Search found 258 matches

by andreym
Sep 27 2016 3:01pm
Forum: Items for Sale - New
Topic: Eaton APR48-ES 2000w 96% efficiency power supply for sale
Replies: 8
Views: 2004

Re: Eaton APR48-ES 2000w 96% efficiency power supply for sal

4 units are on the way to liveforphysics, 3 NEW units remaining. I will also have couple used units later, they would go at a discount price. Please remember, this is not your average Eaton PSU, these are higher efficency. Almost the best efficiency on the market! Although if you buy 2 or more with ...
by andreym
Sep 02 2016 2:11am
Forum: Items for Sale - New
Topic: Eaton APR48-ES 2000w 96% efficiency power supply for sale
Replies: 8
Views: 2004

Re: Eaton APR48-ES 2000w 96% efficiency power supply for sal

Yes - I can program 4 of them to 57.5 and max current.
by andreym
Sep 01 2016 4:20pm
Forum: Items for Sale - New
Topic: Eaton APR48-ES 2000w 96% efficiency power supply for sale
Replies: 8
Views: 2004

Re: Eaton APR48-ES 2000w 96% efficiency power supply for sal

Hi Luke, The best it could do is 57.53(3.6 per cell in case of 16S life), even if I try to set higher voltage it would not go there. And I checked the CC mode at 23.8volts it charges my tesla module at 40amps (I can actually upper it a bit to like 42amps, but default setting is 40) All this at 220v ...
by andreym
Aug 31 2016 8:59pm
Forum: Items for Sale - New
Topic: Eaton APR48-ES 2000w 96% efficiency power supply for sale
Replies: 8
Views: 2004

Re: Eaton APR48-ES 2000w 96% efficiency power supply for sal

liveforphysics wrote:Can you program them to be 58.4v and whatever it's max current is like the previous generation? Do they have CC/CV function?
They do CC\CV function. I will try to program one tomorrow and will let you know :wink:
by andreym
Aug 31 2016 6:34pm
Forum: Items for Sale - New
Topic: Eaton APR48-ES 2000w 96% efficiency power supply for sale
Replies: 8
Views: 2004

Eaton APR48-ES 2000w 96% efficiency power supply for sale

Hi Folks, I have couple PSU-s with the very high efficiency. Eaton APR48-ES If you compare it with famous APR48-3G it would generate twice less heat! So more silent operation and overal better efficiency and power Could be used with adaptto controllers for up to 2000w charging power at 220-240v inpu...
by andreym
Sep 17 2015 9:26am
Forum: E-Bike Technical
Topic: Adaptto Mini-E/Max-E Owner's Thread
Replies: 5153
Views: 607857

Re: Adaptto Mini-E/Max-E Owner's Thread

for replacing R113 0603 resistor with 2-10ohm should be ok.
by andreym
May 15 2015 11:18pm
Forum: E-Bike General Discussion
Topic: MAXEBIKE Teleporter - new frames on the block
Replies: 41
Views: 11077

Re: MAXEBIKE Teleporter - new frames on the block

rider95 wrote: as a old time motocrosser
If you ever tried to motorcross with a 10kg\22lb hub motor in the rear wheel you would know that it is a bad idea.
Once again, It is a transportation vehicle, not a dirt bike.
We will make sure to eliminate pedals along with bottom bracket on our offroad bike :wink:
by andreym
May 15 2015 11:12pm
Forum: E-Bike General Discussion
Topic: MAXEBIKE Teleporter - new frames on the block
Replies: 41
Views: 11077

Re: MAXEBIKE Teleporter - new frames on the block

I know Elon Musk is pretty open about sharing his tech but the Tesla branding is a little cheeky :lol: Is this designed for 2 people ? I reckon the long, chunky moto style seat lets down the look of the bike. You know the name "Tesla" does not belong to Elon Must, don`t you? :D The owner decided to...
by andreym
May 14 2015 5:21pm
Forum: E-Bike General Discussion
Topic: MAXEBIKE Teleporter - new frames on the block
Replies: 41
Views: 11077

