found the solution, the problem was in the bluetooth serial app, it considered the command "10"(53.5V) as "1"(43V). the solution simplifies the commands to just 9 commands. now the psu can be set up to 58V. thanks all.
I'm making a project using serial Bluetooth and managed to set the DC output on, limit current, voltage 41v - 48v, except that setting the voltage above 48v didn't work. for example, if the psu voltage is 41v then I set it to 48v it immediately changes. but from 48v to 53v it gets 43v instead. I...
found another problem with the psu, the voltage could not be set above 48v, when I tried to set it to 49v - 58v the psu instead changed to 43.5v. i tried it on r48-2000e3 and r48-1000, online and offline commands. both same respond
Yes i have set both to 1.20% current limit with offline command (default), along with setting output on, walking time, default voltage. and everything seems to work.
I use this command for set current
03 F0 00 19 3F 99 99 9a (1.20%)
Thank you friend. if the problem is in the r48-1000 then I will try setup 2x r48-2000e3 and hope that the current can be close to 1C.
I found chart for r48-1000
today i tried charging at an ac charging station with a new setup, vertiv r48-2000e3 and emerson r48-1000 in series. the battery only draws 7.5a, the same as the previous 2x r48-1000 setup. finally I paralleled it with a 24s lifepo4 charger 10A to get close to 1C. I'm still confused, is the...
After many experiments you have done with emerson, eltek, huawei, etc, which PSU do you recommend for use as a charger, looking at its power, durability, communication, and when they are connected in series or parallel?
Hai friend.. I want to ask you, I have the same problem when connecting in series, 1 psu 43v, 1 other psu drops to 33v. The current is only 7.5a from a maximum of 20a. is this normal?
What if I add 1 psu 48v 40a set to 43.8v, then I series it with the 2 previous psu that I paralleled at 43.8v...
I think this is the old version. I bought it in used condition. The goal is to get a 20A charger. Compared to buying a new LifePo4 charger 20A, the price is much cheaper. Im so happy now :D
thank you friends. I succeeded in changing the voltage of the Emerson R48-1000 to 43.8 v, I connected it in series to charge the lifepo4 24s 87.6v. I use mcp2515 and esp32.
Thank You