at the moment i have a 7P13S battery consisting of 91 LG MG1 and after only about 170 cycles it lost already about 40%. I tested it multiple times and its quite disappointing. My setup looks like following:

Charge overnight with about 3A or 0,3C.
Commuting to work and back, each way is about 35-40mins, with a about 0,75C or 15A.
Then i recharge again, with about 10% Capacity untouched.
Temperature is between 12°C and 23°C
With this scenario battey is toast after only 170 cycles.

I want a battery that lasts as long as possible, something like 10 years.
What kind of cell do you recommend? Sanyo GA, Panasonic PF (too old?) or Samsung 50E looked promising concerning cycle life.

john61ct   100 GW

100 GW
Posts: 5634
Joined: Dec 18 2018 2:06pm

Re: Which cell for long lasting battery

Post by john61ct » Jun 10 2019 10:15am

If you can carry about 30%? more weight per Ah

LFP is around 220 Wh/L (790 kJ/L), 120 Wh/kg vs LCO 150-190 ?

At a .75C discharge rate, and ideally stopping at 15% SoC rather than 10%

you should IMO get 4000+ cycles

The larger size prismatics - CALB, GBS, Winston, Sinopoly let you build a larger pack with only one or two strings, 180Ah is considered a medium cell size.

A123 pouches are more difficult to DIY but also great quality.

Note the charge V is 3.5-3.6 rather than 4.1-4.2Vpc.

_____
LTO is the new hotness, over 10000 cycles claimed, but crazy low charge voltage, not sure about energy density.

DrKraut   1 W

1 W
Posts: 64
Joined: Jun 29 2013 12:00pm
Location: alemania

Re: Which cell for long lasting battery

Post by DrKraut » Jun 10 2019 10:21am

I tought that too at my first design phase for the battery. But I'm limited to the triangle size of my bike. Which just fits about 91 cells plus the controller. So i have to stay high energy density cells, since I can't charge at work.

User avatar
Easy_Rider   1 mW

1 mW
Posts: 18
Joined: Mar 04 2018 11:34am

Re: Which cell for long lasting battery

Post by Easy_Rider » Jun 10 2019 12:29pm

Are your battery cells assembled into plastic cavities, or just connected to eachother with glue?
Do you know, with which materail the cells are welded to eachother? Pure Nickel, or Hilumin?
I love riding a bike, but I love the most riding my eBike

User avatar
spinningmagnets   100 GW

100 GW
Posts: 11673
Joined: Dec 21 2007 10:27pm
Location: Ft Riley, NE Kansas

Re: Which cell for long lasting battery

Post by spinningmagnets » Jun 10 2019 12:42pm

For some reason, the factory specs on cells continue to list 4.2V as the max charge per cell. Although lithium cells will work at 4.2V per cell, their life can be roughly doubled if you only charge to 4.1V per cell..and 4.0V is even better (going down to 3.9V per cell provides no benefit).

It is useful to charge to the full amount once a month or so, to ensure that the BMS will balance all of the cells. However, I continue to be shocked that nobody is making a BMS that will balance the cells at 4.1V...

I guess if I would order 1,000 units and pay cash up front, China will make whatever I want, but...if the majority of your profits come from selling battery packs, why would they sell a pack (and charger) that lasts longer? They WANT your pack to die soon.

DrKraut   1 W

1 W
Posts: 64
Joined: Jun 29 2013 12:00pm
Location: alemania

Re: Which cell for long lasting battery

Post by DrKraut » Jun 10 2019 1:41pm

I just found something interesting while digging around:

Its about the Sammy 35E cell but anyway really suspicious or strange:

From this datasheethttp://downloads.cdn.re-in.de/1400000-1 ... AH_10A.pdf
Thats the cycle life stats:
inr18650-35E cycle life per.png
So you can see its about 80% after 500 cycles, while noting the charging/discharging conditions.

