Hi,
I'm mid into rebuilding two Segway batteries. I've got one taken apart to see what cells are needed. The OEM cells are Valence Saphion 3.2V 1400 mAh IFR-18650EC. I'm going to need just under 200 cells for the rebuild. I called and talked to valence, but they won't sell the cells to...