Postby neoplasticity » Tue Jul 31, 2012 11:31 am

Free batteries

I have four Turnigy 5000mAH 6s batteries. I babied them and they were treated very well BUT i went on vacation and forgot to disconnected them from my bike and over two weeks they slowly overdischarged. I tried to charge them back up but it looks like 1 or two cells on each battery are done for. The remaining 4-5 cells seem ok? I dunno. I dont have the knowledge or the inclination to take them apart to make good batteries out of the remaining cells but if someone wants them, they can have them. I prefer someone local so they can just pick them up. Im in redlands, ca. if not, can someone tell me how to dispose of them properly or any other uses you can think of for them?
neoplasticity
1 W
1 W
 
Posts: 63
Joined: Thu Aug 27, 2009 9:08 am
Location: Redlands, CA

Re: free lipos

Postby Ykick » Tue Jul 31, 2012 11:44 am

neoplasticity wrote:Free batteries

I have four Turnigy 5000mAH 6s batteries. I babied them and they were treated very well BUT i went on vacation and forgot to disconnected them from my bike and over two weeks they slowly overdischarged. I tried to charge them back up but it looks like 1 or two cells on each battery are done for. The remaining 4-5 cells seem ok? I dunno. I dont have the knowledge or the inclination to take them apart to make good batteries out of the remaining cells but if someone wants them, they can have them. I prefer someone local so they can just pick them up. Im in redlands, ca. if not, can someone tell me how to dispose of them properly or any other uses you can think of for them?


PM sent
User avatar
Ykick
10 MW
10 MW
 
Posts: 2457
Joined: Thu Nov 26, 2009 6:10 pm
Location: North America

Re: free lipos

Postby cal3thousand » Tue Jul 31, 2012 12:56 pm

Got there in 13 minutes... Nice one Ykick
#1: Diamondback Menona 700c (Commuter)
M/C: e-BikeKit geared rear w/BB7 with 12FET 40A Infineon ebikes.ca
GM 48V LiFePO4 10Ah racked; moving to 12S Turnigy 10Ah framed
+ Speedict, XC30TK disc, Alex Adventurer 700c Disc, Tektro 180mm hyd. with 42mm Kenda Urban


#2: Norco VPS Six DH (Fun) WIP
M/C: Clyte HT3525 (Thanks Meth!!!) http://Methtek.com with Lyen 18FET 24S Regen
Battery: 24S Turnigy 10Ah frame (ABS)

#3: Wifey Bike, Giant eSuede fully customized WIP
cal3thousand
100 kW
100 kW
 
Posts: 1259
Joined: Mon Mar 26, 2012 4:47 pm
Location: California

Re: free lipos

Postby pdf » Tue Jul 31, 2012 4:21 pm

Good to see someone is interested. Just wanted to chime in to say I did the EXACT same thing with the EXACT same battery (Turnigy 5000mAh, 6s), but with three instead of four of them. It turned out that the same cell in each battery was bad (zero volts) and the others were, as far as I could tell, fine. It was the second cell from one end (don't remember which end). I'd be curious to know if it is the same cell in these (don't know why it would be though).
-------------
Jamis Commuter 1.0/Xtracycle Stokemonkey 36V LiFePO4, 15 ahr
Giant Boulder 9C 6x10, 18s1p LiPO, 5 ahr, 18FET Lyen edition
User avatar
pdf
1 kW
1 kW
 
Posts: 499
Joined: Thu Aug 20, 2009 11:31 am
Location: Knoxville, Tennessee, USA

Re: free lipos

Postby etriker » Wed Aug 01, 2012 3:30 am

pdf wrote:Good to see someone is interested. Just wanted to chime in to say I did the EXACT same thing with the EXACT same battery (Turnigy 5000mAh, 6s), but with three instead of four of them. It turned out that the same cell in each battery was bad (zero volts) and the others were, as far as I could tell, fine. It was the second cell from one end (don't remember which end). I'd be curious to know if it is the same cell in these (don't know why it would be though).


I would also like to know. Did the cells that went to zero have different markings on them ?

I took some failed nanotech 10 cell 5000mah batteries apart and the cells were all marked nano 5000 on them except the cells that failed.

What's up with that ? Did they put made to fail early cells in those packs ?

Most everyone blames the user or charger when they fail so I can see how they could get away with it.
I Think We're All Bozos On This Bus

http://www.youtube.com/watch?v=lmWFrMq3qNY
etriker
10 kW
10 kW
 
Posts: 863
Joined: Sun May 27, 2012 8:21 am
Location: Florida USA

Re: free lipos

Postby dogman » Wed Aug 01, 2012 5:19 am

Hmm, well if the user left em plugged into the controller and overdischarges em, I blame the user for sure.

But the well known 10% rate of packs that arrive dead or puffed, or get that way in less that 25 cycles I have always blamed on RC lipo factory quality controll.

But putting a few lower quality cells in a big buck nano pack, that's really crossing the line. Not that I find it suprising though, wanna buy a really cheap rolex? Solid gold, I swear it!
THE LIPO RULES. NEVER ABOVE 4.3V NEVER BELOW 2.7V DON'T PUNCTURE

Ideal charging /discharging range for Lipo, 3.65v minimum 4.1v maximum

See battery technology section, FAQ thread at the top of the page for lipo noob info.
User avatar
dogman
100 GW
100 GW
 
Posts: 22281
Joined: Sat May 17, 2008 12:53 pm
Location: Las Cruces New Mexico USA

Re: free lipos

Postby Ykick » Wed Aug 08, 2012 10:34 am

Thanks to neoplasticity for gifting me these bricks. Picked em up yesterday while running errands and spent a little time qualifying what's what. Unable to post pics right now but here's a quick rundown of their condition.

1 brick seems to be okay. Slight puff but all cells 3.8V resting and accepting seemingly normal charge.

Next brick appears okay except cell #6 which is completely 0V. Unable to bring that cell up. Surgical candidate.

3rd brick only 2 cells appear to be okay. 4 of 6 cells 0V. Will scavenge 2 working cells.

4th brick very puffed and completely 0V. So far my limited attempts include venting pouches and resealing. Unfortunately, they do not appear to accept small charge.

With a little surgical work will likely wind up with 2 working 6S Turnigy bricks. Of course, these will always be suspect, used and stored appropriately but still useful for recreational purposes.

Thanks again to neoplasticity!
User avatar
Ykick
10 MW
10 MW
 
Posts: 2457
Joined: Thu Nov 26, 2009 6:10 pm
Location: North America


Return to Battery Technology

Who is online

Users browsing this forum: No registered users and 8 guests