Next datasheet:https://akkuzentrum.de/media/datasheets ... g__35E.pdf
Thats what it tells us now:
inr18650-35E cycle life-60p.png
inr18650-35E cycle life-60p.png (22.04 KiB) Viewed 3063 times
So somehow they reduced the cycle life from 80% to 60% with the same conditions, if I'm not mistaken :confused:

What do you guys say to something like that? :idea:

User avatar
pwd   1 kW

1 kW
Posts: 384
Joined: Oct 11 2011 12:01pm
Location: Ontario, Canada

Re: Which cell for long lasting battery

Post by pwd » Jun 10 2019 1:57pm

spinningmagnets wrote:
Jun 10 2019 12:42pm
It is useful to charge to the full amount once a month or so, to ensure that the BMS will balance all of the cells. However, I continue to be shocked that nobody is making a BMS that will balance the cells at 4.1V...
Someone correct me if I am wrong but I believe since em3ev has been using a smart BMS; their packs will balance from as low as 4.0V.
Commuter/Street Build viewtopic.php?f=6&t=98286:
Rocky Mountain Element
Magic Pie 4 front + Leafmotor 1500 rear w/ WCEC 18fet
Samsung 40T 14S7P

Offroad Build viewtopic.php?f=6&t=102195:
2019 Rocky Mountain Blizzard 20
Cyclone "3kw" 13T motor to 36T chain ring then 32T chain ring to 11T-46T Cassette
em3ev 14S5P 30Q or 14S6P 25R pack

john61ct   100 GW

100 GW
Posts: 5634
Joined: Dec 18 2018 2:06pm

Re: Which cell for long lasting battery

Post by john61ct » Jun 10 2019 5:35pm


spinningmagnets wrote: nobody is making a BMS that will balance the cells at 4.1V...
Wut?

I thought there were dozens of BMS that allow user-custom setpoints? Maybe only in LFP land? Only ones costing more? I dunno. . .

Of course, no need to rely on the BMS to balance anyway, plenty of units dedicated to balancing, do not do so at piddly sub - amp rates either.

Or use a hobby charger.

I see balancing as a regular maintenance thing, depending on the use case once a year can be more frequent than necessary.

Of course monitoring things more frequently is required, especially as the bank ages.


john61ct   100 GW

100 GW
Posts: 5634
Joined: Dec 18 2018 2:06pm

Re: Which cell for long lasting battery

Post by john61ct » Jun 10 2019 5:42pm

DrKraut wrote:I just found something interesting while digging around:

Its about the Sammy 35E cell but anyway really suspicious or strange:

From this datasheethttp://downloads.cdn.re-in.de/1400000-1 ... AH_10A.pdf
Thats the cycle life stats:
inr18650-35E cycle life per.png
So you can see its about 80% after 500 cycles, while noting the charging/discharging conditions.

Next datasheet:https://akkuzentrum.de/media/datasheets ... g__35E.pdf
Thats what it tells us now:
inr18650-35E cycle life-60p.png
So somehow they reduced the cycle life from 80% to 60% with the same conditions, if I'm not mistaken :confused:

What do you guys say to something like that? :idea:
Not same termination profile.

Each factory run differs.

Each lab test run will differ.

Point is no on should be using this data to set their own usage patterns in real life.

Don't charge that fast, Do not use that high a V setpoint. Do not hold CV that long. Do not discharge that low.

User avatar
e-beach   1 GW

1 GW
Posts: 3364
Joined: Jan 10 2012 9:48pm
Location: Any Los Angeles area beach I am at. Or Santa Monica or possibly the south bay beaches.

Re: Which cell for long lasting battery

Post by e-beach » Jun 10 2019 6:13pm

Been running Headway 40152S 15Ah LiFePO4 for 6 1/2 years. Over 800 cycles of daily use. They are at 80% of original capacity but sag really bad now. 10 years is probably out of reach for today's 18650's. LTO might do it for you, but it hasn't been used enough around here enough to know for sure. It is also big and heavy. But all the other numbers on it look great.

