Re: E-Max 90S questions.

Post by jonescg » Aug 24 2018 3:45am

offpist1 wrote:
Aug 24 2018 12:36am
Maybe you did not read the whole tread, but i have 21S of 50AH Lithium-Ion (3,9KWH nominel), not SLA.
My apologies - was hard to see the whole context on the phone.
21s - must go pretty quickly!

offpist1   10 mW

10 mW
Posts: 26
Joined: Jun 17 2018 3:14am

Re: E-Max 90S questions.

Post by offpist1 » Aug 24 2018 7:38am

Yes, its quick ;)
Pushing 90+ km/h and it gets there very fast.
Quite happy about it.

I also ordered an new rear damper for it, should arrive sometime next week.
Attachments
damper.jpg
damper.jpg (49.89 KiB) Viewed 1295 times

User avatar
jonescg   1.21 GW

1.21 GW
Posts: 3964
Joined: Aug 07 2009 9:22pm
Location: Perth, Western Australia

Re: E-Max 90S questions.

Post by jonescg » Aug 26 2018 6:32am

Any improvement to the suspension is going to be noticeable right away.

offpist1   10 mW

10 mW
Posts: 26
Joined: Jun 17 2018 3:14am

Re: E-Max 90S questions.

Post by offpist1 » Sep 06 2018 10:24am

The rear suspension is now perfect..

This winter i will take apart the front suspention and try to find some softer springs to fit.. the front is way to stiff.
Attachments
20180906_170919_resized.jpg

olalid   1 µW

1 µW
Posts: 3
Joined: Oct 04 2018 8:59am
Location: Sweden

Re: E-Max 90S questions.

Post by olalid » Oct 04 2018 11:30am

Interesting thread, I have an E-Max 90S with a broken motor controller, since it is the same type of epoxy covered design as in the pictures in this thread it is very hard to examine it and try to understand what can be wrong with it.
I have had very little luck in finding any information about the original motor controller on the internet, but the schematic in this thread is very interesting information and should make it easier to replace it with something else.

Did you find out everything you posted in this thread by reverse engineering, or did you find some documentation somewhere?

offpist1   10 mW

10 mW
Posts: 26
Joined: Jun 17 2018 3:14am

Re: E-Max 90S questions.

Post by offpist1 » Oct 04 2018 11:23pm

[Moderation: forsale offer in tech forum deleted]

The schematics for it is attached.
Attachments
Controller user manua- proud-eagle.doc
(463.5 KiB) Downloaded 78 times

olalid   1 µW

1 µW
Posts: 3
Joined: Oct 04 2018 8:59am
Location: Sweden

Re: E-Max 90S questions.

Post by olalid » Oct 08 2018 11:00am

The manual you attached offpist1 mentions an LED code reference table, but it is not included in the document.
My controller does flash some pattern on the LED, so would kind of be interesting to find out what it means, in case the problem is actually external to the controller...
So if anyone knows about those codes, please let me know.

Otherwise, well, for the right price I can perhaps be interested in the original controller, do you have any idea what you want for it?
I was originally thinking I wanted something more robust and potentially better performance, since it seems from what I read that these controllers break quite easily.
But of course just replacing it with an equivalent is a lot easier...

I am not interested in another complete scooter, actually I was not planning on keeping mine either in the long run. :)

whereswally606   100 kW

100 kW
Posts: 1155
Joined: Jun 19 2011 2:11pm
Location: Cheshire, UK

Re: E-Max 90S questions.

Post by whereswally606 » Oct 09 2018 10:53am

from the file in the software manual filename begins E2 - ...
controller led blink codes.png
controller led blink codes.png (53.82 KiB) Viewed 1178 times
hope this helps
Distributing "Lebowski" FOC Controller PCB (Through hole) since 2016
Moped: Emax 110s 2009

olalid   1 µW

1 µW
Posts: 3
Joined: Oct 04 2018 8:59am
Location: Sweden

Re: E-Max 90S questions.

Post by olalid » Oct 11 2018 3:41pm

Great, thanks.

Interesting, mine is blinking 6 times.
Which either is "Scooter disabled", whatever that means (it does say "Vehicle disabled" in the instrument cluster display), or side stand out.
As I remember it when the side stand is out, it displays a message more specifically about that in the display, does it not?

whereswally606   100 kW

100 kW
Posts: 1155
Joined: Jun 19 2011 2:11pm
Location: Cheshire, UK

Re: E-Max 90S questions.

Post by whereswally606 » Oct 12 2018 10:19am

yeah I think you get side stand out message on the display.
Distributing "Lebowski" FOC Controller PCB (Through hole) since 2016
Moped: Emax 110s 2009

squall.eu   1 mW

1 mW
Posts: 10
Joined: Mar 15 2015 5:07am

Re: E-Max 90S questions.

Post by squall.eu » Jun 07 2020 12:02pm

offpist1 wrote:
Aug 01 2018 2:38am
Thanks.
I measured the voltage on the "speed (11)" wire and it gives out 5V.
If i repeatedly short to ground the needle moves up a little. Fastest i can do by hand is moving the needle to 5 km/h.
But at-least I know what kind of signal i need.

I also connected the brake and boost wire from the bike to the controller so now it regenerates even more when brake is applied.
The most i could see is +25A at 84V, so about 2kW.

I also increased the output from the controller from 70% to 80% so now it draws 145A at 86V so about 12KW peak short therm (from the battery). That gives more than enough acceleration, and so far the hub motor does seem to handle it without overheating.
Hi,
would you be able to advise on how have you managed to get brake and boost switches working with Kelly? Old Proud Eagle MCU switches everything to the GND, while Kelly needs +12V switching signal, so they seem incompatible?
Also Kelly KLS-H series have Hall Meter output on PIN8, which connected to PIN 11 on MCU operates the speedometer.