electric motion 5.7. Need new BMS

General Discussion about large electric scooters and motorcycles and other things with no pedals.
Post Reply
offpist1   10 mW

10 mW
Posts: 26
Joined: Jun 17 2018 3:14am

electric motion 5.7. Need new BMS

Post by offpist1 » Sep 29 2018 1:23pm

I bought an second hand Electric Motion 5.7 from really cheap with an broken "battery module".
The previous owner opened the battery and somehow managed to damage the BMS.
Then he contacted electric motion and got an offer for an new battery for 4000 pound.. The BMS can not be sold desperately.
So, then he sold the whole bike to me for 1000 pounds.

I removed the defective BMS and charged the battery by bypassing the BMS and monitoring each cell with an regular volt meter.
Some cells were a little bit off but not more than 0,1V
I did some manual balancing by charging some of the lower cells and discharging some of the higher cells.
Now they are all within 0,03V.

The rest of the bike works perfect. It comes originally with an Kelly Controller KEB 48601.
I own two other bikes with Kelly controllers so i already have some knowledge to that brand, and cable/software.

The motor is 5KW made by Golden Motor and it has an reduction gear box as this is an trail bike.

Battery is 13S, 25 AH.

Now I need an new BMS and it needs to be built in to the battery. I would like to have Bluetooth.
Any recommendations? I am looking at the Speedict Neptune 15.
But i can not let all the power go thru the BMS as this needs 200A power, acutally the fuse to the controller is 300A.
Can the Speedict instead control the large relay allready build in to the battery module?
Last edited by offpist1 on Sep 29 2018 1:52pm, edited 3 times in total.

offpist1   10 mW

10 mW
Posts: 26
Joined: Jun 17 2018 3:14am

Re: electric motion 5.7. Need new BMS

Post by offpist1 » Sep 29 2018 1:33pm

Here is also an picture of the bike.
The battery modules is held together with 30+ rivets that has to be drilled out to open the battery.
I installed M4 rivet nuts instead, making it more easy to access the battery later on.
Attachments
1671252350_20180929_155906_4935731_resized.jpg
-1934531996_20180929_122538_2812692_resized.jpg

User avatar
fechter   100 GW

100 GW
Posts: 15407
Joined: Dec 31 2006 3:23pm
Location: California Bay Area, USA

Re: electric motion 5.7. Need new BMS

Post by fechter » Sep 29 2018 1:57pm

See if you can pull the BMS and get a picture.

Also, see if you can measure the voltages along the connector for the balance wires. You might just have a wire that came loose somewhere.

Does it charge through the BMS OK?
"One test is worth a thousand opinions"

offpist1   10 mW

10 mW
Posts: 26
Joined: Jun 17 2018 3:14am

Re: electric motion 5.7. Need new BMS

Post by offpist1 » Sep 29 2018 2:25pm

I did open the BMS and several component are burned.
The previous owner messed up somehow and connected reverse polarity or something.

And no, the BMS is completely dead will not allow charge or balance.

The connectors from "buttom and upper link" and the RS232 was not in use.
So its very basic, only cell balancing and 7 temp sensors(!), then relay output for charge and discharge.
Plus current sensor (magnetic field type, not shunt).
Attachments
bms.jpg

offpist1   10 mW

10 mW
Posts: 26
Joined: Jun 17 2018 3:14am

Re: electric motion 5.7. Need new BMS

Post by offpist1 » Oct 20 2018 10:37am

New BMS mounted.
I went with the Speedict 15S.

I am also working on building two more batteries.

One will be 37AH using cells from 2018 model E-Golf.
This one will be slightly heavier than the oem one but much better range an also less voltage sag.

The other one i think i will make an light wheight edition. Only 13S6P using LG HG2 18650 cells. This should make it less than 6 kg with relay, casing etc..
Attachments
313324138_20181012_174649_2413092_resized.jpg
Screenshot_20181012-183745_Neptune.jpg
838621623_20181020_114252_1140034_resized.jpg
1641894632_20181020_120326_1286100_resized_5.jpg
1641894632_20181020_120326_1286100_resized_5.jpg (158.3 KiB) Viewed 2511 times

Xtr6   100 W

100 W
Posts: 142
Joined: Jan 17 2015 1:20pm

Re: electric motion 5.7. Need new BMS

Post by Xtr6 » Mar 18 2019 3:25pm

Nice job, was thinking of buying a EM 5.7 but they are too expensive so building a trail bike myself.

pbert   100 mW

100 mW
Posts: 49
Joined: May 08 2019 11:08pm

Re: electric motion 5.7. Need new BMS

Post by pbert » May 10 2019 9:33am

@offpist1, i'm looking to build a battery for the EM 5.7 sport and have been thinking of a 13S5P of Sanyo NCR2070C 20700 3500mAh 30A Battery. 5 in P would do 150A continuous.

i have been looking for a BMS and also arrived at looking at the speedict neptune but saw it says 60 amps max continuous ... ? how is it working out for you or were you able to modify that max amperage ?

also wondering about how to connect the individual cells together. i've build 18650 packs in the past with a maletriks spot welder but layered nickel strips to get sufficient metal thickness for amperage requirement. for this 201700 battery i was thinking of using 10AWG wire between cells that would not be soldered down but rather i would spot weld the nickel strip arouund the wire to make contact with the top of the battery and it would be tight enough that would actually hold the wire in place. i've done it before for the positive nad negative termials of the battery packs.

also if you could tell me what kind of batteries are used in the original EM battery. They are lipo packs of some format i imagine from the pic. thanks.

and one last question, do you think the Kelly controller would allow 52v (14S) pack, or would not work ? or if you know any other reason not to use a 52V instead of the 48V pack.

sorry for the rant ;)

Xtr6   100 W

100 W
Posts: 142
Joined: Jan 17 2015 1:20pm

Re: electric motion 5.7. Need new BMS

Post by Xtr6 » Jun 05 2019 4:14pm

Kelly will go up to 60 Volt, so 15 S is the max.

steve 101   1 µW

1 µW
Posts: 1
Joined: Jul 26 2019 6:35pm

Re: electric motion 5.7. Need new BMS

Post by steve 101 » Jul 26 2019 6:44pm

Hi wondering if you could give an update on the new BMS fitted to your EM 5.7 I've got a EM with a failed BMS so looking for a new one Is the speedict 15 still working fine and is there any tips I need to know when fitting one

Cheers Steve

User avatar
Rut Row   1 mW

1 mW
Posts: 10
Joined: Jul 26 2019 6:10am

Re: electric motion 5.7. Need new BMS

Post by Rut Row » Jul 27 2019 7:00am

steve 101 wrote:
Jul 26 2019 6:44pm
Hi wondering if you could give an update on the new BMS fitted to your EM 5.7 I've got a EM with a failed BMS so looking for a new one Is the speedict 15 still working fine and is there any tips I need to know when fitting one

Cheers Steve
Agree on the update plus would like to have more details. I have a 2016 EM Sport+ (16ah battery) and want a second battery.

Post Reply