Received 150 NCR18650GA cells from Nkon to California USA

A place to list links to sources for EV related parts and services.
Post Reply
bigdeezs
10 µW
10 µW
Posts: 6
Joined: Sat Jun 25, 2016 7:53 pm

Received 150 NCR18650GA cells from Nkon to California USA

Post by bigdeezs » Wed May 10, 2017 2:51 pm

I did alot of research trying to find the GA cells shipped to the US. I looked at fastech but they were going to run about $4.63/cell. I tried Tumich (his thread: https://endless-sphere.com/forums/viewt ... 31&t=61608) but he didnt have any GAs anymore. So I took a gamble and ordered through nkon even though I had read they might not be the best for US customers due to shipping issues. I used a capital one credit card directly (not through paypal) so as not to incur and international transaction or currency conversion fees. The 150 cells ended up costing $622.75 USD shipped (580euro) making it $4.15 USD/cell.

Ordered on 4/21/17 received on 5/10/17 via fedex. Not too bad considering I thought it would be about 2 months before I would see them. Paperwork says they were shipped out of Berlin and I had just received tracking info on 5/7/17 (3 days before to receiving them).

They were shipped in a unmarked box with paperwork about Nickel-metal hydride batteries. I imagine this was to get around the lithium shipping issues. All cells shipped at 3.5v.

I've read only positive things about Arjan (from nkon) but I will likely test the cells before building my 24s 6p battery to makes sure capacity is where it should be.

Image
Image
Image
Image
Image
Image
Image
Last edited by bigdeezs on Thu May 11, 2017 5:33 am, edited 1 time in total.

User avatar
teslanv
100 MW
100 MW
Posts: 2809
Joined: Sun Nov 03, 2013 8:42 pm
Location: Bellevue, WA - USA

Re: Received 150 NCR18650GA cells from Nkon to California US

Post by teslanv » Wed May 10, 2017 3:04 pm

Nice.
I build custom ebikes.
http://www.westcoastelectrics.com
West Coast Electric Cycles
Bellevue, WA
USA

bigdeezs
10 µW
10 µW
Posts: 6
Joined: Sat Jun 25, 2016 7:53 pm

Re: Received 150 NCR18650GA cells from Nkon to California US

Post by bigdeezs » Thu May 11, 2017 5:32 am

lol...good point...thanks :!:

bigdeezs
10 µW
10 µW
Posts: 6
Joined: Sat Jun 25, 2016 7:53 pm

Re: Received 150 NCR18650GA cells from Nkon to California US

Post by bigdeezs » Thu Jul 27, 2017 7:47 pm

Tested a cell after cycling it one time. Charged it to 4.2V...then Discharged it at .7A or 700 Milliamps down to 2.5V... and only got 3267 MAH. I believe I had read someone else getting a slightly low reading as well from NKON. Minimum should be 3350. I used a IMAX B6 clone to do the testing so take it for what it's worth. I'll still be using my cells but it's possible they are not top quality cells.

zackclark70
100 W
100 W
Posts: 210
Joined: Fri Feb 21, 2014 4:46 am
Location: My House UK :)

Re: Received 150 NCR18650GA cells from Nkon to California US

Post by zackclark70 » Thu Jul 27, 2017 8:00 pm

bigdeezs wrote:Tested a cell after cycling it one time. Charged it to 4.2V...then Discharged it at .7A or 700 Milliamps down to 2.5V... and only got 3267 MAH. I believe I had read someone else getting a slightly low reading as well from NKON. Minimum should be 3350. I used a IMAX B6 clone to do the testing so take it for what it's worth. I'll still be using my cells but it's possible they are not top quality cells.
warm the battery to 25c and discharge at 0.25C to get the full capacity

timmy66
100 mW
100 mW
Posts: 35
Joined: Tue Jul 12, 2016 1:07 am

Re: Received 150 NCR18650GA cells from Nkon to California US

Post by timmy66 » Thu Oct 05, 2017 12:12 pm

Some cells actually need higher discharge rates to get the rated value, eg, Samsung 25R I think needed 10A discharge to get a higher capacity rating, instead of a simple 1C or less.