BATTERIES: 7 Nissan Leaf battery modules (7.8V each) connected in series for 54V nominal (approximately 58 amp hours). The picture of the go kart frame shows the proposed placement of the battery modules (4 on one side and 3 on the other side).

BATTERY MANAGEMENT SYSTEM (BMS): Orion Jr. BMS with pre-wired CANBUS harness, voltage tap harness, shunt resistor (500A) and basic analog display

MOTOR: Motenergy ME0708 Permanent Magnet Direct Current (DC) Motor, 48V, 8 hp cont, 15 hp pk (300 amps max/150 amps continuous)

CONTROLLER: Alltrax SR-48300 48V/300A. The charge controller would go in front of the driver (under the steering wheel).

WIRING: 4 AWG gauge wire to/from charge controller, motor, and battery pack

THROTTLE: EZ-GO Pot Box

CONTACTOR:
Gigavac GV200QA-1 48V 500 Amp

Stay tuned for more updates.

The VenomKarts Team
VenomKarts, LLC

999zip999   100 GW

100 GW
Posts: 9966
Joined: Jan 10 2010 1:40pm
Location: Dana Point So. Cal

Re: Want to buy a custom made go kart?

Post by 999zip999 » Mar 23 2019 4:55am

Nice. If it ante rubbing it ain't racing !
Free test ride. Love it.

garolittle   1 kW

1 kW
Posts: 453
Joined: Mar 03 2018 1:06pm
Location: Augusta, GA U.S.A
Contact:

Re: Want to buy a custom made go kart?

Post by garolittle » Mar 23 2019 8:46am

999zip999 wrote:
Mar 23 2019 4:55am
Nice. If it ante rubbing it ain't racing !
Free test ride. Love it.
Thanks. Many updates since I posted this. The production version will have a much more powerful motor/controller. 48V AC-9 with 600A Curtis controller. Kart will also include a small roll bar to improve safety. Thrills are free. VenomKarts.com