    First problem after 1800 miles! - Is my BMS Board Dying..?

    Hey all, I have a 48v / 11.6ah Hailong battery running a 1000w rear hub motor on a Cannondale conversion. On my last couple of excursions my power cut off as soon as the battery dropped to around 48v (sits on 54.4v after a full charge). This happened on 2 occasions. This morning I powered the...