Hey everyone. This is my first post on here. So please bear with me as I’m new here. But I rebuild lithium ion battery packs for all bikes and electric vehicles, mountain boards scooters solar powerwalls. Any voltage 24v 36v 48v 52v 58v 60v 72v 90v. Any capacity any size. I spot weld all my...