug 10, 2008 8:28 pm
Location: Chicagoland nw suburb Mt. Prospect IL.

Re: 14ga to 12ga Spoke Upgrade

Postby DrkAngel » Thu Mar 22, 2012 6:57 pm

jateureka wrote:
DrkAngel wrote:My experience has been with the EZip type non-hubmotor wheels. (EZip Wheel Re-builds)

Spoke "Lacing" #1 Plan on a pattern that puts the torque on the outside spokes.




Can you elaborate on how to achieve this? Should the outside spokes be leading or trailing?


OEM - Wrong

Image

Corrected - The hub should pull the wheel around

Image

Motor & pedal turn this wheel clockwise.

Image
A little learning is a dangerous thing;
Drink deep, or taste not the Pierian spring:
There, shallow draughts intoxicate the brain,
And drinking largely, sobers us again.

I enjoy enlightening ... and enlivening the spirit of the innovators.

New & Improved - Acronym Definitions

Index - Homemade Battery Packs

Endless Sphere Wiki
User avatar
DrkAngel
100 kW
100 kW
 
Posts: 1214
Joined: Wed Dec 15, 2010 11:14 am
Location: Upstate NY. USA

Re: 14ga to 12ga Spoke Upgrade

Postby jateureka » Thu Mar 22, 2012 7:33 pm

So you suggest outside spokes on both sides of the rear wheel should point forward (leading)? Interesting, I'll have to look into that further.

That is the opposite of what Shimano and Magura say with regrads to disc brake rotors and drive sides, but they also suggest braking forces are stronger than drive forces... http://www.peterverdone.com/wiki/index.php?title=Disc_wheel_Lacing

"... to keep the outside spokes on each respective side in full tension while braking and only the drive side of the rear wheel being changed..."

"...Head-inside-spokes (= arc outside spokes) have to be pulled, i.e. these spokes point forward on the front wheel; on the back wheel these spokes point forward on the rotor side and backwards on the drive side..."
Bafang; Mac; Ezee; Easy2Ride; PowerPed; Nope; Condor; Aprilia; eLation V2; Razor
jateureka
1 kW
1 kW
 
Posts: 423
Joined: Tue Apr 06, 2010 7:18 pm
Location: Brisbane QLD Australia

Re: 14ga to 12ga Spoke Upgrade

Postby DrkAngel » Fri Mar 23, 2012 1:13 am

This picture illustrates the problem I ran into.

OEM - Wrong

Image

The problem was 2-fold.
The "elbow inward" "stressed" spokes were continually breaking, at the elbow stress point.
Various eZips were laced differently but the inward elbowed side was always the side that broke!
The "inward" spokes are poorly supported leading to amplified stress on the elbow.
This problem is amplified by the use of a "too thin" hub spoke flange.

Changing the direction of the spokes appears to support the elbow closer to the bend, reducing the "leverage" at that weak point.
The addition of washers pulled the bend fairly tight, to the hub flange, reducing the "torsional stress" even further.

With a wider, or better designed, "hub spoke flange" this might not be a factor.
For example, the "present source unknown" replacement hub supported the spokes excellently.
There was some "spring" just crossing the spokes.

Image
A little learning is a dangerous thing;
Drink deep, or taste not the Pierian spring:
There, shallow draughts intoxicate the brain,
And drinking largely, sobers us again.

I enjoy enlightening ... and enlivening the spirit of the innovators.

New & Improved - Acronym Definitions

Index - Homemade Battery Packs

Endless Sphere Wiki
User avatar
DrkAngel
100 kW
100 kW
 
Posts: 1214
Joined: Wed Dec 15, 2010 11:14 am
Location: Upstate NY. USA


Return to E-Bike Technical

Who is online

Users browsing this forum: Bing [Bot], docnjoj, RichiePA and 5 guests