In July 2012 I received an order of 9 packs of 6s, 5 amp hour, 20C Turnigy's, plus some cables and connectors at a cost of $580 shipped.
The packs were mostly run at 24s 2p, 88.8v 10 amp hours. Current has been between 40 and 90 amps. However past few months I've been running 24s 1p, again...