Does this look like electrical failure?
Does this look like electrical failure?
A customer returned this charger I sold them, claiming it overheated and melted the wires.
I opened the case and it looks flawless inside. Is it me or do these wires look like they were cut? I just don't see melted insulation anywhere.
This customer has said some conflicting things about how they used it.
I opened the case and it looks flawless inside. Is it me or do these wires look like they were cut? I just don't see melted insulation anywhere.
This customer has said some conflicting things about how they used it.
- Attachments
-
- 20200608_180927-1.jpg (315.34 KiB) Viewed 873 times
-
- 20200608_180957-1.jpg (359.9 KiB) Viewed 873 times
-
- 20200608_180937-1.jpg (389.85 KiB) Viewed 873 times
-
- 20200608_180950-1.jpg (392.82 KiB) Viewed 873 times
Mush! Mush you electrons! Push harder!
Re: Does this look like electrical failure?
Those cables were cut somehow.
-
- Posts: 81
- Joined: Apr 02 2020 7:42pm
Re: Does this look like electrical failure?
What he said.
Sent from my SM-G975F using Tapatalk
Sent from my SM-G975F using Tapatalk
Re: Does this look like electrical failure?
Probably got stuck in the spokes. Rewire, test, and send it.
- e-beach 1.21 GW
- Posts: 3788
- Joined: Jan 10 2012 9:48pm
- Location: Any Los Angeles area beach I am at. Or Santa Monica or possibly the south bay beaches.
Re: Does this look like electrical failure?
IMO the insulation was cut, the wires pulled and cut and the mess was made. Shorts happen on one spot that is closest/is the short. You have seen it before, a burned spot where the short happened. As stated above, rewire and test. BTW, document your testing of the unit for future proof in case of dispute.



Favorite Quotes:
"This is L.A., sugar. There is no 'over the top." Chris Erskine
"At a certain point the entropy wins." Maria Helena Braga
Current Build: ProFlex 757 Expert full suspension. Yescomusa 36v 800w Rear DD, upgraded 10AWG solid core through axle phase wires. 15ah Headway, 1000+ cycles, 80% DOD 30A Tronsung controller.
Past: Trek 4500 Yescomusa 36v 800w front DD.
Liahona, Yescomusa 36v 800w generic front DD.
1992 Trek 800, Yescomusa 800w 36v front DD.
"This is L.A., sugar. There is no 'over the top." Chris Erskine
"At a certain point the entropy wins." Maria Helena Braga
Current Build: ProFlex 757 Expert full suspension. Yescomusa 36v 800w Rear DD, upgraded 10AWG solid core through axle phase wires. 15ah Headway, 1000+ cycles, 80% DOD 30A Tronsung controller.
Past: Trek 4500 Yescomusa 36v 800w front DD.
Liahona, Yescomusa 36v 800w generic front DD.
1992 Trek 800, Yescomusa 800w 36v front DD.
Re: Does this look like electrical failure?
Thanks guys.
I can't believe how evil some customers can be.
I can't believe how evil some customers can be.
Mush! Mush you electrons! Push harder!
- amberwolf 100 GW
- Posts: 31732
- Joined: Aug 17 2009 6:43am
- Location: Phoenix, AZ, USA, Earth, Sol, Local Bubble, Orion Arm, Milky Way, Local Group
- Contact:
Re: Does this look like electrical failure?
Actually, that looks exactly like assorted cords that Yogi (one of my St Bernards) chewed thru when he first came here. The shearing and tearing is virtually identical to the way his teeth tore thru stuff.
But is most definitely NOT electrical failure.
If that cord had been plugged in to the wall and powered on at the time it was destroyed, it would be melted with plasma burns and spattered copper all over the place, at minimum.
But is most definitely NOT electrical failure.
If that cord had been plugged in to the wall and powered on at the time it was destroyed, it would be melted with plasma burns and spattered copper all over the place, at minimum.
If you found this advice helpful, supporting contributions are accepted here.
"if it ain't broke, improve it till it is"----Dog-Hauler Cargo eTrike SB Cruiser----The HI-Lebowski: a Lebowski SMD brain running a zombified Honda IMA Inverter: a HOW-TO guide----Cargo eBike CrazyBike2----General Blog
"if it ain't broke, improve it till it is"----Dog-Hauler Cargo eTrike SB Cruiser----The HI-Lebowski: a Lebowski SMD brain running a zombified Honda IMA Inverter: a HOW-TO guide----Cargo eBike CrazyBike2----General Blog
Re: Does this look like electrical failure?
You wouldn't believe the elaborate story she concocted with so much detail. Its crazy. I did some research and she has a dog that is an aggressive chewer. That also explains why the paper sticker on the unit had some moisture damage (from dog saliva and cleaning attempt). And indentations from teeth.
