Post by Jason27 » Jun 19 2014 7:12am

Honey Badger wrote:AllCell Technology in Chicago makes great batteries. They incorporate a proprietary PCM (phase change material) that absorbs excess heat and allows for higher performance/longer life. I've been using one of their 36v 15Ah packs with a 750 Aotema front direct drive for 3 months with great results. They also warranty their packs for two years. If you're interested, I can refer you to a shop in my neighborhood that is an AllCell dealer/shipper.
Agree 100%. I bought my battery pack from Chicago Electric bikes and it is still running great since 2011. So its almost been 3 years and no difference in performance. The prices are higher, but the quality and service is excellent.

:mrgreen:
My ebike:
Diamondback with WE 800 watt hub motor with AllCell 48V 20AH Lithium Manganese battery pack.

k-harvey   100 W

100 W
Posts: 268
Joined: Aug 05 2011 4:47pm
Location: New Zealand

Battery retailers

Post by k-harvey » Apr 18 2016 9:04pm

I always bought Chinese LiFePo4 batteries other than getting the BMS far too lower wattage then replacing BMS have had good service from ---
BMS battery , Greenbikekit , & battery bikekit . Having trouble at the moment with shipping to our bottom of planet country New Zealand-- are there any other
battery supply people who others can recommend.-----By the way one of my past batteries is near 9 years old as don't ride every day .
Proves LiFePo4 are cheap over the years.

Tats   1 kW

1 kW
Posts: 429
Joined: Apr 17 2014 9:51pm
Location: NOR Perth, worlds best kept secret, Australia

Re: Battery retailers

Post by Tats » Apr 19 2016 7:00am

I had a ping delivered to Perth -> http://www.pingbattery.com/

k-harvey   100 W

100 W
Posts: 268
Joined: Aug 05 2011 4:47pm
Location: New Zealand

Re: Battery retailers

Post by k-harvey » Apr 20 2016 1:35am

We're wanting battery in carrier type pack , seems ping only have the square shrink wrap ones .. Its Definitely better with key operating
turn off as with our type kit there is never a total off until battery disconnected..

User avatar
flangefrog   1 kW

1 kW
Posts: 371
Joined: Jun 26 2013 10:21pm
Location: Auckland, New Zealand

Re: Battery retailers

Post by flangefrog » Apr 20 2016 2:18am

Are you just looking for LiFePO4?

I've been getting 18650 cells from tumich. Sea shipping takes 2-3 months but well worth it and very cheap (both cells and shipping).

k-harvey   100 W

100 W
Posts: 268
Joined: Aug 05 2011 4:47pm
Location: New Zealand

Re: Battery retailers

Post by k-harvey » Apr 24 2016 1:44am

looks like i'l have to buy ebay but have to add 15% tax as price marked at real price . They can be risky with as bms can be to low a amps .
i think this motor is about 300w.(36v)Usualy am buying for 500 & 24v & this is big amp for most 24v (have replaced a fair few BMS's)

k-harvey   100 W

100 W
Posts: 268
Joined: Aug 05 2011 4:47pm
Location: New Zealand

Re: Battery retailers

Post by k-harvey » Apr 25 2016 10:57am

thank you eva-macheal
thanks for the good information .
I just bought one on Ebay hope it gets to us have tax yet on it to pay etc I've built up the cells & BMS with the large screw headway ones AH does never seem to be as each cell is claimed & Ihave had problems as with the way I made the pack.Also i wish one could buy a key operated high amp switch for simple connection .
As an electrical guy said to me once -kev your'e playn round with nothing ya know about. Don't make a dime at what i do but if it werent for these batteries I'd not be biking I'd propably have a muss'el vintage pony. (car)

Ron Paul's Blimp   10 W

10 W
Posts: 85
Joined: Jun 12 2017 3:17am

Re: Battery Packs - Where to buy them

Post by Ron Paul's Blimp » Jun 27 2017 2:06pm

Where can I get a 14s2p 18650 pack? I ordered the one Luna sells, but they seem unable to ship it and I'd like to find a more reliable source for future orders. Is there a vendor that will make a custom pack like that for me?

ndondo   1 µW

1 µW
Posts: 1
Joined: Aug 29 2016 4:41pm

Re: Battery Packs - Where to buy them

Post by ndondo » Aug 02 2017 11:14pm

I was running 3 SLA battery I got about 300 km out of it , and now I learned my lesson, since the SLA battery now dead not even 5 months in.

If I want to go with the cheapest option that is not SLA,

is LIPO from hobby king will be the best choice. price wise. please Keep in mind I need a battery and charger combo.

