by thegavo » Mon Apr 30, 2012 6:38 pm
Ok here's what I did, as I've only been getting two to 3 mile on the 20 ah , I've removed the ribbon wire that had the low cell From the bms, leaving the other ribbon in place, (balance wires) I took the bike out tonight after checking all cell volts , still 3.8v bar the one at 3.2v, I figured the bms would not shut off the power if the balance wire was disconnected, I rode the bike with wot most of the time and no pedalling at all, even from standing starts and had it up to top speed for at least one mile on way back (34mph) for aprox 10 miles , I then tested voltage and all cells were down from 3.8 to 3.3 the duff one read 3.0 from 3.2, I plugged the ribbon back into bms and charged up, it took 50 mins 5a charger , and the cells were all 3.8 and the duffer was upto 3.3, dunno what this tells me really but it was great to be out on it for a longer blast, will it damage anything doing that? Will the bms cut the power based on balance wire that gets left in or do I have to be careful ??