Search found 9041 matches

by Hillhater
Jan 23 2019 6:39am
Forum: E-Bike Technical
Topic: Alternative Battery packs
Replies: 5
Views: 129

Re: Alternative Battery packs

What voltage & capacity pack do you need ? Personally, i would keep it intact as a backpack ( i run 36-42 v system). and prefer to use a backpack set up anyway, Other options.. Tumic , in the sales section...sells both single sells (various brands) , v cheap, ....also premade 36v, 14ah packs for app...
by Hillhater
Jan 23 2019 6:10am
Forum: Battery Technology
Topic: cylinder vs prismatic battery cell advantages?
Replies: 13
Views: 2983

Re: cylinder vs prismatic battery cell advantages?

...... hence Tesla can smash out thousands of Model 3 packs each day. ...... i
They hope.....but Not quite yet ..
Teslas current M3 production rate is under 700/day, and one of their main problems has been insufficient pack supply.
by Hillhater
Jan 23 2019 5:54am
Forum: Battery Technology
Topic: Toyota and Panasonic form huge battery R&D & production partnership
Replies: 12
Views: 342

Re: Toyota and Panasonic form huge battery R&D & production partnership

dustNbone wrote:
Jan 22 2019 1:51pm
I find it interesting that the biggest (only?) players in the lithium battery business (Panasonic, LG, Toshiba, Sony and Samsung) are based in Japan and Korea.

2 countries that also happen to be very good at making cars.
SAFT..France
A123.. USA
BYD..China
XALT..USA
Etc
by Hillhater
Jan 18 2019 1:56am
Forum: E-Vehicles General Discussion
Topic: Wind and Solar vs Coal, Gasoline, Nuclear
Replies: 3228
Views: 109927

Re: Wind and Solar vs Coal, Gasoline, Nuclear

Cephalotus wrote:
Jan 17 2019 3:14pm

The Haliade-X 12 MW also features a 63% capacity factor
You do realise that is a THEORETICAL gross capacity factor. ?
Its not an actual monitored result....its just sales patter exaggeration !
..and they never disclose the internal power consumption or NET output under controlled tests.
by Hillhater
Jan 17 2019 9:57pm
Forum: E-Vehicles General Discussion
Topic: Wind and Solar vs Coal, Gasoline, Nuclear
Replies: 3228
Views: 109927

Re: Wind and Solar vs Coal, Gasoline, Nuclear

, .......that's where oil and fossils have been almost priceless to the point of our own climates destruction.... ...climate destruction ?... What indicators of this climate destruction do you have ? Last i heard, the planet was getting greener, and the population increasing ! (too much). Hardly in...
by Hillhater
Jan 16 2019 6:00pm
Forum: E-Vehicles General Discussion
Topic: Wind and Solar vs Coal, Gasoline, Nuclear
Replies: 3228
Views: 109927

Re: Wind and Solar vs Coal, Gasoline, Nuclear

Settling Mars ? Even if we had a Nuclear Holocost, combined with double the predicted global warming.... The Earth would still be a far more habitable place than Mars .! We couldnt even sustain an orbiting space station with only a few hours travel from support, let alone a remote colony base on a p...
by Hillhater
Jan 14 2019 2:52pm
Forum: E-Vehicles General Discussion
Topic: Wind and Solar vs Coal, Gasoline, Nuclear
Replies: 3228
Views: 109927

Re: Wind and Solar vs Coal, Gasoline, Nuclear

Our economy is fine. Privatley for me energy prices are perfectly fine. I could very easy pay twice or three times per kWh for electricity, heating and fuel. If needed I could even pay 10 times (would not like to do that), but this is not even likely. But..its not about YOU .! ...its about that hug...
by Hillhater
Jan 14 2019 5:51am
Forum: E-Vehicles General Discussion
Topic: Wind and Solar vs Coal, Gasoline, Nuclear
Replies: 3228
Views: 109927

Re: Wind and Solar vs Coal, Gasoline, Nuclear

^^^^^
I wonder how much power is used in those "accellerators" ...
..IE what is the energy conversion efficiency of the system ?
by Hillhater
Jan 13 2019 7:28pm
Forum: E-Bike Non-hub Motor Drives
Topic: New "TSDZ2 Torque Sensor Central Motor"
Replies: 4240
Views: 296633

