bms and spot welder

hi. 1, am looking to buy a spot welder that is a level up from the cheap Chinese ones so that it is within its comfort zone to make quality welds and not need to be rested too often. and 2 please, am having great difficulty finding a bms for a 80A peak, 50A continuous rating make from either 14s8p 2...