G'day. I have a 48v 25a LiPO4 battery i use on my ebike. The battery shuts down at around 48v and it should be 45v. The manufacturer (China) has sent me another BMS to suit the battery and i was wondering if someone was able to install the new BMS for me. Any info much appreciated. Cheers. Brian in Melbourne Australia.

User avatar
amberwolf
100 GW
100 GW
Posts: 24215
Joined: Aug 17, 2009 6:43 am
Location: Phoenix, AZ, USA, Earth, Sol, Local Bubble, Orion Arm, Milky Way, Local Group
Contact:

Re: Battery BMS replacement LIPo4

Post by amberwolf » Jan 08, 2018 11:34 pm

Most likely there is nothing wrong with the BMS, and it is just doing it's job: it is probably shutting down the pack to protect against overdischarging a cell (group) that is dropping below LVC under load faster/further than others do.

What are the voltages of the individual cell groups as measured at the sense wires on the BMS? Measure them both without a load, and under load, at the low end of charge (and you can also check them at the high end, but definitely do it at the low end when almost empty).

User avatar
fechter
100 GW
100 GW
Posts: 11979
Joined: Dec 31, 2006 3:23 pm
Location: California Bay Area, USA

Re: Battery BMS replacement LIPo4

Post by fechter » Jan 09, 2018 9:20 am

Right, the BMS doesn't respond to a particular pack voltage, it shuts down when any single cell reaches the low cutoff point, which should be around 2.75v or so. It's possible you have one (or more) cells that are weaker than the others and it's shutting off to protect it.