    Help me decide: Motor/Charge Controller for 55-MPH Go Kart (PICS)

    My son and I went with this package. http://www.evdrives.com/product_p/ck-0708.htm We used a 14S Nissan Leaf pack (7 modules in series) with no BMS. With my son's weight and the proper sprocket selection you can hit 55mph easily. Since we are not running a BMS we are instead monitoring the...
  2. E

    E-Kart Build

    Thanks for the clarification on the motor voltage and RPM. Everything is more complex that it seems, appreciate the simple explanation. The Alltrax SR48300 has a max voltage of 62v, so I will definitely rethink the battery situation. Good catch on the Satiator only a 360watt. I was...
  3. E

    E-Kart Build

    I have been spending a great deal of time reading and trying learn and tailor for my build. I believe that the direction i am going is a good one, but before I spend any more time and money some opinions are a good thing Hardware currently in hand: Motoenergy ME-0708 48V, 100 amps continuous...