LG HG6 20650 cell

Batteries, Chargers, and Battery Management Systems.
Post Reply
User avatar
Overclocker
1 kW
1 kW
Posts: 453
Joined: Mar 17, 2014 5:48 am
Location: Philippines

LG HG6 20650 cell

Post by Overclocker » Nov 28, 2016 10:46 am

Image

Hillhater
100 GW
100 GW
Posts: 8514
Joined: Aug 03, 2010 10:33 pm
Location: Sydney ..(Hilly part !) .. Australia/ Down under !

Re: LG HG6 20650 cell

Post by Hillhater » Nov 28, 2016 4:22 pm

Yes, its another high drain 3.0Ahr cell....but 10% heavier and 10% bigger that the others. ! :roll:
This forum owes its existence to Justin of ebikes.ca

User avatar
liveforphysics
100 GW
100 GW
Posts: 14520
Joined: Oct 29, 2008 1:48 am
Location: Santa Cruz, CA, USA

Re: LG HG6 20650 cell

Post by liveforphysics » Nov 28, 2016 6:12 pm

I saw that sheet and was thinking, that's a pretty nice option for my sportier RC multirotor/heli builds. Then I noticed it's a 20650 not 18650...

That cell is either super cheap to make $/Wh, or it better cycle >2,000x, because it's specs and even power density isn't very impressive compared to 1+year old existing LG 18650s.
Each carcinogen vapor exposure includes a dice roll for cancer.

Each mutagen vapor exposure includes a dice roll for reproductive genetic defects in your children.

Each engine start sprays them into a shared atmosphere which includes beings not offered an opportunity to consent accepting these cancer experiences and defective genetics life experiences.

Every post is a free gift to the collective of minds composing the living bleeding edge of LEV development on our spaceship.

Pajda
100 W
100 W
Posts: 133
Joined: Jan 24, 2016 3:45 am
Location: Czech Republic

Re: LG HG6 20650 cell

Post by Pajda » Nov 29, 2016 3:31 pm

Nice finding Overclocker...

Btw. anybody seen any evidence about new 20650,20700,21700,21-70 format cells in "High Density" design with parameters better than (still a waporware) Samsung INR21700-47P? It's been some time when appeared first report on these new formats.

Hillhater
100 GW
100 GW
Posts: 8514
Joined: Aug 03, 2010 10:33 pm
Location: Sydney ..(Hilly part !) .. Australia/ Down under !

Re: LG HG6 20650 cell

Post by Hillhater » Nov 30, 2016 12:25 am

Pajda wrote: Btw. anybody seen any evidence about new 20650,20700,21700,21-70 format cells in "High Density" design with parameters better than (still a waporware) Samsung INR21700-47P? It's been some time when appeared first report on these new formats.
Well there is supposedly the Sony/BMZ 21700 "3Tron" cell, that has some pretty impressive claims..
such as..
50% more energy
60% more capacity ?
68% increase in output ?
4 times more discharge current ?
http://www.bike-eu.com/home/nieuws/2016 ... e-10127504
This forum owes its existence to Justin of ebikes.ca

User avatar
Overclocker
1 kW
1 kW
Posts: 453
Joined: Mar 17, 2014 5:48 am
Location: Philippines

Re: LG HG6 20650 cell

Post by Overclocker » Nov 30, 2016 11:07 am

cutoff voltage of 2.0v.

strange... have to find the official datasheet

Pajda
100 W
100 W
Posts: 133
Joined: Jan 24, 2016 3:45 am
Location: Czech Republic

Re: LG HG6 20650 cell

Post by Pajda » Nov 30, 2016 1:44 pm

Hillhater wrote:
Pajda wrote: Btw. anybody seen any evidence about new 20650,20700,21700,21-70 format cells in "High Density" design with parameters better than (still a waporware) Samsung INR21700-47P? It's been some time when appeared first report on these new formats.
Well there is supposedly the Sony/BMZ 21700 "3Tron" cell, that has some pretty impressive claims..
such as..
50% more energy
60% more capacity ?
68% increase in output ?
4 times more discharge current ?
http://www.bike-eu.com/home/nieuws/2016 ... e-10127504
Hmm.. interesting but no real data about BMZ batteries to compare. However, I managed to find out that the cells are most probably sourced from SONY. It could be a Sony US21700Vxx cell with 5Ah anounced capacity. But as usual there is no evidence that this cells are already in Mass Production. Anyway 5Ah in 21700 is a real progress because it is finally comparable in energy density with ~3,5Ah in 18650.