Re: New "TSDZ2 Torque Sensor Central Motor"

Does anyone know if there is anywhere to buy spares (blue/metal gears) in Australia ?
by Hillhater
Jan 13 2019 7:25pm
Forum: E-Bike Non-hub Motor Drives
Topic: DH frames for freeriding
Replies: 37
Views: 760

Re: DH frames for freeriding

With a mid drive, i route the power cable up the seat tube (external) to a connector under the seat. Backpack cable runs down to the back of the seat for connection Allow enough coiled cable to enable mount/dismount easy. Recommend a easy pull connector incase of emergency. :wink: All very stealth a...
by Hillhater
Jan 13 2019 4:44pm
Forum: E-Bike Non-hub Motor Drives
Topic: DH frames for freeriding
Replies: 37
Views: 760

Re: DH frames for freeriding

Tommm wrote:
Jan 13 2019 10:31am
Only negative of DH frames is they generally have little space for a battery.
Any ebike, especially serious off road ebiles , ride so much better wothout the battery fixed to the frame.
A backpack battery is a huge step up from fixed packs, and often much more secure from theft.
by Hillhater
Jan 13 2019 4:32pm
Forum: E-Bike Non-hub Motor Drives
Topic: tsdz2 torque assist failure?
Replies: 4
Views: 139

Re: tsdz2 torque assist failure?

Are you running the original factory software, or a reflashed version of the modified software .?
by Hillhater
Jan 12 2019 2:18am
Forum: E-Bike Non-hub Motor Drives
Topic: New "TSDZ2 Torque Sensor Central Motor"
Replies: 4240
Views: 296633

Re: New "TSDZ2 Torque Sensor Central Motor"

Another "clicking noise" ?? Im sure the answer is in this thread somewhere, but searches have not turned up anything like this .. Low km drive ..<< 100 km .48v , and .working fine last time used. After a month or so of no use, i noticed that the drive "jammed" momentarily when movening the bike back...
by Hillhater
Jan 11 2019 5:47pm
Forum: E-Vehicles General Discussion
Topic: Wind and Solar vs Coal, Gasoline, Nuclear
Replies: 3228
Views: 109927

Re: Wind and Solar vs Coal, Gasoline, Nuclear

Numbers and averages can be deceptive. You may well already have 60% power from RE .."Averaged over the year" .. But there are many periods when wind and solar are contributing almost nothing., and the 100% thermal back up plants have to save the day... Where is the problem? At the end of the year ...
by Hillhater
Jan 11 2019 1:57am
Forum: E-Vehicles General Discussion
Topic: Wind and Solar vs Coal, Gasoline, Nuclear
Replies: 3228
Views: 109927

Re: Wind and Solar vs Coal, Gasoline, Nuclear

Numbers and averages can be deceptive. You may well already have 60% power from RE .."Averaged over the year" .. But there are many periods when wind and solar are contributing almost nothing., and the 100% thermal back up plants have to save the day. No matter how many wind turbines and Solar Farms...
by Hillhater
Jan 08 2019 10:12pm
Forum: E-Vehicles General Discussion
Topic: Wind and Solar vs Coal, Gasoline, Nuclear
Replies: 3228
Views: 109927

Re: Wind and Solar vs Coal, Gasoline, Nuclear

rooftop PV solar ! :shock: Don't forget to subtract grid installation and maintenance/distribution costs from that. Why ? If you want to benefit from FIT or have power during the night,...you will need the grid. And if you were off grid, you would have to add on the cost of storage... ......and mos...
by Hillhater
Jan 08 2019 9:59pm
Forum: E-Vehicles General Discussion
Topic: Wind and Solar vs Coal, Gasoline, Nuclear
Replies: 3228
Views: 109927

Re: Wind and Solar vs Coal, Gasoline, Nuclear

According to Lazzard..
The only generating methods more expensive than CSP are diesel reciprocating , and rooftop PV solar ! :shock:
by Hillhater
Jan 08 2019 5:54pm
Forum: E-Vehicles General Discussion
Topic: Video- Inside the massive Gigafactory where Tesla will soon make 60 percent of the world’s lithium-ion batteries
Replies: 21
Views: 748