:D :bolt:
Favorite Quotes:
"This is L.A., sugar. There is no 'over the top." Chris Erskine
"At a certain point the entropy wins." Maria Helena Braga

Current Build: ProFlex 757 Expert full suspension. Yescomusa 36v 800w Rear DD, upgraded 10AWG solid core through axle phase wires. 15ah Headway, 1000+ cycles, 80% DOD 30A Tronsung controller.

Past: Trek 4500 Yescomusa 36v 800w front DD.
Liahona, Yescomusa 36v 800w generic front DD.
1992 Trek 800, Yescomusa 800w 36v front DD.

User avatar
spinningmagnets   100 GW

100 GW
Posts: 11673
Joined: Dec 21 2007 10:27pm
Location: Ft Riley, NE Kansas

Re: Which cell for long lasting battery

Post by spinningmagnets » Jun 10 2019 7:39pm

Its been a while since I researched the termination voltage where the BMS performs the balancing. I know cell-balancing can be done at 4.0V-4.1V with RC chargers on a pack with no BMS.

john61ct   100 GW

100 GW
Posts: 5634
Joined: Dec 18 2018 2:06pm

Re: Which cell for long lasting battery

Post by john61ct » Jun 10 2019 8:06pm

I've looked at spec sheets for hundreds of BMS, and have yet to see a fixed-settings one where the "start-balance V" wasn't higher than where I'd want my bank to sit for the length of time it would take for the too-puny mA "balance-current rate" to do much of anything.

docware   1 kW

1 kW
Posts: 317
Joined: Sep 16 2018 5:36am

Re: Which cell for long lasting battery

Post by docware » Jun 11 2019 12:22am

DrKraut wrote:
Jun 10 2019 7:43am
Hey guys,

at the moment i have a 7P13S battery consisting of 91 LG MG1 and after only about 170 cycles it lost already about 40%. I tested it multiple times and its quite disappointing.
A) Can you please describe in details how did you measure battery capacity at the beginning and after 170 cycles ?

B) Where did you buy the cells ?

Pajda   1 kW

1 kW
Posts: 351
Joined: Jan 24 2016 3:45am
Location: Czech Republic

Re: Which cell for long lasting battery

Post by Pajda » Jun 11 2019 5:58am

DrKraut wrote:
Jun 10 2019 7:43am
Hey guys,

at the moment i have a 7P13S battery consisting of 91 LG MG1 and after only about 170 cycles it lost already about 40%. I tested it multiple times and its quite disappointing. My setup looks like following:

Charge overnight with about 3A or 0,3C.
Commuting to work and back, each way is about 35-40mins, with a about 0,75C or 15A.
Then i recharge again, with about 10% Capacity untouched.
Temperature is between 12°C and 23°C
With this scenario battey is toast after only 170 cycles.

I want a battery that lasts as long as possible, something like 10 years.
What kind of cell do you recommend? Sanyo GA, Panasonic PF (too old?) or Samsung 50E looked promising concerning cycle life.
Hi,

Thanks for detailed destription of your experience with LG MG1 based battery. I can just say that the MG1 cells performs in your application exactly as I expected and it confirms my laboratory cycle life tests of this particular LG chem cell. LG MG1 is my personal favourite for the most shitty cell ever made by LG chem. :( It was some time ago replaced by the LG M29 cells which I hope will perform much better as It is expected from the LG chem production line.

Under my standard test procedure 0.5C charge 1C discharge, 100% DoD the results for MG1 are:
100 cycle: 90% of nominal capacity
200 cycle: 82% of nominal capacity
300 cycle: 70% of nominal capacity
few cycles after 300 and the cell is dead.

For brief comparison:
all LG MH1, MJ1 and M36 are after 1000!!! cycles under the same conditions still at ca 86% of their nominal capacity.

DrKraut   1 W

1 W
Posts: 64
Joined: Jun 29 2013 12:00pm
Location: alemania

Re: Which cell for long lasting battery

Post by DrKraut » Jun 12 2019 2:57pm

john61ct wrote:
Jun 10 2019 5:42pm
Not same termination profile.

Each factory run differs.