I have a pretty good knowledge on how to wire lipo battery to get the voltage I need. (may need a little bit of guide as I never done it for bike, I did it for hobby RC Car )

But I am clueless as to how to charge it , ideally I want to charge them properly but not too cumbersome as to having multiple charger for each battery. as long as the charge setup only use one AC 110V outlet.. it would be great.

or is there general consensus among forum members as to where to get battery online source that gets me battery and charger combo and at a good price too.,


spec of the battery I need is 36v (anything less than 10Ah and above 4Ah will do) and a charger,..


thank you

Speedtospare   1 mW

1 mW
Posts: 11
Joined: Apr 29 2010 10:11pm

Re: Battery Packs - Where to buy them

Post by Speedtospare » Dec 16 2017 10:07am

Use a lipo BMS

User avatar
Chalo   100 GW

100 GW
Posts: 8354
Joined: Apr 29 2009 11:29pm
Location: Austin, Texas

Re: Battery Packs - Where to buy them

Post by Chalo » Dec 18 2017 1:53am

No, good God just get a bottle battery and let it do the battery management.
This is to express my gratitude to Justin of Grin Technologies for his extraordinary measures to save this forum for the benefit of all.

avoleoo   10 W

10 W
Posts: 85
Joined: Feb 12 2014 4:44pm
Location: West Palm Beach, FL

Re: Battery Packs - Where to buy them

Post by avoleoo » Jan 10 2018 12:13pm

Anyone can tell me if it's possible to buy a good cells for let's say $2/pcs?

IssacZachary   1 µW

1 µW
Posts: 2
Joined: Mar 07 2018 2:16pm

Re: Battery Packs - Where to buy them

Post by IssacZachary » Mar 08 2018 3:20pm

Hi all! Any idea of where would be the best place to buy new 18650's in bulk. Planning on a 30 to 60kWh project.

Thanks!

Rideon   10 mW

10 mW
Posts: 24
Joined: Aug 15 2018 4:58pm

Re: Battery Packs - Where to buy them

Post by Rideon » Aug 20 2018 3:43pm

Hi everyone,

Could anyone share a reliable source to buy LiFePo4 battery ... Thanks

Ribfeast   1 W

1 W
Posts: 50
Joined: Oct 07 2018 11:26pm

Re: Battery Packs - Where to buy them

Post by Ribfeast » Oct 07 2018 11:47pm

Ditto, for larger packs, eg 200Ah 48V. In Australia or that will ship to Australia affordably :)

User avatar
jonescg   1.21 GW

1.21 GW
Posts: 3931
Joined: Aug 07 2009 9:22pm
Location: Perth, Western Australia

Re: Battery Packs - Where to buy them

Post by jonescg » Oct 10 2018 11:03pm

Ribfeast wrote:
Oct 07 2018 11:47pm
Ditto, for larger packs, eg 200Ah 48V. In Australia or that will ship to Australia affordably :)
How much do you want to spend? If you're happy with LiFePO4 I'd suggest EV-Power in WA, otherwise I can build you a battery with more amps than most motors can handle.

Ribfeast   1 W

1 W
Posts: 50
Joined: Oct 07 2018 11:26pm

Re: Battery Packs - Where to buy them

Post by Ribfeast » Oct 11 2018 6:14pm

$2-3k incl BMS I'd say, otherwise it doesn't make it cost effective to switch from FLA batts. At that price I'm probably dreaming though. As long as it can handle a peak current of 355A @ 48V then it should be adequate.

I was toying with getting a set of CALB CA180 cells from here and then obtaining a suitable BMS:
https://www.evworks.com.au/calb-ca180

This company doesn't seem to have any pricing on their page but has all the right gear, I've sent an e-mail:
https://www.ev-power.com.au/product/gbs ... -2v-cells/

User avatar
jonescg   1.21 GW

1.21 GW
Posts: 3931
Joined: Aug 07 2009 9:22pm
Location: Perth, Western Australia

Re: Battery Packs - Where to buy them

Post by jonescg » Oct 11 2018 7:25pm

Rods pricing is pretty similar to EV Works, maybe a little more expensive (by like 5% or so). He's pretty good on follow up too.
I can certainly build a battery that will do what you want but it will be about three times your budget - cells aren't cheap for little guys.

I will be bringing some large prismatic NMC cells in next month. If you wanted to get on board with that order you're welcome. They are 100 Ah cells going for about $143 each landed. So that's about $4000 in cells, without a BMS.

Ribfeast   1 W

1 W
Posts: 50
Joined: Oct 07 2018 11:26pm

Re: Battery Packs - Where to buy them

Post by Ribfeast » Oct 11 2018 8:58pm

If the 100Ah cells will hold that kind of current draw then I might be interested, I'd need around 15-16 of them to make 51V.
What would a suitable BMS be worth? With the ability to shut off supply to the battery pack if voltage any any individual cell fell or rose above a safe level?
Worst case when the golf cart gets retired I'll move the pack to the server room, hook it up to the solar array and make the rack partially off-grid.

