Received 150 NCR18650GA cells from Nkon to California USA

A place to list links to sources for EV related parts and services.

Received 150 NCR18650GA cells from Nkon to California USA

Postby bigdeezs » Wed May 10, 2017 2:51 pm

I did alot of research trying to find the GA cells shipped to the US. I looked at fastech but they were going to run about $4.63/cell. I tried Tumich (his thread: viewtopic.php?f=31&t=61608) but he didnt have any GAs anymore. So I took a gamble and ordered through nkon even though I had read they might not be the best for US customers due to shipping issues. I used a capital one credit card directly (not through paypal) so as not to incur and international transaction or currency conversion fees. The 150 cells ended up costing $622.75 USD shipped (580euro) making it $4.15 USD/cell.

Ordered on 4/21/17 received on 5/10/17 via fedex. Not too bad considering I thought it would be about 2 months before I would see them. Paperwork says they were shipped out of Berlin and I had just received tracking info on 5/7/17 (3 days before to receiving them).

They were shipped in a unmarked box with paperwork about Nickel-metal hydride batteries. I imagine this was to get around the lithium shipping issues. All cells shipped at 3.5v.

I've read only positive things about Arjan (from nkon) but I will likely test the cells before building my 24s 6p battery to makes sure capacity is where it should be.

Image
Image
Image
Image
Image
Image
Image
Last edited by bigdeezs on Thu May 11, 2017 5:33 am, edited 1 time in total. View post history.
bigdeezs
10 µW
10 µW
 
Posts: 5
Joined: Sat Jun 25, 2016 7:53 pm

Re: Received 150 NCR18650GA cells from Nkon to California US

Postby teslanv » Wed May 10, 2017 3:04 pm

Nice.
Last edited by teslanv on Thu May 11, 2017 3:55 pm, edited 1 time in total. View post history.
First Build: "Craigslist Hardtail"
Signature Build: "Assault & Battery"
Fastest Drag Bike: "Vector/QS205/Sabvoton"
Current favorite: "Super Deluxe IGH BBS02"
Spoiling my Children with an E-BMX
User avatar
teslanv
100 MW
100 MW
 
Posts: 2764
Joined: Sun Nov 03, 2013 8:42 pm
Location: Bellevue, WA - USA

Re: Received 150 NCR18650GA cells from Nkon to California US

Postby bigdeezs » Thu May 11, 2017 5:32 am

lol...good point...thanks :!:
bigdeezs
10 µW
10 µW
 
Posts: 5
Joined: Sat Jun 25, 2016 7:53 pm


Return to Resources & EV Related Parts and Services

Who is online

Users browsing this forum: No registered users and 1 guest