Each lab test run will differ.

Point is no on should be using this data to set their own usage patterns in real life.

Don't charge that fast, Do not use that high a V setpoint. Do not hold CV that long. Do not discharge that low.
What do you mean with termination profile?
I think you should be able to trust a manufacturers datasheet, right?

DrKraut   1 W

1 W
Posts: 64
Joined: Jun 29 2013 12:00pm
Location: alemania

Re: Which cell for long lasting battery

Post by DrKraut » Jun 12 2019 3:10pm

docware wrote:
Jun 11 2019 12:22am
DrKraut wrote:
Jun 10 2019 7:43am
A) Can you please describe in details how did you measure battery capacity at the beginning and after 170 cycles ?

B) Where did you buy the cells ?
A rough measure always was that I could ride to work, which are 52km total and another 15km until it was empty. As time passed I could barely go to work, so I had to reduce the speed on my way home. And it's getting worse and worse.
First measurements took place with a resistive load and a hobby grade coulomb meter. Same now. So the inaccuracy might be high, but they are the same all the time.

Cycles are pretty easy. The bike is almost purely used for commuting. Which are 52km, my odometer is just shy of 9000km. After every day I recharge the bike overnight. That gives me ~170 cycles, which are not even 100%DoD cycles!

DrKraut   1 W

1 W
Posts: 64
Joined: Jun 29 2013 12:00pm
Location: alemania

Re: Which cell for long lasting battery

Post by DrKraut » Jun 12 2019 3:18pm

Pajda wrote:
Jun 11 2019 5:58am
DrKraut wrote:
Jun 10 2019 7:43am
Hi,

Thanks for detailed destription of your experience with LG MG1 based battery. I can just say that the MG1 cells performs in your application exactly as I expected and it confirms my laboratory cycle life tests of this particular LG chem cell. LG MG1 is my personal favourite for the most shitty cell ever made by LG chem. :( It was some time ago replaced by the LG M29 cells which I hope will perform much better as It is expected from the LG chem production line.

Under my standard test procedure 0.5C charge 1C discharge, 100% DoD the results for MG1 are:
100 cycle: 90% of nominal capacity
200 cycle: 82% of nominal capacity
300 cycle: 70% of nominal capacity
few cycles after 300 and the cell is dead.

For brief comparison:
all LG MH1, MJ1 and M36 are after 1000!!! cycles under the same conditions still at ca 86% of their nominal capacity.
Thanks for the info! Can you specify your charge and discharge method, like Voltage, waiting time and so on.
What cell would you recommend to me, it doesn't need to be super high energy. I'm only concerned about longevity under relatively mild conditions. I think about the Sanyo GA or Sam. 35E, or is the Panasonic PF still any good?

DrKraut   1 W

1 W
Posts: 64
Joined: Jun 29 2013 12:00pm
Location: alemania

Re: Which cell for long lasting battery

Post by DrKraut » Jun 12 2019 3:19pm

e-beach wrote:
Jun 10 2019 6:13pm
Been running Headway 40152S 15Ah LiFePO4 for 6 1/2 years. Over 800 cycles of daily use. They are at 80% of original capacity but sag really bad now. 10 years is probably out of reach for today's 18650's. LTO might do it for you, but it hasn't been used enough around here enough to know for sure. It is also big and heavy. But all the other numbers on it look great.

:D :bolt:
Thanks for the input, I still have some headways laying around! But there to heavy for me :mrgreen:

john61ct   100 GW

100 GW
Posts: 5634
Joined: Dec 18 2018 2:06pm

Re: Which cell for long lasting battery

Post by john61ct » Jun 12 2019 6:25pm


DrKraut wrote:
john61ct wrote:
Jun 10 2019 5:42pm
Not same termination profile.

Each factory run differs.

Each lab test run will differ.

Point is no on should be using this data to set their own usage patterns in real life.

Don't charge that fast, Do not use that high a V setpoint. Do not hold CV that long. Do not discharge that low.
What do you mean with termination profile?
The formula for when charging is stopped.

