Re: LG Chem lgx p1 16s1p 15Ah 10C

Data after tests

12,5Ah under load: 40A
IR 10mOhm
by FietsCycles
May 13 2019 2:28pm
Forum: Items for Sale - Used
Topic: LG Chem lgx p1 16s1p 15Ah 10C
Replies: 8
Views: 350

Re: LG Chem lgx p1 16s1p 15Ah 10C

Sent you PM
by FietsCycles
May 13 2019 12:44pm
Forum: Items for Sale - Used
Topic: LG Chem lgx p1 16s1p 15Ah 10C
Replies: 8
Views: 350

LG Chem lgx p1 16s1p 15Ah 10C

For sale LG Chem lgx p1 modules

16s1p
Capacity 15Ah
Max current 10C
IR 10mOhm
Weight 7,45kg

More than 100 in stock
Possible to buy with BMS wiring

Image

Image

150 euro a module
by FietsCycles
May 06 2019 1:48pm
Forum: Resources & EV Related Parts and Services
Topic: UK & EUROPE EV PARTS SUPPLIERS
Replies: 35
Views: 27012

Re: UK & EUROPE EV PARTS SUPPLIERS

https://ebikers.eu/

Ready to use eletrics kit, motors, controllers
Got some motors from there, everything's good
by FietsCycles
May 06 2019 12:51pm
Forum: Items for Sale - Used
Topic: New Li-Ion Sanyo NCR 18650GA 3450mAh - 10A - Europe - New Cells Panasonic Samsung LG
Replies: 27
Views: 3918

Re: New Li-Ion Sanyo NCR 18650GA 3450mAh - 10A - Europe - New Cells Panasonic Samsung LG

Small amount of Sanyo Ga is in stock.

Price starts at 1,95 euro
+200 1,9 euro
+500 1,8 euro
by FietsCycles
Apr 10 2019 4:54am
Forum: Items for Sale - Used
Topic: New Li-Ion Sanyo NCR 18650GA 3450mAh - 10A - Europe - New Cells Panasonic Samsung LG
Replies: 27
Views: 3918

Re: New Li-Ion Sanyo NCR 18650GA 3450mAh - 10A - Europe - New Cells Panasonic Samsung LG

Sorry for the long response time, I was out of town.

At this moment Sanyo GA, Panasonic PF, Samsung 35E are out of stock.
by FietsCycles
Mar 28 2019 6:58am
Forum: Items for Sale - New
Topic: Kokam Li-ion / Polymer Cell 3.7V 53Ah SLPB120216216
Replies: 0
Views: 189

Kokam Li-ion / Polymer Cell 3.7V 53Ah SLPB120216216

New Kokam cells 3.7V 53Ah Dimension (mm) 226.0 x 227.0 x 12.00 Weight 1.095kg Max. Discharge Rate Max. Discharge Rate Continuous 5C Pulse 8C Energy Density 179 Wh/kg 55 euro a cell https://i.imgur.com/50wP174.jpg?1 https://i.imgur.com/uuskhrD.jpg https://i.imgur.com/XEm8fwZ.jpg Shipping from EU - fr...
by FietsCycles
Mar 26 2019 3:29am
Forum: Items for Sale - Used
Topic: New Li-Ion Sanyo NCR 18650GA 3450mAh - 10A - Europe - New Cells Panasonic Samsung LG
Replies: 27
Views: 3918

Re: New Li-Ion Sanyo NCR 18650GA 3450mAh - 10A - Europe - New Cells Panasonic Samsung LG

nukezero wrote:
Mar 25 2019 3:55pm
Are you able to spot weld some cells?

For example, if I buy 40 cells from you, can you spot weld 10 packs of 1S4P ? Then send me some nickel tabs for me to manually solder later?

Thanks
Yes, we also do spot welding, please send me PM for more details.
by FietsCycles
Mar 06 2019 12:31pm
Forum: Items for Sale - New
Topic: New Sanyo Ga 18650 3450mAh 10A
Replies: 0
Views: 291

New Sanyo Ga 18650 3450mAh 10A

Original Li-Ion Sanyo NCR 18650GA cells 3450mAh - 10A Price starts at 1,95 euro +200 1,9 euro +500 1,8 euro +2000 1,6 euro Sanyo GA from new unused battery packs with zero cycles - 2017-2018. All cells have nominal, factory voltage ~3,5V. If the cell is bad or damaged = refund or we send you new one...
by FietsCycles
Feb 26 2019 10:43am
Forum: Items for Sale - Used
Topic: Bafang BBS02B 750W Europe
Replies: 4
Views: 434

Re: Bafang BBS02B 750W Europe

Shipping in EU 15euro
by FietsCycles
Feb 22 2019 6:47am
Forum: Items for Sale - Used
Topic: New Li-Ion Sanyo NCR 18650GA 3450mAh - 10A - Europe - New Cells Panasonic Samsung LG
Replies: 27
Views: 3918