Re: Video- Inside the massive Gigafactory where Tesla will soon make 60 percent of the world’s lithium-ion batteries

MJSfoto1956 wrote: Tesla. For the same reason that Standard Oil didn't get the credit for the Model T.
:?:
Standard supplied the fuel...Ford made the tank to store it in
Tesla’s fuel is electrons..from the grid or a power point. The “fuel” is stored in cells produced By Panasonic .!
by Hillhater
Jan 08 2019 2:12pm
Forum: E-Vehicles General Discussion
Topic: Video- Inside the massive Gigafactory where Tesla will soon make 60 percent of the world’s lithium-ion batteries
Replies: 21
Views: 748

Re: Video- Inside the massive Gigafactory where Tesla will soon make 60 percent of the world’s lithium-ion batteries

The practical question isn't really who was the first to do it inhouse, or who is still doing it inhouse, but who actually made it work as economy of scale.... Yes, but as I say, that is yet to be done in the GF. They are not yet at 25% capacity, and “who” should be credited with amy success anyway...
by Hillhater
Jan 07 2019 9:26pm
Forum: E-Vehicles General Discussion
Topic: Wind and Solar vs Coal, Gasoline, Nuclear
Replies: 3228
Views: 109927

Re: Wind and Solar vs Coal, Gasoline, Nuclear

That's a huge margin of error!! So yeah, the ~50 years of GOOD data statement applies. We just weren't thinking about climate as much in the past, so the trail from here to there is pretty murky... And remember , the only consistent temperature measurement records available for the past 100+ years ...
by Hillhater
Jan 07 2019 9:11pm
Forum: Large EV General Discussion
Topic: Tesla M3 teardown information video - Hallbach Array Motor
Replies: 15
Views: 436

Re: Tesla M3 teardown information video - Hallbach Array Motor

If you rode a M'bike or drove a Tesla, you might just find your engine does rev to 15k ! And if you worked on a Toyota/Lexus hybrid you might also find 7-800volt drive systems. The race track in often the birthplace and prooving ground of tomorrows road car technology. Industry uses a whole range of...
by Hillhater
Jan 07 2019 5:50pm
Forum: Large EV General Discussion
Topic: Tesla M3 teardown information video - Hallbach Array Motor
Replies: 15
Views: 436

Re: Tesla M3 teardown information video - Hallbach Array Motor

TilmanBaumann wrote:
Jan 07 2019 4:37pm
The future of performance EV seems to be high voltage if you read the current developments on that era.
yes. Note the latest FE cars run 900volt systems..battery included.
by Hillhater
Jan 06 2019 11:16pm
Forum: Electric Aircraft
Topic: Rolls-Royce world’s fastest all-electric aircraft
Replies: 5
Views: 247

Re: Rolls-Royce world’s fastest all-electric aircraft

Flight performance is always dictated by (amoungst many other things)... Power and weight. And in the case of electric aircraft, that weight is dictated by battery capacity/power ratios. I suspect this RR design is a compromise on battery weight/discharge power, endurance, and capacity. IE, they cou...
by Hillhater
Jan 06 2019 6:36pm
Forum: General Discussion
Topic: List of small hatchback cars
Replies: 117
Views: 4262

Re: List of small hatchback cars

An electric 2CV, my dream car. Never hod so much fun driving a slow car. .... In the '70s, i lived/worked in Spain. A group of us "owned" an old 2CV. ..no roof, no doors, no seats other than the drivers, no exhaust, ....and not much rubber on the tires !...... ..but, yes, a great fun car. :lol: :lol:
by Hillhater
Jan 06 2019 5:40pm
Forum: Battery Technology
Topic: Samsung 50E capacity testSamsung 50E capacity test - 5000mAh or not?
Replies: 11
Views: 689

Re: Samsung 50E capacity testSamsung 50E capacity test - 5000mAh or not?

Hmmmm missing true four wire setup for accurate test results. The terminal sens wires must separately connected to the copper plate."... Yes ,.TH has had this pointed out several times, and is working on a revised set up.! For a true "4 wire" test, the voltage sense connections should be directly o...