C-rate is a critical factor, that changes the voltage setpoint if doing "charge to" CC-only.

If adding CV time, holding absorb, then the tapering amps setpoint determines how close to theoretical maximum capacity you push to.

Which is harmful if used in normal daily cycling.

> I think you should be able to trust a manufacturers datasheet, right?

Those numbers are "do not allow your bank to get near", not what you should actually use if you value longevity.


999zip999   100 GW

100 GW
Posts: 9519
Joined: Jan 10 2010 1:40pm
Location: Dana Point So. Cal

Re: Which cell for long lasting battery

Post by 999zip999 » Jun 12 2019 7:44pm

170 cycles over how many years ?

Dak77   100 W

100 W
Posts: 112
Joined: May 24 2019 11:57pm

Re: Which cell for long lasting battery

Post by Dak77 » Jun 12 2019 9:54pm

Pajda wrote:
Jun 11 2019 5:58am
DrKraut wrote:
Jun 10 2019 7:43am
Hey guys,

at the moment i have a 7P13S battery consisting of 91 LG MG1 and after only about 170 cycles it lost already about 40%. I tested it multiple times and its quite disappointing. My setup looks like following:

Charge overnight with about 3A or 0,3C.
Commuting to work and back, each way is about 35-40mins, with a about 0,75C or 15A.
Then i recharge again, with about 10% Capacity untouched.
Temperature is between 12°C and 23°C
With this scenario battey is toast after only 170 cycles.

I want a battery that lasts as long as possible, something like 10 years.
What kind of cell do you recommend? Sanyo GA, Panasonic PF (too old?) or Samsung 50E looked promising concerning cycle life.
Hi,

Thanks for detailed destription of your experience with LG MG1 based battery. I can just say that the MG1 cells performs in your application exactly as I expected and it confirms my laboratory cycle life tests of this particular LG chem cell. LG MG1 is my personal favourite for the most shitty cell ever made by LG chem. :( It was some time ago replaced by the LG M29 cells which I hope will perform much better as It is expected from the LG chem production line.

Under my standard test procedure 0.5C charge 1C discharge, 100% DoD the results for MG1 are:
100 cycle: 90% of nominal capacity
200 cycle: 82% of nominal capacity
300 cycle: 70% of nominal capacity
few cycles after 300 and the cell is dead.

For brief comparison:
all LG MH1, MJ1 and M36 are after 1000!!! cycles under the same conditions still at ca 86% of their nominal capacity.
Is HG2 in that 1000cycle club?

docware   1 kW

1 kW
Posts: 317
Joined: Sep 16 2018 5:36am

Re: Which cell for long lasting battery

Post by docware » Jun 13 2019 12:52am

Well, again, where did you buy the cells ?

Let´s assume the cells are from trustfull source:

Quick 40% loss after 170 cycles indicates that something in the conditions is not relatively mild. Despite of probably not optimal cells like MG1 (I trust to Pajda´s measurement).

Something is wrong about handling with the battery. So discovery what is it is of the upmost importance.

Cells sitting on 4,2 V during night is not OK, you can use timer to have cells charged just 15 – 20 minutes before your departure.

Operating in the temperature about 12 °C means increased stress to cells. You probably were running the battery during this winter. That means much lower temperature then 12 °C.
By the way, what is ambient temperature during charging ?

What is charging current, 3 A or 0,3 C (= 6A) ?
What is battery voltage after charging ?

26 km in 35 – 40 minutes means speed 39 – 45 km/h. Average current is probably somewhere between 9 – 12 A, not 15 A. From your description I understand that you are using the whole range 4,2 - 3 V.
You probably pedal, not using throttle only. Is it flat terrain ? What is total weight (bike, rider, load).
What motor do you have ? What is max current of the control unit ? How many months is battery in the usage ?
Measuring the battery capacity at the start means that you are not novice.
We can assume that your measurement have some inaccuracy, just don´t know how large.