Re: MAXEBIKE Teleportator - new frames on the block


dogman dan wrote:But many will build for 50 mph I'm sure.
that`s for sure :)
overhauledped wrote:anyone know the width of the bottom bracket? Is it a standardized size?
It`s 100mm standart BB, like the one every fatbike has.
by andreym
Feb 16 2015 4:22am
Forum: Items for Sale - New
Topic: Vector e-bike and Parts / WORLDWIDE
Replies: 2368
Views: 376411

Re: Vector. New 10 kW ebike from scratch.

I was about to tell you using a hammer to make it fit, but looks like the seller already told you the same.
Artur, Is this your famous "warranty" work this way?
by andreym
Feb 11 2015 12:52pm
Forum: Items for Sale - New
Topic: Vector e-bike and Parts / WORLDWIDE
Replies: 2368
Views: 376411

Re: Vector. New 10 kW ebike from scratch.

Artur wrote:It is not my frame, and it was not bought from me. Have no idea why did you post it here. lol :lol:
This is from the same manufacture with exactly the same quality :)
by andreym
Feb 11 2015 12:08pm
Forum: Items for Sale - New
Topic: Vector e-bike and Parts / WORLDWIDE
Replies: 2368
Views: 376411

Re: Vector. New 10 kW ebike from scratch.

The next thing to appear would be the following I believe? https://lh4.googleusercontent.com/-IaKXR96MrGU/VMqIZIlKcWI/AAAAAAAAQmY/3zCzH3ZNngk/w1126-h1502-no/IMG_0310.JPG https://lh4.googleusercontent.com/-sQjkJaJp-Zk/VMqIZNnW5_I/AAAAAAAAQmY/keBo48cCAiI/w1126-h1502-no/IMG_0312.JPG https://lh6.googleu...
by andreym
Jan 04 2015 8:45pm
Forum: E-Bike Technical
Topic: Adaptto Mini-E/Max-E Owner's Thread
Replies: 5153
Views: 607857

Re: Adaptto Mini-E/Max-E Owner's Thread

Hey Doc, have you tried to upgrade the firmware of the old max-e with new one? If you tried it could possibly flashed a new firmware to lcd display and refused to update the controller itself. Las lcd firmware could be not completely workable with older max-e firmware. In other words, do you have on...
by andreym
Jul 03 2014 6:15pm
Forum: E-Bike Build Threads / Photos & Video
Topic: E-S Stealth Electric Bike Owners
Replies: 17198
Views: 1847434

Re: E-S Stealth Electric Bike Owners

A small clarification. This is NOT 3000wh battery. 2400max. Middle point is 74v. NOT 84v. And real capacity of element is 2.5ah, with 14p it give 35ah in ideal variant. More realistic data - 2.4ah and 33.6ah. Than you should also compare with ACTUAL stock battery data: 24s at 3.2v life would be mor...
by andreym
May 29 2014 6:29pm
Forum: Battery Technology
Topic: Samsung 25R/LG 18650HE2/ Sony VTC5 high power 18650 battery
Replies: 798
Views: 133521

Re: Samsung 25R/LG 18650HE2/ Sony VTC5 high power 18650 batt

ecruz wrote: I have not had a problem welding .2 strips whatsoever on the cheaper one.
It could be different welder. But looked similar.
The other disadvantage is you cannot use it for the large pack.
by andreym
May 29 2014 6:19pm
Forum: Battery Technology
Topic: Samsung 25R/LG 18650HE2/ Sony VTC5 high power 18650 battery
Replies: 798
Views: 133521

