Search found 66 matches

by avoleoo
Jan 05 2019 4:18pm
Forum: Items Wanted
Topic: Need any kind of Bafang LCD
Replies: 0
Views: 71

Need any kind of Bafang LCD

Hi, I have a couple of Bafang 8FUN controllers that I want to test and I need the LCD. Maybe someone has it...

The plug has to be higo green color female.

Thanks.
by avoleoo
Sep 08 2018 9:58pm
Forum: E-Bike General Discussion
Topic: Please help to identify controller connectors ( pinouts )
Replies: 2
Views: 155

Re: Please help to identify controller connectors ( pinouts )

Allright, Got every except battery connector 3 upper wires.
Is anyone here with the same controller?
by avoleoo
Sep 08 2018 7:33pm
Forum: E-Bike General Discussion
Topic: Please help to identify controller connectors ( pinouts )
Replies: 2
Views: 155

Please help to identify controller connectors ( pinouts )

Hi guys, hopefully someone can point me into right direction. I got this 8fun controller that I would like to use on my bike, but I'm not sure what is what ( pinout ) One of the connectors (top) seems to be splittable with additional cable, splits into Display / Throttle / Brake switches I don't see...
by avoleoo
Sep 08 2018 8:23am
Forum: E-Vehicles General Discussion
Topic: Please help to identify connectors ( pinout )
Replies: 1
Views: 430

Please help to identify connectors ( pinout )

Hi guys, hopefully someone can point me into right direction. I got this 8fun controller that I would like to use on my bike, but I'm not sure what is what ( pinout ) One of the connectors (top) seems to be splittable with additional cable, splits into Display / Throttle / Brake switches I don't see...
by avoleoo
Jun 12 2018 3:20pm
Forum: Battery Technology
Topic: bluetooth BMS?
Replies: 861
Views: 51188

Re: bluetooth BMS?

awesome, thank you!
by avoleoo
Jun 12 2018 2:06pm
Forum: Battery Technology
Topic: bluetooth BMS?
Replies: 861
Views: 51188

Re: bluetooth BMS?

I have a question to Smart BMS owners about balancing. Let's say I set BMS balance voltage to 4.05V but charge the battery to 4.2V, is it going to always bleed down all cells to 4.05V or is it going to balance as long as it's charging? Either way if charger will be set at 4.2 v per cell BMS will try...
by avoleoo
Jun 08 2018 6:16am
Forum: E-Bike General Discussion
Topic: Watt or Ah Meter Options?
Replies: 10
Views: 569

Re: Watt or Ah Meter Options?

Thanks guys for your replies, I have placed an order for this one: https://www.aliexpress.com/item/50A-New-TK15-Professional-Precision-Battery-Tester-for-LiFePO-Coulomb-Counter-Free-Shipping-with-Tracking-Number/32702066121.html And I have also ordered one that Rote suggested to be placed at the Mea...
by avoleoo
Jun 06 2018 6:53am
Forum: Items Wanted
Topic: Cycle Analyst and Controller.
Replies: 0
Views: 159

Cycle Analyst and Controller.

Looking to buy used CA 2.4 or 3 with 30A or more controller in working order.
by avoleoo
Jun 04 2018 12:19pm
Forum: E-Bike General Discussion
Topic: Watt or Ah Meter Options?
Replies: 10
Views: 569

Re: Watt or Ah Meter Options?

Looked into these guys, but I would really like to find a smaller or rather more integrated solution. https://www.ebay.com/itm/150-AMP-WATT-METER-WITH-SPECIAL-HEAVY-GA-WIRE-WIND-GENERATOR-SOLAR-DC-INLINE/272061542420?hash=item3f5821b014:g:w50AAOSwfVpYpd8V:sc:USPSFirstClass!33467!US!-1 Love CA, but i...
by avoleoo
Jun 04 2018 12:16pm
Forum: E-Bike General Discussion
Topic: Watt or Ah Meter Options?
Replies: 10
Views: 569

Watt or Ah Meter Options?

Been using CA 2.4 for last 5 years and really like used Ah meter where I know precisely how much juice I have left. Now building my second bike and planning on using S12S with LCD3, however I believe the only measure is the battery bar which is not good enough for estimating range. What are other op...
by avoleoo
May 24 2018 3:14pm
Forum: E-Bike General Discussion
Topic: How many miles on your e-bike?
Replies: 16
Views: 863

How many miles on your e-bike?

And what's your story? :) Mileage: 6000 Bike: Montague Paratrooper 26" Folding Bike MAC 10T, 9fet Infineon set to 17amps, 14S6P 18650, max speed 32mph, ordered hpc bag for my diy batteries. Started with salvaged laptop cells and now running tesla cells. Amazed that everything is still holding up we...
by avoleoo
May 17 2018 12:14pm
Forum: E-Bike General Discussion
Topic: Ideas about charging batteries
Replies: 8
Views: 444

Re: Ideas about charging batteries

Allright, I think I came up with the solution.