Oh and I replaced the wires today and the charger works fine.
Oh and I replaced the wires today and the charger works fine.
Mush! Mush you electrons! Push harder!
Re: Does this look like electrical failure?
Replace the sticker too and its as good as new!veloman wrote: ↑Jun 10 2020 12:37amYou wouldn't believe the elaborate story she concocted with so much detail. Its crazy. I did some research and she has a dog that is an aggressive chewer. That also explains why the paper sticker on the unit had some moisture damage (from dog saliva and cleaning attempt). And indentations from teeth.
Oh and I replaced the wires today and the charger works fine.
Did you sell it via ebay or amazon?
Re: Does this look like electrical failure?
If you have her contact info you should call her and tell her that her dog ate the cord and she needs to bring him to the vet immediately as the flux inside of the wires is toxic and he will die a slow and pain death if she doesn't get him help as soon as possible.
That's not true either and it won't make you whole, but it'll feel good to know she'll be coming out of pocket for that charger one way or another. Payback is a bitch too.
That's not true either and it won't make you whole, but it'll feel good to know she'll be coming out of pocket for that charger one way or another. Payback is a bitch too.
Re: Does this look like electrical failure?
Ebay. Before I looked closely at the wires, I believed her story enough to refund her. Then I realized it was BS. But I asked her to update her negative feedback and she did. I played her game and she won. But I getting ebay involved may not have necessarily gone well for me. I do plan on telling ebay that she is a shady person and make a note of this scam she pulled.markz wrote: ↑Jun 10 2020 2:48amReplace the sticker too and its as good as new!veloman wrote: ↑Jun 10 2020 12:37amYou wouldn't believe the elaborate story she concocted with so much detail. Its crazy. I did some research and she has a dog that is an aggressive chewer. That also explains why the paper sticker on the unit had some moisture damage (from dog saliva and cleaning attempt). And indentations from teeth.
Oh and I replaced the wires today and the charger works fine.
Did you sell it via ebay or amazon?
Mush! Mush you electrons! Push harder!
Re: Does this look like electrical failure?
Yeah but does telling ebay work, do they even care because they get their fee's.veloman wrote: ↑Jun 10 2020 10:19amEbay. Before I looked closely at the wires, I believed her story enough to refund her. Then I realized it was BS. But I asked her to update her negative feedback and she did. I played her game and she won. But I getting ebay involved may not have necessarily gone well for me. I do plan on telling ebay that she is a shady person and make a note of this scam she pulled.
How many items has this person purchased on ebay and whats the buyers rating?
- e-beach 1.21 GW
- Posts: 3788
- Joined: Jan 10 2012 9:48pm
- Location: Any Los Angeles area beach I am at. Or Santa Monica or possibly the south bay beaches.
Re: Does this look like electrical failure?
I sold an guitar amp through eBay once. The customer calmed that it arrived damaged. eBay made me pay for return shipping and refund the guys money. When I got it back, I opened it to see why it didn't work and found the buyer had tried to pull some of the parts out of it and had damaged it that way. (the reverb tank was 1/2 removed.) In any case I reported him to eBay and they said they would watch him. I never heard anything more from it and was never able to sell the damaged amp again.




Favorite Quotes:
"This is L.A., sugar. There is no 'over the top." Chris Erskine
"At a certain point the entropy wins." Maria Helena Braga
Current Build: ProFlex 757 Expert full suspension. Yescomusa 36v 800w Rear DD, upgraded 10AWG solid core through axle phase wires. 15ah Headway, 1000+ cycles, 80% DOD 30A Tronsung controller.
Past: Trek 4500 Yescomusa 36v 800w front DD.
Liahona, Yescomusa 36v 800w generic front DD.
1992 Trek 800, Yescomusa 800w 36v front DD.
"This is L.A., sugar. There is no 'over the top." Chris Erskine
"At a certain point the entropy wins." Maria Helena Braga
Current Build: ProFlex 757 Expert full suspension. Yescomusa 36v 800w Rear DD, upgraded 10AWG solid core through axle phase wires. 15ah Headway, 1000+ cycles, 80% DOD 30A Tronsung controller.
Past: Trek 4500 Yescomusa 36v 800w front DD.
Liahona, Yescomusa 36v 800w generic front DD.
1992 Trek 800, Yescomusa 800w 36v front DD.
- dogman dan 100 GW
- Posts: 35849
- Joined: May 17 2008 12:53pm
- Location: Las Cruces New Mexico USA
Re: Does this look like electrical failure?
I was thinking dog chewed too, but spoke cut also possible.
The evil customer is why a good CS needs to include a price able to support a few to no questions asked warranty.