Re: Samsung 25R/LG 18650HE2/ Sony VTC5 high power 18650 batt

Very interested. What thickness tabs were you able to weld? What calculations did you use to size the tabs? What vendor did you use for the DN10? Link? Cost? I have not tried more than 0.3mm thick, But manufacture tells it is able to weld up top 2.6mm (what i doubt) but up to 1mm thick I believe it...
by andreym
May 29 2014 9:49am
Forum: Battery Technology
Topic: Battery assembly kit for 18650 cells - first prototype
Replies: 165
Views: 38618

Re: Battery assembly kit for 18650 cells - first prototype

The fuse adds 7.5mΩ per cell. Which is ~10% for LG D1 and most other cells. From my test it is clear that these fuses are not very practical for high power cells, such as Sony VTC5. For those cells a different fuse design would be needed. I do have it in mind and will offer solution later on. So no...
by andreym
May 29 2014 9:32am
Forum: Battery Technology
Topic: Samsung 25R/LG 18650HE2/ Sony VTC5 high power 18650 battery
Replies: 798
Views: 133521

Re: Samsung 25R/LG 18650HE2/ Sony VTC5 high power 18650 batt

These welders are too low power - my friend tested one and he succeed to weld only 0.1 nickel strip max. So I decided to get more powerfull one :twisted: DN-10 means 10kw I believe. 35AC barker is barely usable at 240V AC, 25a hits immediately when you try. btw wires are 50mm2 and they become quite ...
by andreym
May 29 2014 8:44am
Forum: Battery Technology
Topic: Battery assembly kit for 18650 cells - first prototype
Replies: 165
Views: 38618

Re: Battery assembly kit for 18650 cells - first prototype

really nice design! However I have couple questions: -have you tested the resistance of your interconnections? I mean how many milliOhms it adds to the internal resistance of the pack? -what is the material? thickness? The reason I`m asking is when you playing with cells like LG D1 or Samsung 30B, t...
by andreym
Apr 20 2014 3:44pm
Forum: Items for Sale - New
Topic: Advanced ADAPTTO controllers and compatible products
Replies: 1595
Views: 251096

Re: The most advanced Adaptto Mini-E Controller + BMS

Max-E@72v LiFePo4 with Crystalyte 5403. 0-50km/h in 2.2seconds, how it that for an advertiser Andrey :) Just Awesome, Alex! Thanks for the vid, and for all Crystalyte 5403 owners now we know correct pwr timing settings for best acceleration :D although your video shows motor and controller temperat...
by andreym
Apr 20 2014 3:28pm
Forum: Items for Sale - New
Topic: Advanced ADAPTTO controllers and compatible products
Replies: 1595
Views: 251096

Re: The most advanced Adaptto Mini-E Controller + BMS

Falco wrote:I have sent 2 pms and a email
replied in PM yesterday.
by andreym
Apr 16 2014 1:26am
Forum: E-Bike Build Threads / Photos & Video
Topic: GT E-drive from Russia
Replies: 287
Views: 64146

Re: GT E-drive from Russia

ivanovlev wrote:In memories of gt-i drive:
RIP :(
I`d better say, "upgraded" :)
by andreym
Apr 15 2014 1:10am
Forum: Motor Technology
Topic: 3<->8 kW motor comparsion
Replies: 34
Views: 7134

Re: 3<->8 kW motor comparsion

zombiess wrote:John the 90% efficiency I was referring to was the Cromotor V2/V3, the newest design.
Once again, where is your evidence?
I have seen many dyno test datas on QS205 motors, the ones used to make Cromotors V2\3 from and none of them have 90+ % efficiency,
Please post one if you have it.
by andreym
Apr 13 2014 5:52pm
Forum: Motor Technology
Topic: 3<->8 kW motor comparsion
Replies: 34
Views: 7134

Re: 3<->8 kW motor comparsion

The Cromotor is > 90% efficiency. Where is your evidence? There is no data shows any version of cromotor have efficiency more than 87% ! If you have such data please share or do not tell anybody the numbers you cannot proof :) Looking at the 3rd row Max power out you see Vin = 69 Ain = 143 Win in 9...