Buy a charger that would still bulk charge to 4.05 x 14 = 56.7v and charge them off the bike only when going for longer rides. Sounds like a good compromise.
by avoleoo
May 17 2018 11:37am
Forum: E-Bike General Discussion
Topic: Ideas about charging batteries
Replies: 8
Views: 444

Ideas about charging batteries

I run 2 x 7S6P Tesla 18650 packs on my ebike in series for total 14s6p. Since I ride a lot, Im getting tired taking them off the bike, bringing them inside, charging them and putting them back on the bike, so maybe you guys can share with experience about alternative and more convenient ways to char...
by avoleoo
Mar 08 2018 3:22pm
Forum: General Discussion
Topic: Battery Efficiency Question 56v vs 32v
Replies: 12
Views: 724

Re: Battery Efficiency Question 56v vs 32v

Allright, turns out my riding style and the way I use Polaris was the problem. I'm used to use throttle on MAC 10T bike, however, Polaris is just very inefficient with it having a small DD motor. If I do pedal assist only on Polaris, all the readings are good 18wh/m same route and conditions, but as...
by avoleoo
Mar 06 2018 7:20pm
Forum: General Discussion
Topic: Battery Efficiency Question 56v vs 32v
Replies: 12
Views: 724

Re: Battery Efficiency Question 56v vs 32v

Buk: good one, it's a possibility ! I will go for a ride tomorrow and will just ride differently and will use other gears.
by avoleoo
Mar 06 2018 7:01pm
Forum: General Discussion
Topic: Battery Efficiency Question 56v vs 32v
Replies: 12
Views: 724

Re: Battery Efficiency Question 56v vs 32v

Nope, CA is on bike one, which has MAC 10T
Bike two - Polaris, I can only measure what I have used by charging back the battery with iCharger and noting Ah.
by avoleoo
Mar 06 2018 6:29pm
Forum: General Discussion
Topic: Battery Efficiency Question 56v vs 32v
Replies: 12
Views: 724

Re: Battery Efficiency Question 56v vs 32v

Yup, I understand that. Let's assume the issue is within the bike, what could be wrong with it? Heck its production bike and Polaris is bragging about it being very efficient in their videos. It is using direct drive part of the motor while going at 20mph, and if it's very high wind motor, could it ...
by avoleoo
Mar 06 2018 5:51pm
Forum: General Discussion
Topic: Battery Efficiency Question 56v vs 32v
Replies: 12
Views: 724

Re: Battery Efficiency Question 56v vs 32v

Completely flat ! all pavement, both ridden at 20mph.

Top speeds:
bike 1: 35mph
bike 2: 20mph limited by factory, so I don't know the wind count of the motor, but feels like it could go way faster. Maybe around 260 - 320.
by avoleoo
Mar 06 2018 5:43pm
Forum: General Discussion
Topic: Battery Efficiency Question 56v vs 32v
Replies: 12
Views: 724

Battery Efficiency Question 56v vs 32v

Allright having a problem here. Two bikes, two different voltage batteries, both ridden the same. The bike with 56v system averages 18wh/m The bike with 32v system averages 30wh/m Am I missing something why there is such a difference? Bike one: Mac 10T in 26" | 15A max | 56v, 8AH = averages 18wh/m @...
by avoleoo
Feb 19 2018 2:26pm
Forum: Battery Technology
Topic: Tesla 18650 question
Replies: 16
Views: 873

Re: Tesla 18650 question

Right BT-C3400 is all over the place with results, very unreliable and heats up the batteries even at 0.5A disharge. Would not suggest to anyone. Yes iChargers are awesome !
by avoleoo
Feb 18 2018 7:48pm
Forum: Battery Technology
Topic: Tesla 18650 question
Replies: 16
Views: 873

Re: Tesla 18650 question

https://cdn.pbrd.co/images/H8hErJ0.png Allright, managed to hook up 206B to the laptop and attach the temp sensor. The only 18650 holder I had was cheap chinese one with thin wires, that explains the voltage sag, however, my goal was to check the temperature. So here is the discharge graph at 3.5A....
by avoleoo
Feb 17 2018 7:28am
Forum: Battery Technology
Topic: Tesla 18650 question
Replies: 16
Views: 873

Re: Tesla 18650 question

Will see if I can hook up temperature sensor to 206B and link it with the PC to get any useful data. Then we can evaluate.
by avoleoo
Feb 16 2018 9:33pm
Forum: Battery Technology
Topic: Tesla 18650 question
Replies: 16
Views: 873

Re: Tesla 18650 question

Amberwolf : I am using Opus BT-C3400 to discharge them at 1A and for more discharging power I use iCharger 206B, so current and capacity measures comes from these chargers. Hillhater : Assuming my inside temperature is 25C and your chart data, by the end of the discharge cycle I would get 55C which...
by avoleoo
Feb 15 2018 10:18pm
Forum: Battery Technology
Topic: Tesla 18650 question
Replies: 16
Views: 873

Re: Tesla 18650 question

Okey, discharged another one at 3A and did not noticed any difference in heat. I'm assuming that it's just a working temperature. I can keep my fingers on it as long as I want, it's hot but not burning. Too bad i don't have a IR temp meter.
by avoleoo
Feb 15 2018 7:43pm
Forum: Battery Technology
Topic: Tesla 18650 question
Replies: 16
Views: 873

Tesla 18650 question

Hi guys, got a tesla module and took it apart, measured some cells, comes up at 3000 - 3050mah - good, however, when discharging at 1A, which is what, like 0.3C, cells do get hot. Does anyone has experience with these cells? I had an impression that I could do at least 1.5C to 2C without them being ...