User avatar
Dui, ni shuo de dui   1 kW

1 kW
Posts: 441
Joined: Jan 29 2016 3:21am

Re: Which cell for long lasting battery

Post by Dui, ni shuo de dui » Jun 13 2019 5:04am

It seems to me like you didn't really test each cell, did you?
Are you sure that there is not one weak paralleled group?

Could be that you just got one or a few bad cells and that the rest is fine, so the BMS shuts down/indicates a low SOC because of these while the rest is still fine.
:bolt: :bolt: My electric Ninja 250 clone: 16 000W 72V40Ah A123 cells : :bolt: :bolt:
https://endless-sphere.com/forums/viewt ... 12&t=90032

:bolt: :bolt: My electric Scooter: 11 000W 72V 50Ah LiFePO4 cells: :bolt: :bolt:
https://endless-sphere.com/forums/viewt ... 12&t=75912

Pajda   1 kW

1 kW
Posts: 351
Joined: Jan 24 2016 3:45am
Location: Czech Republic

Re: Which cell for long lasting battery

Post by Pajda » Jun 13 2019 6:56am

Dak77 wrote:
Jun 12 2019 9:54pm
Is HG2 in that 1000cycle club?
Sure it is. But HG2 also has its own issues. The problem with HG2 is that it loses capacity very quickly during the first 50 cycles (ca 8-10% of nominal capacity). Between 50-100 cycles the capacity drop start with stabilization and after ca 150 cycle there is only minor capacity loss (86% of nominal capacity at 1C discharge 100% DoD after 1000 cycles). The good thing is that HG2 behave practically the same even under 3C continuous discharge (82% capacity drop at 3C discharge 100% DoD after 1000 cycles). For example LG MH1, MJ1 and M36 dies very quickly at 3C discharge torture.

So this is the reason why many users prefers Samsung 30Q or Sony VTC6 before LG HG2. Because for flashlight, powertools and many other applications the 50-100 cycles is the whole life. I am charging my cordless drill no more than 10 times per year. So it is useless that LG HG2 in cycle life totally outperforms both above mentioned cells after ca 400 cycles, when particularly 30Q dies.

Pajda   1 kW

1 kW
Posts: 351
Joined: Jan 24 2016 3:45am
Location: Czech Republic

Re: Which cell for long lasting battery

Post by Pajda » Jun 13 2019 7:32am

DrKraut wrote:
Jun 12 2019 3:18pm
Thanks for the info! Can you specify your charge and discharge method, like Voltage, waiting time and so on.
What cell would you recommend to me, it doesn't need to be super high energy. I'm only concerned about longevity under relatively mild conditions. I think about the Sanyo GA or Sam. 35E, or is the Panasonic PF still any good?
Sure, I am using for cycle life test calibrated battery testers with sufficient accuracy. Cells are tested in cell holders with true 4-wire connection. The temperature during measurement is 23°C +/- 2°C. I am designing my own test procedures. Each 50th cycle is inserted nominal capacity and DCIR 10s test.

The most common test have those steps:
0.5C charge (4.2V @ 100mA cut-off) - 10 min rest time - 1C discharge (LVC by manufacturer) - 10 min rest time / 100% DoD

You should choose from the equivalent category of cells:

In high-end category: LG MJ1, M36, Sony VC7, Samsung 35E and Sanyo GA I would recommend both LGs and then Samsung 35E (35E is good choice for the first 500 cycles when the fast charging is not needed = 0.3C charge rate is maximum for 35E otherwise it dies very soon). If you insist on longer cycle life (500 full cycles should be enough for most applications) or faster charging like 0.5C then take only LGs. Sanyo GA suffers with steep initial capacity loss and the most important problem is its huge DCIR rise. VC7 is very expensive and inferior to both LGs.

in best price category: Samsung 29E, Panasonic PF, LG M29, Sony NC1 I would recommend 29E as the best chioce. Panasonic PF is slightly worse under almost all cycle life test. PF is only better in fast charging (like 0.7-1C). I do not already have data for M29 and NC1 because I started with their cycle life tests only few days ago.