The evil customer is why a good CS needs to include a price able to support a few to no questions asked warranty.
Frankenbike longtail
http://endless-sphere.com/forums/viewto ... cing+betty.
bolt on longtail https://endless-sphere.com/forums/viewt ... =6&t=74584
The mixte long tail. https://endless-sphere.com/forums/viewt ... =6&t=74384
Beach cruiser converted to long tail. https://endless-sphere.com/forums/viewt ... r#p1045572
http://endless-sphere.com/forums/viewto ... cing+betty.
bolt on longtail https://endless-sphere.com/forums/viewt ... =6&t=74584
The mixte long tail. https://endless-sphere.com/forums/viewt ... =6&t=74384
Beach cruiser converted to long tail. https://endless-sphere.com/forums/viewt ... r#p1045572
Re: Does this look like electrical failure?
You have been defrauded and scammed. The topmost wire in the first and last pictures show several clear indentations which appear to be teeth marks, there is no evidence of melting, scorching, carbon deposits, or excessive heat of any kind.
If this was transported through the US mail, that is mail fraud and a serious Federal offense. Many countries have similar laws.
I would send a strongly worded written document stating your intention to pursue a criminal prosecution involving prison time, which you will forgo provided she submit a complete, signed, witnessed and notarized, description of her willful attempt to defraud, which will be submitted publicly in multiple locations. Any negative comments on your business, by her, will result in immediate instigation of the criminal proceeding, which in most jurisdictions can be done at any time for anywhere from 3 to 7 years from now.
Nail her lying ass to the wall.
Or just lie down, roll over, put your ass in the air and take it.
If this was transported through the US mail, that is mail fraud and a serious Federal offense. Many countries have similar laws.
I would send a strongly worded written document stating your intention to pursue a criminal prosecution involving prison time, which you will forgo provided she submit a complete, signed, witnessed and notarized, description of her willful attempt to defraud, which will be submitted publicly in multiple locations. Any negative comments on your business, by her, will result in immediate instigation of the criminal proceeding, which in most jurisdictions can be done at any time for anywhere from 3 to 7 years from now.
Nail her lying ass to the wall.
Or just lie down, roll over, put your ass in the air and take it.
"Not being treated like a dumb dick is one of the incentives we have to become less stupid." - Balmorhea.
Re: Does this look like electrical failure?
Flux and toxic asbesto's.HK12K wrote: ↑Jun 10 2020 8:39amIf you have her contact info you should call her and tell her that her dog ate the cord and she needs to bring him to the vet immediately as the flux inside of the wires is toxic and he will die a slow and pain death if she doesn't get him help as soon as possible.
That's not true either and it won't make you whole, but it'll feel good to know she'll be coming out of pocket for that charger one way or another. Payback is a bitch too.
- Dauntless 100 GW
- Posts: 10880
- Joined: May 29 2010 1:49am
- Location: Coordinates: 33°52′48″N 117°55′43″W
Re: Does this look like electrical failure?
It'll never work. Not how capitalism works. Funny how the real winners are the scum that are complaining about it. I don't suggest doing anything unless you don't want to sell anything on eBay anymore. Which I've never wanted to do.AngryBob wrote: ↑Jun 12 2020 7:52amIf this was transported through the US mail, that is mail fraud and a serious Federal offense. Many countries have similar laws.
I would send a strongly worded written document stating your intention to pursue a criminal prosecution involving prison time, which you will forgo provided she submit a complete, signed, witnessed and notarized, description of her willful attempt to defraud, which will be submitted publicly in multiple locations. Any negative comments on your business, by her, will result in immediate instigation of the criminal proceeding, which in most jurisdictions can be done at any time for anywhere from 3 to 7 years from now.
Nail her lying ass to the wall.
Last edited by Dauntless on Jun 14 2020 1:33am, edited 1 time in total.
Any sufficiently advanced technology is INDISTINGUISHABLE FROM MAGIC!
- Arthur C. Clarke
- Arthur C. Clarke
Re: Does this look like electrical failure?
eBay is a strange place, and I have close to 5,000 transactions over a 20 year time span, so I know. 99% of the time everything goes well, but sometimes you just can't win. I stopped selling any big ticket photography stuff on there due to their policies, which lean totally toward the buyer. They could claim anything. Keep the item, send you a rock in a box with a tracking number, and claim they returned the item and eBay will debit your seller account for the refund. Don't ask me how I know this. It's easier to just refund their money and block them so they can't buy anything else from me.
Re: Does this look like electrical failure?
