Re: A2B Metro - www.ultramotor.com - Video Page4 by Ypedal ยป Tue Feb 11, 2014 7:39 pm Yikes !! rider weight ? Rider weight = 80kg+5kg satchel. No extra loading apart from rear battery. The second hand replacement swingarm was also already showing hairline cracks in the same locations. Definitely a ...
- Feb 11 2014 7:38pm
- Forum: E-Bike Reviews & Testing
- Topic: A2B Metro - www.ultramotor.com - Video Page4
- Replies: 405
- Views: 72347
Re: A2B Metro - www.ultramotor.com - Video Page4
Check your frame from underside and thoroughly cleaned before dropping big $$$ into new batteries. My frame with cracks from the drain and cable holes finally let go, spread to swingarm weld and snapped the banana swinger like... A banana. Locked rear wheel on rear battery pack was good because it ...