Unused cells harvested out of battery packs that got put on the shelf after being manufactured.
I've tested about 1/3 of the cells and they all test above or at 6000mAh

13A continuous discharge
23A max discharge 10s
10A continuous charge
5300mAh rated
3000 cycle life to 80% DOD

$500NZD plus shipping within New Zealand, or pickup is OK. Located Christchurch.

3kWh of lithium cells here for not much money!
 