Is my battery toast?

Batteries, Chargers, and Battery Management Systems.

Is my battery toast?

Postby wildblueyonder » Mon May 28, 2012 4:26 am

Ok, my first e-bike project (yeah!), I've got a 48v rear hub motor and I ordered, and received, a 48v 30ah vpower battery from China. Upon receiving the battery the voltage read 55.3, good to go right?

So I order some Anderson powerpoles and solder the ends so I've got a nifty, efficient connection, rig the whole thing up for a test run and BAM! off and running like a shot! Sooo exciting, that sucker flies, awesome, right?

So the thing is really just jury rigged on there just to see if its gonna go, so I take it apart to charge the battery and fashion a more sturdy and permanent arrangement... And now the thing won't work. Not even a jerk. Lights to the throttle, yes, but zero movement.

Looks like its the battery, after plenty of charge time it only registers 45.9v. I assume this is just not enough to move a 48v motor, correct?

So any thoughts. The battery is a duct taped job, my feeling is that I'll have to go ahead and take it apart and diagnose and replace the offending cells. Could this be a BMS issue? If so, where to start a diagnoses. Any help would be great, thanks!

Man, though I only rode it a few times around the block it was sweeeet!!
wildblueyonder
100 µW
100 µW
 
Posts: 9
Joined: Tue Nov 08, 2011 11:10 am

Re: Is my battery toast?

Postby Tench » Mon May 28, 2012 4:32 am

Check the polarity on your charger output first, do you have another charger you could connect to see if the pack voltage rises with a different charger? Was the chargers input voltage correct for your mains supply?

Where you trying to charge it through the output leads?
Project Two viewtopic.php?f=6&t=37489
Project one viewtopic.php?f=28&t=20304&hilit=tench

The uk's first Stealth Bomber
Tench
1 kW
1 kW
 
Posts: 423
Joined: Tue Jul 13, 2010 12:48 pm
Location: UK

Re: Is my battery toast?

Postby dnmun » Mon May 28, 2012 4:48 am

do you have a voltmeter? can you measure the voltages of the cells while the battery is charging? at the sense wire plug if the pack is still wrapped up in tape.
dnmun
100 GW
100 GW
 
Posts: 9066
Joined: Mon Jun 09, 2008 1:32 pm
Location: portland, or and loveland, co

Re: Is my battery toast?

Postby liveforphysics » Mon May 28, 2012 5:01 am

The BMS has tripped off for some reason.

You should try to get some charge in the pack ASAP, after checking balance on the cells to confirm you don't have one at 0v or something.
For ebike parts, don't be a douche, buy from http://www.ebikes.ca or http://www.MethTek.com

Justin saved the forum at great personal expense! The man is a legend and a hero!
User avatar
liveforphysics
100 GW
100 GW
 
Posts: 10960
Joined: Wed Oct 29, 2008 1:48 am
Location: Santa Cruz, CA, USA

Re: Is my battery toast?

Postby dogman » Mon May 28, 2012 6:46 am

How is the charger acting? Does the red charging led ever turn on? Don't peel it just yet, just get acess to the wiring from the pack to the bms.

You could have a few different things happening, bad bms, or bad charger. Kind of unlikely that the battery died that fast, but still possible.

Get a voltmeter, and check stuff, charger works, to start with. Polarities are correct. If the charger works, attach it to the + and - leads of the battery before the bms, and try to get some voltage into it if the battery is that low.

Most likely, is your bms just smoked, and you can fairly easily replace it.
THE LIPO RULES. NEVER ABOVE 4.3V NEVER BELOW 2.7V DON'T PUNCTURE

Ideal charging /discharging range for Lipo, 3.65v minimum 4.1v maximum

See battery technology section, FAQ thread at the top of the page for lipo noob info.
User avatar
dogman
100 GW
100 GW
 
Posts: 21938
Joined: Sat May 17, 2008 12:53 pm
Location: Las Cruces New Mexico USA

Re: Is my battery toast?

Postby Jason27 » Tue May 29, 2012 12:26 am

Dude, seriously people need to stop buying crap batteries from china. More and more people are having bms issues which is probably the problem your having. have you tried to contact vpower??

Just because you think you're getting a great price does not mean you're getting a great product. Lessons learned.
My ebike:
Diamondback with 800 watt hub motor with AllCell 48V 12AH Lithium Manganese battery pack.
36v hobby king lipo as backup.

"Conquering the hills of SF"
User avatar
Jason27
10 kW
10 kW
 
Posts: 518
Joined: Sun Apr 17, 2011 8:10 pm
Location: San Francisco, CA

Re: Is my battery toast?

Postby 999zip999 » Tue May 29, 2012 2:24 am

Voltage on main output.
voltage before bms
voltage from charger
voltage on 16 cells, can you get to sense wires to check. Should be between 2.5 to 3.6v and not over 3.9v per cell, but all should be in same range like 3.2-3.3v. ect
999zip999
100 MW
100 MW
 
Posts: 2944
Joined: Sun Jan 10, 2010 1:40 pm
Location: Dana Point So. Cal

Re: Is my battery toast?

Postby wildblueyonder » Thu Jun 07, 2012 10:12 am

Well, its occam's razor - used a new charger and while not back to my base voltage I'm at 53.5 - that should be sufficient, no? Thanks to you all for your suggestions. Going forward, is there any way to 'test' a battery charger? Any advice at all when it comes to chargers, or charging batteries?

So still not back up and running, I think I've got a controller issue now. The lights on my throttle light up but I just get a 'click' noise inside my controller when I try and engage the throttle, I will start another thread once I open it up and see what's up. Boy they sure don't make it simple to do that, looks like about 20 screws just to open a little 8x4 box.....
wildblueyonder