Re: New Li-Ion Sanyo NCR 18650GA 3450mAh - 10A - Europe - New Cells Panasonic Samsung LG

Hi I am looking to build a 20s12p or 20s14p battery which will be combined with a MXUS 4t motor. I am thinking of Sanyo 18650 GA as you describe: genuine Li-Ion Sanyo NCR 18650GA cells 3450mAh - 10A. How much will you charge me for 250 cells shipped to UK (or 280 cells )? You mentioned in your post...
by FietsCycles
Feb 21 2019 5:53pm
Forum: Items for Sale - New
Topic: New 18650 Li-Ion LG MG1 3,6V 2900mAh 10A 1,45€
Replies: 0
Views: 293

New 18650 Li-Ion LG MG1 3,6V 2900mAh 10A 1,45€

New cells from unused batterypacks which were wrongly welded. Cells hold factory parameters. Voltage 3,6V Capacity 2900mAh Max. continuous discharge current 10A 2017-2018 Cells are packed by 10's Nickel strips are very easy to remove with simple pliers. 1,45€ < 100 1,40€ <200 +300 individual discou...
by FietsCycles
Feb 20 2019 2:04am
Forum: Items for Sale - Used
Topic: Bafang BBS02B 750W Europe
Replies: 4
Views: 434

Re: Bafang BBS02B 750W Europe

Cheburator wrote:
Feb 20 2019 12:20am
Could you please add detailed photo of cracked mounting bracket?
In attachment
by FietsCycles
Feb 19 2019 1:35pm
Forum: Items for Sale - Used
Topic: Bafang BBS02B 750W Europe
Replies: 4
Views: 434

Bafang BBS02B 750W Europe

Bafang BBS02B 750W The contoller set for 15A, about 7000km on it. Recent service - cleaned and re-greased - motor and controller in perfect condition. Visual 3/5 - rock hits marks, paint scratches The mounting bracket has a small crack - probably can be welded; and the thumb throttle need to be repl...
by FietsCycles
Feb 19 2019 1:19pm
Forum: Items for Sale - Used
Topic: DH FR frame for eletric bike Antidote Lifeline Europe
Replies: 0
Views: 261

DH FR frame for eletric bike Antidote Lifeline Europe

For sale frame from my private collection: Antidote LifeLine 2010/2011 size L One of a few aluminium frames made by Antidote Frame has built in battery case (3D printed elements with acryl covers) for 80 cells + BMS Perfect for mid drive conversion Technical condition 5/5 Visual condition 4/5 some s...
by FietsCycles
Feb 09 2019 10:02am
Forum: Items for Sale - Used
Topic: New Li-Ion Sanyo NCR 18650GA 3450mAh - 10A - Europe - New Cells Panasonic Samsung LG
Replies: 27
Views: 3918

Re: New Li-Ion Sanyo NCR 18650GA 3450mAh - 10A - Europe - New Cells Panasonic Samsung LG

glyndwr wrote:
Feb 07 2019 6:43pm
only looking for 4 cells delivery to the UK,

you ok with only selling 4.

Thanks
Sent you pm
by FietsCycles
Dec 31 2018 10:32am
Forum: Items for Sale - New
Topic: New 250W and 500W geard bldc motors
Replies: 6
Views: 712

Re: New 250W and 500W geard bldc motors

Shipping in EU 15euro
by FietsCycles
Dec 27 2018 10:38am
Forum: Items for Sale - Used
Topic: New Li-Ion Sanyo NCR 18650GA 3450mAh - 10A - Europe - New Cells Panasonic Samsung LG
Replies: 27
Views: 3918

Re: New Li-Ion Sanyo NCR 18650GA 3450mAh - 10A - Europe

Winter stock clearance sale

2.10 euro for cell, order 100+

Even bigger discounts for orders above 200+
by FietsCycles
Dec 16 2018 8:10am
Forum: Items for Sale - New
Topic: New 250W and 500W geard bldc motors
Replies: 6
Views: 712

Re: New 250W and 500W geard bldc motors

mxer wrote:
Dec 16 2018 7:36am
FietsCycles wrote:
Dec 15 2018 3:31pm
mxer wrote:
Dec 15 2018 11:51am
Free shipping to the UK? :wink:
500w or 250w?
500w freewheel

Currently in stock I have only with cassette mounting 500w motor, but I should have spacers if you want to put only 1 cog
by FietsCycles
Dec 15 2018 3:31pm
Forum: Items for Sale - New
Topic: New 250W and 500W geard bldc motors
Replies: 6
Views: 712

Re: New 250W and 500W geard bldc motors

mxer wrote:
Dec 15 2018 11:51am
Free shipping to the UK? :wink:
500w or 250w?