I also highly recomend to study this document if you haven't found it yet. :)

http://www.emove360.com/wp-content/uplo ... rences.pdf

Pajda
100 W
100 W
Posts: 133
Joined: Jan 24, 2016 3:45 am
Location: Czech Republic

Re: LG HG6 20650 cell

Post by Pajda » Nov 30, 2016 1:48 pm

Overclocker wrote:cutoff voltage of 2.0v.

strange... have to find the official datasheet
Indeed, but new Sony US18650VC7 have the same 2.0V cut-off voltage too. :roll:

User avatar
Overclocker
1 kW
1 kW
Posts: 453
Joined: Mar 17, 2014 5:48 am
Location: Philippines

Re: LG HG6 20650 cell

Post by Overclocker » Nov 30, 2016 10:00 pm

Pajda wrote:
Overclocker wrote:cutoff voltage of 2.0v.

strange... have to find the official datasheet
Indeed, but new Sony US18650VC7 have the same 2.0V cut-off voltage too. :roll:

sounds like a "new" chemistry, or a heavily tweaked one

NCA are 2.5v

Hillhater
100 GW
100 GW
Posts: 8514
Joined: Aug 03, 2010 10:33 pm
Location: Sydney ..(Hilly part !) .. Australia/ Down under !

Re: LG HG6 20650 cell

Post by Hillhater » Nov 30, 2016 11:11 pm

Overclocker wrote:
Pajda wrote:
Overclocker wrote:cutoff voltage of 2.0v.
strange... have to find the official datasheet
Indeed, but new Sony US18650VC7 have the same 2.0V cut-off voltage too. :roll:
sounds like a "new" chemistry, or a heavily tweaked one
NCA are 2.5v
Possibly, but from those discharge curves it doesnt seem to bring much to the party.
All these cells are "over the cliff" on voltage once down to 3.0v with very little extra capacity between 3 and 2.0 v.
But At least the Sony VC7 seems to sag less at higher discharges.
This forum owes its existence to Justin of ebikes.ca

Pajda
100 W
100 W
Posts: 133
Joined: Jan 24, 2016 3:45 am
Location: Czech Republic

Re: LG HG6 20650 cell

Post by Pajda » Dec 01, 2016 3:31 am

Here is a first datasheet/technical information list from Sony about VC7. It confirms 2,0V cut-off (but for nominal 0.2C discharge only, otherwise they use standard 2.5V). Also there is a correction for 10A discharge temperature rise of VC7 seen in the Shmuel presentation on page 10. The end temperature is reaching 70°C, which is pretty the same as for MJ and GA. (They probably accidentally used the data for 5A).

https://e2e.ti.com/cfs-file/__key/commu ... R0.1.2.pdf

.. So I think that the information about Sony VC7 would deserve a separate thread.

User avatar
Overclocker
1 kW
1 kW
Posts: 453
Joined: Mar 17, 2014 5:48 am
Location: Philippines

Re: LG HG6 20650 cell

Post by Overclocker » Dec 01, 2016 10:14 pm

Pajda wrote:Here is a first datasheet/technical information list from Sony about VC7. It confirms 2,0V cut-off (but for nominal 0.2C discharge only, otherwise they use standard 2.5V). Also there is a correction for 10A discharge temperature rise of VC7 seen in the Shmuel presentation on page 10. The end temperature is reaching 70°C, which is pretty the same as for MJ and GA. (They probably accidentally used the data for 5A).

https://e2e.ti.com/cfs-file/__key/commu ... R0.1.2.pdf

.. So I think that the information about Sony VC7 would deserve a separate thread.

their cycle life tests use 2.5v

i think in their desire to advertise 3500mah they overdischarged the cell to 2.0v in that one test

not very honest :roll:

User avatar
The Battery Doctor
1 mW
1 mW
Posts: 17
Joined: Aug 05, 2017 7:43 pm
Location: Stockholm
Contact:

Re: LG HG6 20650 cell

Post by The Battery Doctor » Nov 25, 2017 11:16 am

Today i noticed the Sony Konion US18650VC7 was actually released! I order 40 pcs but they are expensive so for testing only. But at low current they can have 3600mah or more!
I operate a battery repair shop in Stockholm, Sweden called batteridoktorn (The Battery Doctor).

Se my videos on youtube: https://www.youtube.com/channel/UCxgrRl ... JI2MKqnmWw