Search found 506 matches

by cassschr1
Oct 18 2017 12:45am
Forum: E-Bike General Discussion
Topic: Electric heated clothing
Replies: 13
Views: 1491

Re: Electric heated clothing

Check out Gerbing 12v heated motorcycle clothing. Stuff works great, very warm.
by cassschr1
May 31 2017 7:34pm
Forum: Items for Sale - Used
Topic: A123 pack - 16ah 40v with BMS - 100$ - SOLD
Replies: 5
Views: 976

Re: A123 pack - 16ah 40v with BMS - 100$ -

has the bms been connected the whole time?
How bout testing the 8p cells and post voltages.
by cassschr1
May 26 2017 4:55pm
Forum: Battery Technology
Topic: HUGE EMPTY Downtube/Craddle Battery Box with Keylock
Replies: 28
Views: 5257

Re: HUGE EMPTY Downtube/Craddle Battery Box with Keylock

that ashland was for tidal force bikes when they went under.
by cassschr1
May 26 2017 7:42am
Forum: Items for Sale - Used
Topic: 9C hub motors E-Bike Kit clones 6X10 winding - SOLD
Replies: 3
Views: 654

Re: 9C hub motors E-Bike Kit clones 6X10 winding

I'm gonna buy both of these. PM sent also.
by cassschr1
May 21 2017 10:10am
Forum: Items for Sale - Used
Topic: MXUS 3000 4T with FF and Hubsinks 19" Tire
Replies: 7
Views: 1395

Re: MXUS 3000 4T with FF and Hubsinks 19" Tire

your 2nd picture might as well not even be there.
Put about 10 pics up and you might get some interest . Both sides.
If there's a winding wire broke, show it.
by cassschr1
Apr 27 2017 7:45pm
Forum: Items Wanted
Topic: 5300 series sator
Replies: 5
Views: 593

Re: 5300 series sator

i was gonna suggest Tench, but he hasn't posted in a couple years.
by cassschr1
Apr 03 2017 11:07pm
Forum: Battery Technology
Topic: cell checker draw
Replies: 5
Views: 662

Re: cell checker draw

now i find out after its done the damage.
by cassschr1
Apr 03 2017 9:44pm
Forum: Battery Technology
Topic: Battery charging is less than capacity of battery?
Replies: 11
Views: 1192

Re: Battery charging is less than capacity of battery?

Leave the charger on it.
ride a couple km.
charge again, ride a bit, not alot.
charge again. Leave charger on it 24/48 hrs, aint gonna hurt it. I was surprised how many ah my pack picked up.
by cassschr1
Feb 18 2017 4:18pm
Forum: Items Wanted
Topic: 5300 series sator
Replies: 5
Views: 593

5300 series sator

Anybody got an old fried 5300 motor? I want to rewind one. I know these are getting to be old. Would like to make a 5306. location lacrosse, wi.54603
by cassschr1
Jan 05 2017 3:37am
Forum: General Discussion
Topic: ion ice auger battery
Replies: 2
Views: 483

Re: ion ice auger battery

bump
by cassschr1
Jan 04 2017 4:45pm
Forum: General Discussion
Topic: ion ice auger battery
Replies: 2
Views: 483

ion ice auger battery

My son just bought one of these. Anybody know what cells are in it? Maybe I'll just borrow it when he's not looking! LOL
by cassschr1
Jan 04 2017 4:09pm
Forum: Items for Sale - Used
Topic: 8s >10ah LTO lithium packs sold out
Replies: 46
Views: 6146

Re: 8s >10ah LTO lithium packs

I went and visited this guy last night,turns out I met him 40 years ago. Nice guy he is. He gave me a messed up pack of 8s to measure (broken tab on outer cell, and balance leads were cut off.These packs also have temp sensors and possibly other monitoring capability. The plugs are extreme quality. ...
by cassschr1
Mar 05 2016 10:58pm
Forum: Items for Sale - New
Topic: US Group buy for the new MXUS 3000w V3
Replies: 384
Views: 38730

Re: US Group buy for the new MXUS 3000w V3

Can someone explain bent magnets.
by cassschr1
Oct 26 2015 9:28pm
Forum: Items for Sale - New
Topic: Free Methods LVC/HVC Parallel parts, unused
Replies: 16
Views: 2199

Re: Free Methods LVC/HVC Parallel parts, unused

I would appreciate these if you still have them zip 54603
by cassschr1
Oct 14 2015 10:50pm
Forum: E-Bike Technical
Topic: controller compatibility
Replies: 0
Views: 292

controller compatibility

Anybody know if grins 9 fet controller works with bmc geared hubs ? Its about 6 years old. Thanks
by cassschr1
Nov 16 2014 3:49pm
Forum: Battery Technology
Topic: Nissan Leaf Cells Test Data
Replies: 386
Views: 81397

Re: Nissan Leaf Cells Test Data

This is a PM I sent to John in CR. He asked me if I could post some pictures of my enclosure. So with the help of my wife here are the pictures along with the reply and my pm to John. 6 of my pictures were bigger than 512 KiB size so it would not let me upload them to this site. I do not know how to...
by cassschr1
Nov 16 2014 11:29am
Forum: E-Bike Build Threads / Photos & Video
Topic: Electric Drift Trike
Replies: 2
Views: 2912

Re: Electric Drift Trike

With a screen name of OCD I had to check out your posts. Looks like a fun time on a adult big wheel!
by cassschr1
Nov 12 2014 8:29pm
Forum: E-Bike General Discussion
Topic: Comments from strangers about your bike
Replies: 184
Views: 17230

Re: secret agent man

I got it just fine.
by cassschr1
Oct 24 2014 8:11am
Forum: General Discussion
Topic: ICE engine, 4.6L Ford, Intake Manifold Basket, what for?
Replies: 135
Views: 23135

Re: ICE engine, 4.6L Ford, Intake Manifold Basket, what for?

so let's back up a bit here. Is that picture of this engine? Do you have the engine pulled?did you find pieces of plastic in the oil pump?are the slides broken on the timing chain tensioners?
by cassschr1
Oct 24 2014 8:00am
Forum: General Discussion
Topic: ICE engine, 4.6L Ford, Intake Manifold Basket, what for?
Replies: 135
Views: 23135

Re: ICE engine, 4.6L Ford, Intake Manifold Basket, what for?

ironically I'm rebuilding a 4.0 L Ford it's still on the engine stand I didn't read this whole thread. But did you connect that wire underneath the intake manifold. That is a knock sensor maybe the computer needs it in order to work.I hope you have a Ford shop manuaI . To put the front cover on, and...
by cassschr1
Oct 20 2014 9:08pm
Forum: Battery Technology
Topic: DIY Programmable BMS (now using ATtiny/Arduino)
Replies: 218
Views: 52431

Re: DIY Programmable BMS (now using ATtiny/Arduino)

the threads been dormant for months
by cassschr1
Aug 20 2014 7:32pm
Forum: E-Bike General Discussion
Topic: Weird noise, Crystalite 5305 v2
Replies: 5
Views: 540

Re: Weird noise, Crystalite 5305 v2

I don't think it's in the hall sensor because the c_a did the blinking and I don't think Hall hall sensor would cause that