User avatar
amberwolf   100 GW

100 GW
Posts: 31716
Joined: Aug 17 2009 6:43am
Location: Phoenix, AZ, USA, Earth, Sol, Local Bubble, Orion Arm, Milky Way, Local Group
Contact:

Re: Battery Packs - Where to buy them

Post by amberwolf » Oct 11 2018 9:07pm

Ribfeast wrote:
Oct 11 2018 8:58pm
If the 100Ah cells will hold that kind of current draw then I might be interested, I'd need around 15-16 of them to make 51V.
If you mean 51v fully charged, then with NMC you only need 13s, and would only charge them to 3.92v each (instead of 4.1-4.15v).

If you mean a typical "52v" pack, then it'd be 14s, and it'd end up 58v fully charged, for 4.14v/cell.


If you were using LiFePO4, then you'd use 16s for 58v fully charged, which would typically quickly drop off to 52v or so during use.


FWIW, my 20Ah EIG NMC cells are rated for 100A continuous, so I expect a good 100Ah cell could do 500A continuous.

Ribfeast   1 W

1 W
Posts: 50
Joined: Oct 07 2018 11:26pm

Re: Battery Packs - Where to buy them

Post by Ribfeast » Oct 11 2018 9:20pm

I was leaning towards LFP batteries preferably for safety, capacity is not a massive issue as long as it is at least 100Ah.
It would need to be a suitable voltage replacement for the current 48V (8x 6V) lead acid pack.

https://www.lfp.net.au/product-page/3-2 ... calb-ca100
According to this they can do 300A, and in my case they would only be doing that briefly when I stab the accelerator to move from standstrill, and maybe a bit when going up a small hill.

If the EIG NMC cells are cost effective they might be a good alternative though, especially with that extra current capacity :)
What are they worth?

User avatar
jonescg   1.21 GW

1.21 GW
Posts: 3931
Joined: Aug 07 2009 9:22pm
Location: Perth, Western Australia

Re: Battery Packs - Where to buy them

Post by jonescg » Oct 12 2018 1:58am

EIG weren't known for being cheap.

What is the application? E-moto? E-Scooter? E-car?

A 100 Ah LiFePO4 cell will be okay with 100 A for several minutes, but they sag pretty bad under heavy load. If 350 A is your target peak current they will be OK, but 200 Ah would be safer.

The pouch cells I use are good for 30 C continuous - so 350 A from a 100 Ah pack is child's play. At 14s (nominal 48 volts) that's only 5.1 kWh and about $6000 without a BMS.

But if you're after a safe battery and weight/space aren't critical, 180 Ah CALB cells are the way to go.

Ribfeast   1 W

1 W
Posts: 50
Joined: Oct 07 2018 11:26pm

Re: Battery Packs - Where to buy them

Post by Ribfeast » Oct 14 2018 4:55pm

It's for this one:
viewtopic.php?f=34&t=96717&p=1417763#p1417763
Toro Workman MDE.
It currently has a pack of 8 6V T105 lead acid batteries, two are faulty. I've popped in some "new" replacements over the weekend but these had been sitting for a year on a concrete floor without a charge and had 5.5V when I tested them. Gave them a good charge over the weekend and they seem to have held it, but I reckon they have reduced capacity.
Just trying to find a way to convert this cart to lithium for under $3k if possible.

Hillhater   100 GW

100 GW
Posts: 11415
Joined: Aug 03 2010 10:33pm
Location: Sydney ..(Hilly part !) .. Australia/ Down under !

Re: Battery Packs - Where to buy them

Post by Hillhater » Oct 14 2018 5:42pm

Ribfeast,.. Where are you based ?
Several other aussie members have been through this similar situation already and could be useful contacts for you.
Swapping to salvaged GM Volt cells (imported ?). seems to be the preferred cost/benifit result,
..Though jones'es EIG cells are very tempting for performance !.
Read this thread from Galderdi (Brisbane based)..
viewtopic.php?f=34&t=76189&start=25
.. Battery discussion seems to start on the 2nd page..
Note also input from Kwiev (Jindabine) who did a similar swap on his buggy.
I believe both bought imported cells ,..so its not too difficult.
Use the "pm contact" function to talk to them off line if you prefer.
This forum owes its existence to Justin of ebikes.ca

Ribfeast   1 W

1 W
Posts: 50
Joined: Oct 07 2018 11:26pm

Re: Battery Packs - Where to buy them

Post by Ribfeast » Oct 14 2018 7:58pm

I'm based in the Newcastle NSW area. Happy to have a crack at importing some, or going in on a group buy, but I'll need to make sure all the protective measures are in place too. BMS, "fuel gauge", suitable charger etc. Lots of research ahead of me and thread skimming :)