Powerlab 8 confusion...

Batteries, Chargers, and Battery Management Systems.

Powerlab 8 confusion...

Postby x88x » Sun Apr 22, 2012 11:19 am

So, I picked up a Powerlab 8 on Jozzer's recommendation, and I'm trying to set it up to do some stress tests on the 5kWh of Turnigy lipo I have sitting here.. :D

Running into a problem though. I tell it to discharge at 40A, it immediately goes to ~4.6A, then very, very slowly increases...it's been 8 minutes now, and it's only up to 4.98A. ...wtf?
That we enjoy great advantages from the inventions of others, we should be glad of an opportunity to serve others by any invention of ours, and this we should do freely and generously.
--Benjamin Franklin

Battery stats comparison spreadsheet.
x88x
10 kW
10 kW
 
Posts: 625
Joined: Mon Oct 11, 2010 4:10 pm
Location: MD, USA

Re: Powerlab 8 confusion...

Postby ZOMGVTEK » Sun Apr 22, 2012 11:26 am

That's designed to discharge at 100W. You can set the current to anything you want, if its over 100W, it will be limited to 100W.

It will regenerative discharge up to 1,000W. You might want to take a peek at the user manual.
ZOMGVTEK
100 kW
100 kW
 
Posts: 1197
Joined: Sat Jun 06, 2009 1:40 am

Re: Powerlab 8 confusion...

Postby x88x » Sun Apr 22, 2012 11:43 am

Ah, ok, that explains it. I'll get it set up with a battery to work off of once it drops down.

And yes, I have the users manual, just haven't gotten through all 86 pages yet. :roll:
That we enjoy great advantages from the inventions of others, we should be glad of an opportunity to serve others by any invention of ours, and this we should do freely and generously.
--Benjamin Franklin

Battery stats comparison spreadsheet.
x88x
10 kW
10 kW
 
Posts: 625
Joined: Mon Oct 11, 2010 4:10 pm
Location: MD, USA

Re: Powerlab 8 confusion...

Postby chilledoutuk » Sun Apr 22, 2012 12:58 pm

That's a great charger if they made a 10s Powerlab I would get that but my next charger has to be able to do 10s to make my charging life much easier.

Probably will go with a cellpro 10s personally.
chilledoutuk
100 W
100 W
 
Posts: 122
Joined: Sun Aug 28, 2011 6:09 pm

Re: Powerlab 8 confusion...

Postby cassschr1 » Sun Apr 22, 2012 1:16 pm

AND it will only do about 600 watts if on 12v battery. It needs two batteries for max capabilities. If you do a heavy discharge from lipos MAKE SURE 12V BAT ARE NOT AT FULL CHARGE cause it still won't do the max. check your settings in the menu. Cass
cassschr1
10 kW
10 kW
 
Posts: 507
Joined: Fri Aug 14, 2009 11:57 am
Location: LaCrosse, Wisconsin

Re: Powerlab 8 confusion...

Postby x88x » Sun Apr 22, 2012 1:22 pm

cassschr1 wrote:AND it will only do about 600 watts if on 12v battery. It needs two batteries for max capabilities. If you do a heavy discharge from lipos MAKE SURE 12V BAT ARE NOT AT FULL CHARGE cause it still won't do the max. check your settings in the menu. Cass

Thanks for the tip. Am actually running it off a 6S3P pack of 5Ah Zippy's, so had to tweak the setting a bit for the input pack. ;)
That we enjoy great advantages from the inventions of others, we should be glad of an opportunity to serve others by any invention of ours, and this we should do freely and generously.
--Benjamin Franklin

Battery stats comparison spreadsheet.
x88x
10 kW
10 kW
 
Posts: 625
Joined: Mon Oct 11, 2010 4:10 pm
Location: MD, USA


Return to Battery Technology

Who is online

Users browsing this forum: etriker and 4 guests