I want to prosecute her but yes, I'm more concerned about it affecting my ability to sell on eBay where I've been making some decent money. I've read numerous stories about eBay suspending accounts in similar situations. This criminal has a convincing story with elaborate detail and eBay may not want to risk me selling if they think her story could be true.Dauntless wrote: ↑Jun 13 2020 12:04amIt'll never work. Not how capitalism works. Funny how the real winners are the scum that are complaining about it. I don't suggest doing anything unless you don't want to sell anything on eBay anymore. Which I've never wanted to do.AngryBob wrote: ↑Jun 12 2020 7:52amIf this was transported through the US mail, that is mail fraud and a serious Federal offense. Many countries have similar laws.
I would send a strongly worded written document stating your intention to pursue a criminal prosecution involving prison time, which you will forgo provided she submit a complete, signed, witnessed and notarized, description of her willful attempt to defraud, which will be submitted publicly in multiple locations. Any negative comments on your business, by her, will result in immediate instigation of the criminal proceeding, which in most jurisdictions can be done at any time for anywhere from 3 to 7 years from now.
Nail her lying ass to the wall.
Mush! Mush you electrons! Push harder!
- e-beach 1.21 GW
- Posts: 3788
- Joined: Jan 10 2012 9:48pm
- Location: Any Los Angeles area beach I am at. Or Santa Monica or possibly the south bay beaches.
Re: Does this look like electrical failure?
I have been selling on eBay since June 2001. In all that time I have only had only 2 real bad experiences with buyers. I contacted the eBay dispute resolution center both times and reported them. In one of the cases the buyer gave me a negative feedback and I got eBay to removed it because it was inaccurate. I would contact eBay and report her to the eBay resolution department if for nothing else to help some other eBay seller when she try's it again. If your seller dashboard says your performance is above standard and you have 100% feedback, (or close to it) eBay isn't going to stop you from selling there. (check out evassemble's positive feedback...87% !!!veloman wrote: ↑Jun 14 2020 8:16am
I want to prosecute her but yes, I'm more concerned about it affecting my ability to sell on eBay where I've been making some decent money. I've read numerous stories about eBay suspending accounts in similar situations. This criminal has a convincing story with elaborate detail and eBay may not want to risk me selling if they think her story could be true.




Edit: Also, if the cord you replaced looks as good as new, sell the unit as refurbished for about 90% of a new price so you can keep from loosing all the money on that deal.
Favorite Quotes:
"This is L.A., sugar. There is no 'over the top." Chris Erskine
"At a certain point the entropy wins." Maria Helena Braga
Current Build: ProFlex 757 Expert full suspension. Yescomusa 36v 800w Rear DD, upgraded 10AWG solid core through axle phase wires. 15ah Headway, 1000+ cycles, 80% DOD 30A Tronsung controller.
Past: Trek 4500 Yescomusa 36v 800w front DD.
Liahona, Yescomusa 36v 800w generic front DD.
1992 Trek 800, Yescomusa 800w 36v front DD.
"This is L.A., sugar. There is no 'over the top." Chris Erskine
"At a certain point the entropy wins." Maria Helena Braga
Current Build: ProFlex 757 Expert full suspension. Yescomusa 36v 800w Rear DD, upgraded 10AWG solid core through axle phase wires. 15ah Headway, 1000+ cycles, 80% DOD 30A Tronsung controller.
Past: Trek 4500 Yescomusa 36v 800w front DD.
Liahona, Yescomusa 36v 800w generic front DD.
1992 Trek 800, Yescomusa 800w 36v front DD.
Re: Does this look like electrical failure?
Good advice, thanks guys.
I ended up reporting her to ebay.
I ended up reporting her to ebay.
Mush! Mush you electrons! Push harder!
Re: Does this look like electrical failure?
You use the threat of prosecution to get her letter admitting the truth, then submit that to Ebay.
I once had a competitor arrange to have a ton of cow manure delivered to my front yard. I decided it was necessary for that individual to sincerely and deeply regret his action. He did.
You can just eat it, or you can decide to take action. Five minutes to write the letter. Less than an hour to research jurisdictions and applicable laws, so you can cite them specifically. Much less hassle of this type in the future, and satisfaction that lasts a very long time.
If helps if you have learned how to be mean and nasty, and like to read law books.
If you just want everybody to think you are a nice guy, you are going to get screwed a lot, and not in the good way.
I once had a competitor arrange to have a ton of cow manure delivered to my front yard. I decided it was necessary for that individual to sincerely and deeply regret his action. He did.
You can just eat it, or you can decide to take action. Five minutes to write the letter. Less than an hour to research jurisdictions and applicable laws, so you can cite them specifically. Much less hassle of this type in the future, and satisfaction that lasts a very long time.
If helps if you have learned how to be mean and nasty, and like to read law books.
If you just want everybody to think you are a nice guy, you are going to get screwed a lot, and not in the good way.
"Not being treated like a dumb dick is one of the incentives we have to become less stupid." - Balmorhea.